Hastelloy G30 / UNS N06030 / 2.4603

Hastelloy G30 / UNS N06030 / 2.4603
Product Introduction:
Type:
Pipes
Plates
Bars
Fittings
Forgings
Flanges
Prefabrication
We are Hastelloy G30 manufacturer and supplier, top quality, competitive price, professional distribution and after-sales service team.
Send Inquiry
Description
Technical Parameters

Hastelloy G30 features

 

Hastelloy® G-30 is an improved version of nickel-chromium-iron-molybdenum-copper alloy G-3. With higher chromium, added cobalt and tungsten, the G-30 shows superior corrosion resistance over most other nickel and iron based alloys in commercial phosphoric acids as well as complex environments containing highly oxidizing acids. The resistance of the alloy to the formation of grain boundary precipitates in the heat-affected zone makes it suitable for use in most chemical process applications in the as-welded condition.

 

Hastelloy G30 Chemical Composition, %

 

Grade

C≤

Mn≤

P≤

S≤

Si≤

Cr

Mo

Fe

Co≤

Cu

Nb+Ti

W

Ni

G30

0.03

1.5

0.04

0.02

0.8

28.0--31.5

4.0--6.0

13.0-17.0

5.0

1.0--2.4

0.3--1.5

1.5--4.0

Remainder

 

Hastelloy G30 Mechanical Properties

 

Mechanical properties

Tensile, min, MPa

Yield, min, MPa

Elongation, %(min)

Metric, g/cm³

Melting Point

Hastelloy G30

586

241

30

8.22

1350--1390℃

 

Hastelloy G30 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Hastelloy G30

2.4603

N06030

 

ASTM SPECIFICATION

 

Pipe &Tube
Welded

Pipe&Tube
Seamless

Sheet/Plate

Bar /Rod

Forging /Flange

Fittings

ASTM A619

ASTM B622

ASTM B582

ASTM B581/ B472

ASTM A462

ASTM B366/B462

 

Hastelloy G30 Application

 

  • Phosphoric acid equipment
  • Pickling operations
  • Sulphuric acid equipment
  • Petrochemical products
  • Nitric acid equipment
  • Fertilizer production
  • Nuclear fuel reprocessing
  • Pesticide production
  • Nuclear waste disposal
  • Gold extraction

 

Hot Tags: hastelloy g30 / uns n06030 / 2.4603, China hastelloy g30 / uns n06030 / 2.4603 manufacturers, suppliers, jis steel, stainless steel alternative, quality assurance steel, manufacturer steel, reliability assurance steel, railway steel

Send Inquiry
Come To Us
And Start Your RFQs Now.
contact us