Hastelloy C2000 features
Designated as UNS N06200, Hastelloy C-2000 is a nickel-chromium-molybdenum alloy with a deliberate amount of copper addition which provides enhanced temperature capability in sulfuric acid, hydrofluoric acid, and dilute hydrochloric acid. The high chromium content maximizes its resistance to oxidizing chemicals and process streams contaminated with ferric ions and dissolved oxygen. Besides, Hastelloy C-2000 has excellent ductility and weldability, as well as has outstanding resistance to stress-corrosion cracking in chloride-bearing solutions.
Hastelloy C2000 Chemical Composition, %
|
Grade |
C≤ |
Mn≤ |
P≤ |
S≤ |
Si≤ |
Cr |
Mo |
Fe≤ |
Co≤ |
Ni |
Cu |
Al≤ |
|
C2000 |
0.01 |
0.5 |
0.025 |
0.01 |
0.01 |
22.0-24.0 |
15.0-17.0 |
3.0 |
2.0 |
Remainder |
1.3-1.9 |
0.5 |
Hastelloy C2000 Mechanical Properties
|
Mechanical properties |
Tensile, min, ksi[MPa] |
Yield, min, ksi[MPa] |
Elongation, %(min) |
Metric, g/cm³ |
|
C2000 |
100[690] |
45[310] |
45 |
8.5 |
Hastelloy C2000 Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
|
Hastelloy C2000 |
2.4675 |
N06200 |
NW 6200 |
ASTM SPECIFICATION
|
Pipe &Tube |
Pipe&Tube |
Sheet/Plate |
Bar /Rod |
Forging /Flange |
BW Fittings |
|
ASTM A619/ ASTM B626 |
ASTM B622 |
ASTM A575 |
ASTM A574 |
ASTM A564 |
ASTM A366/ ASTM B462 |
Hastelloy C2000 Application
- Chemical reactor
- Heat exchanger
- Petrochemical pipeline
- Pharmaceutical industry
- Gas desulfurization system
Hot Tags: hastelloy c2000 / uns n06200 / 2.4675, China hastelloy c2000 / uns n06200 / 2.4675 manufacturers, suppliers, pipe fitting steel, storage tank steel, power generation steel, project specific steel, engineering steel, drawing process steel