Hastelloy G30 (UNS N06030 / W.Nr. 2.4603) is a high-chromium nickel-base superalloy developed by Haynes International specifically to provide superior resistance to commercial phosphoric acid and highly oxidizing acid mixtures containing nitric acid, hydrofluoric acid, ferric ions, and copper chlorides.

Since its introduction in the late 1980s, G-30 has become the material of choice in wet-process phosphoric acid evaporators, acid heat exchangers, and aggressive mixed-acid services where traditional 316L, 904L, or even Alloy 28 fail rapidly.
Hastelloy G30 Chemical Composition
|
Element |
Content (%) |
Element |
Content (%) |
|
Nickel (Ni) |
Balance |
Tungsten (W) |
1.5 - 4.0 |
|
Chromium (Cr) |
28.0 - 31.5 |
Copper (Cu) |
1.0 - 2.4 |
|
Iron (Fe) |
13.0 - 17.0 |
Niobium (Nb) |
0.3 - 1.5 |
|
Molybdenum (Mo) |
4.0 - 6.0 |
Cobalt (Co) |
5.0 max |
|
Manganese (Mn) |
1.5 max |
Carbon (C) |
0.03 max |
|
Silicon (Si) |
0.8 max |
Phosphorus (P) |
0.04 max |
|
Sulfur (S) |
0.02 max |
Source: ASTM B581/B582, DIN 2.4603
This composition can also be represented visually to show the principal elements:

Hastelloy G30 Material Properties
Physical Properties
Hastelloy G30 has the following physical properties:
Density: 8.22 g/cm³ (0.297 lb/in³).
Melting Point: 1371°C (2500°F).
Thermal Conductivity: 10.2 W/mK at room temperature.
Electrical Resistivity: 1.16 μΩ·m at 20°C.
Modulus of Elasticity: 202 GPa (29.3 × 10^6 psi) at room temperature.
Thermal Expansion Coefficient: 14.4 μm/m°C (30-316°C range).
Mechanical Properties
Mechanical Properties of Hastelloy G30 at Room Temperature:
|
Property |
Metric |
Imperial |
|
Tensile Strength |
689 MPa (min) |
100 ksi (min) |
|
Yield Strength (0.2% Offset) |
317 MPa (min) |
46 ksi (min) |
|
Elongation |
55% (min) |
55% (min) |
|
Hardness (Rockwell) |
HRB 80 (max) |
HRB 80 (max) |
The alloy maintains good mechanical properties at elevated temperatures, with a tensile strength of approximately 524 MPa (76 ksi) and a yield strength of 200 MPa (29 ksi) at 538°C.
Hastelloy G30 Corrosion Resistance

Oxidizing Acids: The high chromium content provides outstanding resistance to nitric acid across a wide range of concentrations and temperatures. Testing shows corrosion rates of just 0.01 mm/year in 10% boiling nitric acid and 0.13-0.14 mm/year in 60-65% boiling nitric acid.
Phosphoric Acid: Hastelloy G30 offers superior performance in "wet process" phosphoric acid (P₂O₅), even with chloride and fluoride impurities present. This makes it particularly valuable in phosphoric acid evaporators and concentration systems in the fertilizer industry.
Sulfuric Acid: The alloy maintains good resistance to sulfuric acid across various concentrations. Corrosion rates remain below 0.5 mm/year in concentrations up to 50% at temperatures up to 107°C.
Mixed Acids: Hastelloy G30 demonstrates excellent stability in complex acid mixtures, including nitric/hydrochloric and nitric/hydrofluoric acid blends, making it suitable for pickling operations and chemical processes involving multiple acids.
Localized Corrosion: The molybdenum and tungsten content provide good resistance to chloride-induced pitting and crevice corrosion, while the nickel-chromium balance reduces susceptibility to stress corrosion cracking compared to stainless steels.
Hastelloy G30 Applications

Chemical Processing
Hastelloy G30 is extensively used in chemical process equipment handling oxidizing acids, mixed acids, and other corrosive chemicals. Its resistance to complex chemical environments makes it suitable for reactors, vessels, heat exchangers, and piping systems that must maintain integrity under aggressive conditions.
Fertilizer Production
In the fertilizer industry, the alloy is particularly valued for phosphoric acid production equipment, including evaporator tubes, reboilers, and concentration systems. Its ability to withstand "wet process" phosphoric acid containing chlorides, fluorides, and solid particles makes it essential in this application.
Metal Pickling and Surface Treatment
The alloy's resistance to nitric-hydrofluoric acid mixtures makes it suitable for pickling equipment used in stainless steel and other metal production. It maintains performance in both oxidizing and reducing acid conditions encountered in metal surface treatment processes.
Nuclear Waste Processing
Hastelloy G30 is specified for nuclear waste reprocessing applications, particularly in reboiler systems where corrosion resistance and reliability are critical for safe operation.
Petrochemical Industry
The alloy finds application in petrochemical processes involving corrosive catalysts, acid contaminants, and other aggressive chemical environments where standard stainless steels offer insufficient corrosion resistance.
Typical Product Forms We Supply in Hastelloy G30
Seamless & welded pipe (ASME SB-619 / SB-622).
Butt-weld fittings (ellipsoidal caps, tees, reducers, elbows – ASME SB-366).
Flanges (B16.5, B16.47).
Bar, plate, and sheet.
Welding consumables (ERNiCrMo-11).
Conclusion
Hastelloy G30 is one of the most cost-effective and reliable nickel alloys. It consistently outperforms 316L, 904L, Alloy 20, Alloy 28, and in many cases even G35 or Alloy 690 in phosphoric acid service.
Our mill maintains full material traceability and supplies Hastelloy G30 products with EN 10204 Type 3.1 or 3.2 certificates, accompanied by positive material identification and third-party inspection when required. For technical datasheets or quotations, please contact our team directly.