Introduction
ASME B16.9 is the standard for factory-made wrought butt-welding fittings, establishing essential dimensions, tolerances, ratings, and marking requirements. For engineers and specifiers working with highly corrosive process streams, combining this dimensional standard with the superior material properties of UNS N06022 (Hastelloy C22) creates a critical fitting for pipe systems.

This blog provides a professional overview of ASME B16.9 and details the types and specifications of pipe fittings manufactured from UNS N06022 alloy.
Understanding the ASME B16.9 Standard
The American Society of Mechanical Engineers (ASME) B16.9 standard specifies the requirements for fittings designed to be butt-welded to piping systems. Its primary purpose is to ensure dimensional uniformity and interchangeability between components from different manufacturers. Main standards include:
Dimensional Consistency: It defines center-to-end and end-to-end dimensions for all fitting types, ensuring a smooth internal profile and proper alignment when welded to matching pipe.
Pressure Ratings: B16.9 fittings are designed to match the pressure-temperature ratings of seamless pipe of the same material and schedule. Their rating is derived from the associated material standard, not B16.9 itself.
Tolerances: The standard provides strict tolerances for outside diameter, wall thickness, and fitting orientation, which are crucial for facilitating correct fit-up and welding.
ASME B16.9 UNS N06022 Pipe Fittings Types and Specifications
A factory producing ASME B16.9 UNS N06022 fittings must conform to both the dimensional rules of B16.9 and the material requirements of ASTM B366. The most common fitting types include:

1. Elbows (90° and 45°)
Elbows are used to change the direction of a pipeline. ASME B16.9 specifies two radii for 90° elbows:
Long Radius (LR) Elbows: The most common type, with a center-to-end dimension of 1.5 times the nominal pipe size (NPS). For example, an NPS 10 LR elbow has a center-to-end dimension of 15 inches.
Short Radius (SR) Elbows: Have a center-to-end dimension equal to the NPS. They are more compact but introduce a sharper turn, resulting in a higher pressure drop.
2. Tees (Straight and Reducing)

Tees provide a branch connection from a main pipeline.
Straight Tees: The branch diameter is the same as the main run (e.g., 8" x 8" x 8").
Reducing Tees: The branch diameter is smaller than the main run (e.g., 8" x 8" x 6"). Dimensions like the center-to-end distance on the run and the branch height are standardized by NPS.
3. Reducers (Concentric and Eccentric)
Reducers are used to connect pipes of different diameters.
Concentric Reducers: Create a symmetrical, cone-shaped transition, maintaining the centerline of the pipeline. Used in vertical pipes or where fluid drainage is not a concern.
Eccentric Reducers: Have one flat side, allowing one edge of the pipe to remain level. They are essential in horizontal pipelines to prevent air or vapor accumulation (when the flat side is on top) or to facilitate drainage (when the flat side is on the bottom).
4. Caps
Caps are used to seal the end of a pipe. The ASME B16.9 standard defines the inside diameter and the wall thickness at the bevel end to match the pipe, as well as the overall height.
ASME B16.9 Dimensional Standards and Tolerances
Tolerances for UNS N06022 butt weld fittings:
|
Parameter |
Tolerance |
|
Outside diameter at bevel |
±1.6 mm (NPS ≤ 18), ±3.2 mm (NPS ≥ 20) |
|
Inside diameter at ends |
±1.6 mm |
|
Wall thickness at ends |
Not less than 87.5% of nominal |
|
Center-to-end (90°/45° LR) |
+0 / –2.4 mm (NPS ≤ 10), ±3.2 mm (NPS ≥ 12) |
|
Overall length of reducers |
±3.2 mm |
|
Lap-joint stub end lap thickness |
+0 / –0.8 mm |
|
Ovality (excluding ends) |
≤ 3% of nominal OD |
Disclaimer: The information provided is for reference purposes. For specific projects, always consult the latest editions of the ASME B16.9 and ASTM B366 standards.
UNS N06022 Buttweld Fitting Types and Size
We manufacture the complete range of ASME B16.9 fittings in Hastelloy C22:
|
Fitting Type |
Schedule Availability |
Size Range (Seamless) |
Size Range (Welded) |
|
90° & 45° Long Radius Elbows |
Sch 10S, 20S, 40S, 80S, XS, XXS |
1/2″ – 24″ (DN 15 – DN 600) |
Up to 48″ |
|
90° Short Radius Elbows |
Sch 10S – 80S |
1″ – 12″ |
On request |
|
180° Long Radius Returns |
Sch 10S – 80S |
2″ – 24″ |
Up to 48″ |
|
Equal & Reducing Tees |
Sch 10S – 80S |
1/2″ – 24″ |
Up to 48″ |
|
Concentric & Eccentric Reducers |
Sch 10S – 80S |
3/4″×1/2″ – 48″×40″ |
Larger on request |
|
Caps |
Sch 10S – 80S |
1/2″ – 48″ |
Up to 60″ |
|
Lap-Joint Stub Ends (MSS SP-43) |
Sch 10S, 40S, 80S |
1/2″ – 24″ |
Up to 48″ |
|
Crosses |
Sch 10S – 80S |
2″ – 24″ |
On request |
All fittings are supplied in the solution-annealed condition (typically 1120–1145 °C rapid quench) to ensure optimum corrosion resistance and freedom from sensitization.
Why Choose UNS N06022 over C276 or Alloy 625?

Superior resistance to oxidizing acids (nitric, ferric chloride, seawater).
Better performance in wet chlorine and chloride-containing environments.
Higher chromium (≈22%) and optimized Mo+W content.
Virtually immune to stress corrosion cracking in hot concentrated sulfuric acid.
For projects demanding the highest corrosion performance with full compliance to ASME B16.9, our UNS N06022 butt weld fittings provide proven reliability backed by decades of field service in the most aggressive chemical and petrochemical environments.
Contact our team for quotations, material certificates, or custom fabrication of standard ASME B16.9 dimensions.