ASTM A790 S31803 Duplex Steel Pipes Supply

Oct 30, 2025

Leave a message

ASTM A790 S31803 steel pipe refers to seamless or welded steel pipe manufactured in accordance with the American Society for Testing and Materials (ASTM) A790 standard and designated UNS S31803 (Duplex 2205 duplex stainless steel).

 

ASTM A790 S31803 steel pipe

 

The microstructure of S31803 steel pipe consists of two phases: ferrite and austenite. Compared to traditional austenitic stainless steel, it offers higher mechanical strength and superior resistance to stress corrosion cracking. Furthermore, its high content of chromium, molybdenum, and nitrogen provides excellent resistance to pitting and crevice corrosion in chloride environments and acidic media.

 

Duplex 2205 steel pipe is widely used in the oil and gas, offshore engineering, chemical, petrochemical, desalination, and pulp and paper industries. The A790 standard sets strict requirements for the chemical composition, mechanical properties, heat treatment, and non-destructive testing of S31803 steel pipe, ensuring its reliability and long-term durability.

 

ASTM A790 UNS S31803 Duplex Steel Pipe Specification Chart

 

ASTM A790 UNS S31803 Chemical Composition

 

Composition

Value (Weight %)

Carbon (C)

0.030 max

Manganese (Mn)

2.00 max

Phosphorus (P)

0.030 max

Sulfur (S)

0.020 max

Silicon (Si)

1.00 max

Nickel (Ni)

4.50 – 6.50

Chromium (Cr)

21.0 – 23.0

Molybdenum (Mo)

2.50 – 3.50

Nitrogen (N)

0.08 – 0.20

Iron (Fe)

Balance

 

ASTM A790 UNS S31803 Mechanical Property

 

Property

Imperial Units

Metric Units

Tensile Strength (Min)

90 ksi

620 MPa

Yield Strength (0.2% Offset, Min)

65 ksi

450 MPa

Elongation (in 2 in. or 50 mm, Min)

25%

25%

Hardness (Max)

290 HBW (Brinell)

30 HRC (Rockwell C)

 

ASTM A790 UNS S31803 Heat Treatment and Corrosion

 

Requirement

Specification

Detail / Purpose

Heat Treatment

Solution Annealing

Pipe must be heated to a minimum temperature of 1020℃.

Cooling

Rapid Quench

Followed by rapid cooling in air or water to achieve the desired biphasic (ferrite/austenite) microstructure and prevent the formation of harmful intermetallic phases.

Intergranular Corrosion Test

ASTM A923 Practice C

Mandated for quality assurance. Measures the material's resistance to pitting and crevice corrosion, ensuring correct heat treatment and microstructure.

Microstructure

Ferrite Content

Generally required to be within the range of 30% to 70%.

 

Manufacturing and Dimensional Standards

 

Specification Aspect

Detail

Governing Standard

ASTM A790 / ASME SA-790

Manufacturing Process

Seamless or Welded (EFW, ERW, or Fusion Welded)

Applicable Dimensional Standards

ASME B36.10M or ASME B36.19M

Non-Destructive Testing (NDT)

Required

Weld Testing (for Welded Pipe)

Required

 

ASTM A790 UNS S31803 Duplex Steel Pipe Advantages

 

ASTM A790 UNS S31803 Duplex Steel Pipe Advantages

 

Excellent Resistance to Stress Corrosion Cracking

 

S31803 steel pipe offers excellent resistance to chloride stress corrosion cracking, surpassing traditional austenitic stainless steels. Duplex 2205's ferrite phase imparts high resistance to SCC, making it primarily used in offshore engineering, desalination plants, heat exchangers, and oil and gas production.

 

Excellent Mechanical Strength and Durability

 

S31803's yield strength is typically twice that of standard austenitic stainless steels, meaning thinner-walled pipes can be used for the same internal pressure or external load. This high strength not only improves the durability and safety of piping systems but also significantly reduces overall pipe weight, simplifying installation and reducing support structures.

 

Excellent Resistance to Localized Corrosion

 

Its high content of chromium, molybdenum, and nitrogen, S31803 steel pipe has an extremely high pitting equivalent index, providing excellent resistance to pitting and crevice corrosion. This characteristic is particularly critical in acidic environments, seawater or high-salinity brines, ensuring the long-term operational integrity of the pipeline and minimizing maintenance costs.

 

Excellent Resistance to Localized Corrosion

 

Cost-Effective

 

Although the initial cost of S31803 steel pipe is higher than stainless steel, its overall cost performance is highly significant over the project's lifecycle. Its high strength allows for thinner wall thicknesses, reducing weight, procurement costs, and transportation expenses.

 

At the same time, its excellent corrosion resistance and durability extend service life and reduce replacement frequency, making Duplex 2205 an economical, long-term solution for harsh environment applications.

 

Excellent Weldability and Processability

 

Compared to some high-alloy materials, S31803 duplex steel pipe exhibits excellent weldability. When properly welded, it maintains corrosion resistance and mechanical properties in both the weld and heat-affected zones.

 

Furthermore, S31803 steel pipe's good toughness makes cold working and forming relatively easy, facilitating its adaptation to various complex piping layouts and on-site installation.

 

ASTM A790 UNS S31803 Duplex Steel Pipe Price

 

Pipe Type

Size Range

Price (per Kg/lb)

Seamless Pipe

1" NB to 8" NB (Schedule 40/80)

$9.00 – $14.00 USD/Kg

Seamless Pipe

Large OD or Heavy Wall

$10.00 – $15.00+ USD/Kg

Welded Pipe

4" NB to 24" NB (Standard Wall)

$7.00 – $11.00 USD/Kg

Plate/Sheet) & other forms

Raw materials used to manufacture welded pipes

$6.00 – $10.00 USD/Kg

 

Note: NB stands for nominal diameter. The above prices are estimates of Bare Pipe's raw material and processing costs and do not include freight, inspection fees, taxes, or other additional service charges.

 

price of S31803 duplex steel

 

The price of S31803 duplex steel is closely tied to market price fluctuations for three alloys: nickel, chromium, and molybdenum.

 

Nickel and molybdenum are particularly expensive and fluctuate significantly, while S31803 contains high levels of chromium, moderate amounts of nickel, and the critical element molybdenum. Price increases for these elements directly impact the raw material cost of S31803. Therefore, suppliers often base their quotes on the real-time or recent monthly average prices of metal market indices.

 

The ASTM A790 standard imposes stringent requirements on the manufacturing process for S31803 pipe. Duplex steel requires a precise solution annealing treatment at temperatures above 1020°C, followed by rapid cooling to achieve the ideal ferrite/austenite phase equilibrium.

 

This heat treatment is more complex and energy-intensive than that for standard stainless steel, requiring additional equipment and longer processing times.

 

A790 standard

 

In addition, the A790 standard mandates rigorous nondestructive and corrosion testing, and these inspection costs are factored into the final quote.

 

The dimensions of seamless or welded pipe also significantly impact price. Seamless pipe is generally more expensive per unit weight than welded pipe due to its greater production difficulty and lower raw material loss. Welded pipe manufacturing involves sheet rolling and automated welding, and its cost is primarily determined by sheet price and post-weld heat treatment requirements.

 

Finally, small-diameter and special thick-wall specifications often have higher unit prices than medium-standard pipe due to smaller production batches and greater processing complexity. Specific customer-required lengths, tolerances, and surface finishes can also contribute to price differences.

 