Hastelloy C22 / UNS N06022 / 2.4602

Hastelloy C22 / UNS N06022 / 2.4602
Product Introduction:
Type:
Pipes
Plates
Bars
Fittings
Forgings
Flanges
Prefabrication
We are Hastelloy C22 manufacturer and supplier, top quality, competitive price, professional distribution and after-sales service team.
Send Inquiry
Description
Technical Parameters

Hastelloy C22 characteristics

 

Hastelloy® C22 (UNS N06022/2.4602) Alloy C22 is a nickel-chromium-molybdenum solid solution strengthened super-alloy with a nominal chemical composition of 56% nickel, 22% chromium, and 13% molybdenum, with additions of iron, tungsten, and cobalt. Hastelloy C22 is a versatile nickel-chromium-molybdenum-tungsten alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including Hastelloy C276, C4 alloy, and 625 alloy.

Hastelloy C22 alloy has good resistance to pitting corrosion, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media including wet chlorine, nitric acid or a mixture of oxidative acids containing chloride ions. At the same time, Hastelloy C22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments, or in a variety of production purpose factories. Hastelloy C22 alloy is exceptionally resistant to a variety of chemical environments, including strong oxidizing substances such as ferric chloride, cupric chloride, chlorine, hot contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solution, etc. Hastelloy C22 alloy has the ability to resist the formation of grain boundary precipitation in the welding heat affected zone, which makes it suitable for many chemical process applications in the welded state.
 

Hastelloy C22 Chemical Composition, %

 

Grade

C≤

Mn≤

P≤

S≤

Si≤

Cr

Mo

Fe

Co≤

W

V≤

Ni

Hastelloy C22

0.01

1.0

0.04

0.03

0.08

20.0-22.5

12.5-14.5

2.0-6.0

2.5

2.5-3.5

0.35

remainder

 

Hastelloy C22 Mechanical Properties

 

Grade

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Hastelloy C22

100[690]

45[310]

45

 

Hastelloy C22 Physical Properties

 

Grade

Metric

Melting point

Hastelloy C22

8.90 g/cm3

1325-1370 ℃
 

 

Hastelloy C22 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

EN

Hastelloy C22

2.4602

N06022

NW 6022

NiCr21Mo14W

 

Hastelloy C22 Specifications

 

UNS

Bar

Sheet

Plate

Forging

Pipe

BW fittings

UNS N06022

ASTM B574

ASTM B575

ASTM B575

ASME SB-564

ASME B474

ASME B366

 

Hastelloy C22 Metallographic structure

 

Hastelloy C22 has a face-centered cubic lattice structure.

 

Hastelloy C22 Applications

 

Hastelloy C22 alloy has been widely used in chemical and petrochemical fields, such as components and catalytic systems in contact with chloride-containing organics. This material is especially suitable for use in high temperature, inorganic and organic acids mixed with impurities (such as formic acid and acetic acid), and seawater corrosive environments.

  • Chemical Processing
  • Food Processing
  • Pharmaceutical Industry
  • Oil & Gas
  • Power Generation
  • Pulp & Paper Industries
  • Marine Engineering

 

Hot Tags: hastelloy c22 / uns n06022 / 2.4602, China hastelloy c22 / uns n06022 / 2.4602 manufacturers, suppliers, ,

Send Inquiry
Come To Us
And Start Your RFQs Now.
contact us