When engineers and procurement specialists select stainless steel pipe for industrial projects, one of the first decisions they face is choosing between welded pipe types - specifically between Electric Resistance Welded (ERW) pipe and Submerged Arc Welded (SAW) pipe. Both are economical alternatives to seamless pipe, yet they serve very different purposes, carry different pressure capabilities, and are governed by different ASTM/ASME standards.

This guide cuts through the confusion. Written for plant engineers, project managers, and purchasing teams alike, it explains - in plain, rigorous language - what ERW and SAW pipe actually are, how they are made, how they differ in performance, and which type is the right choice for your specific application. The article also covers the key standards (ASTM A312, A358), grade suitability, dimensional ranges, cost considerations, and quality-inspection requirements.
ERW vs SAW at a Glance
Before diving into technical detail, the table below provides a side-by-side snapshot of the two pipe types.
|
Attribute |
ERW Pipe |
SAW Pipe (LSAW / SSAW) |
|
Welding process |
High-frequency electric resistance (forge weld; no filler metal) |
Submerged arc fusion weld (filler wire + flux; inside & outside passes) |
|
Weld type |
Forge bond - no filler added; weld metal is parent material |
Fusion bond - filler wire engineered to match or exceed base metal |
|
Primary standard |
ASTM A312 (WLD) |
ASTM A358 / ASME SA358 (EFW) |
|
Diameter range |
NPS 1/8" – NPS 24" (typical) |
NPS 8" – NPS 72" (LSAW); up to NPS 100"+ (SSAW) |
|
Wall thickness |
SCH 5S to SCH 80S |
3 mm – 60 mm (heavier walls achievable) |
|
Surface finish |
Smooth, flat weld seam; tighter OD tolerances |
Internal/external weld reinforcement; slightly wider seam |
|
Relative cost |
Lower (high-speed continuous production) |
Higher (plate forming, double-weld pass, RT/UT inspection) |
|
Weld defect risk |
Low; only straight weld / wire-line defects - easy to UT detect |
Slightly higher variety (slag inclusion, porosity) but flux shields arc |
|
Pressure service |
Low-to-medium; limited by thin walls and no filler |
Medium-to-high; engineered filler enables full-penetration joints |
|
Joint efficiency (ASME B31.3) |
0.85 (A312 WLD, with RT) |
0.85–1.00 (A358 Class 1 with 100% RT) |
|
Common grades |
TP304/304L, TP316/316L, TP321, TP347 |
TP304L, TP316L, TP317L, TP321H, TP347H, 904L, 2205, 2507 |
|
Typical applications |
General process, HVAC, food/pharma, light chemical, architectural |
Heavy chemical, petrochemical, power gen, large-diameter infrastructure |
Table 1: ERW vs SAW Stainless Steel Pipe - Master Comparison. Source: ASTM A312/A358, ASME B31.3, ASME B36.19M.
How Each Pipe Type Is Made
ERW (Electric Resistance Welded) Pipe
ERW pipe is produced by a continuous, high-speed forming process. A flat strip of stainless steel coil is progressively roll-formed into a cylindrical tube shape. Two copper disc electrodes apply high-frequency current to the two free edges of the strip. The skin effect and proximity effect of the high-frequency current concentrate intense heat at the abutting edges, raising them to welding temperature. A set of squeeze rollers then forces the hot edges together under controlled pressure, forging the seam.
The critical technical point: ERW is a forge weld, not a fusion weld. No filler metal is added. The weld seam is formed entirely from the parent stainless steel strip, meaning the weld's chemical composition is identical to the base material - but its grain structure and heat-affected zone (HAZ) differ from the pipe body. After welding, the pipe undergoes solution annealing to normalize the HAZ grain structure, followed by pickling or bright annealing to restore the passive oxide layer.
Under ASTM A312 (WLD designation), the automatic welding process does not allow filler metal addition. This makes ERW pipe highly cost-effective for standard diameters but inherently limits wall thickness and pressure capability. For stainless steel, the most common ERW sizes run from NPS 1/8" to NPS 24", in schedule designations from 5S through 80S.
SAW (Submerged Arc Welded) Pipe
SAW pipe - produced as either Longitudinal SAW (LSAW) or Spiral SAW (SSAW) - belongs to the Electric Fusion Welding (EFW) family. The fundamental difference is fusion: a consumable wire electrode is continuously fed into the arc, and a granular flux blanket shields the molten weld pool from atmospheric contamination. The result is a deep-penetration fusion weld with engineered metallurgy.
LSAW pipe is formed from a single heavy steel plate (sourced to ASTM A240). The plate is pressed or roll-bent into a cylinder (commonly via UOE or JCOE press forming), then welded on the inside seam first, followed by an outside pass - known as Double Submerged Arc Welding (DSAW). This double-pass approach maximises weld integrity and enables Class 1 joint efficiency under ASTM A358.
SSAW pipe is formed by unwinding a hot-rolled coil and feeding the strip at a helix angle into a forming cage, creating a spiral seam. The helix angle (typically 50–75 degrees) means the weld seam never runs perpendicular to the pipe axis, which gives a specific type of stress distribution advantage under internal pressure. SSAW is most economical for very large diameters (above NPS 24") but is generally limited to lower-pressure service (API Class 3/4 areas in pipeline design) due to the longer seam length.
Manufacturing Process Summary Table
|
Step |
ERW Pipe |
SAW Pipe (LSAW) |
|
Starting material |
Hot-rolled stainless strip/coil (ASTM A240) |
Heavy steel plate (ASTM A240, typically thicker gauges) |
|
Forming |
Continuous roll forming through fin rolls |
UOE or JCOE press forming (batch process) |
|
Welding |
HF current - forge bond, no filler metal |
Inside SAW pass → outside SAW pass; filler wire + flux |
|
Post-weld heat treatment |
Solution annealing (entire pipe); water quench or rapid cool |
Solution annealing; may be localized or full pipe depending on class |
|
Surface finishing |
Annealed & pickled (AP) or bright annealed (BA) |
AP, pickling, No. 4, or electropolished per application |
|
NDE / inspection |
Eddy-current test (ECT) or hydrostatic test; UT optional |
100% RT (Class 1/3) or spot RT (Class 2/5); UT + hydrostatic |
Table 2: ERW vs SAW Manufacturing Process Comparison. Source: ASTM A312, ASTM A358, ASME B36.19M; EETA technical summary.
Governing Standards: ASTM A312 vs ASTM A358
Understanding which standard governs your pipe type is essential for correct specification, quality assurance, and code compliance. The two dominant standards for stainless steel welded pipe are ASTM A312/ASME SA312 and ASTM A358/ASME SA358.

ASTM A312 / ASME SA312
ASTM A312 is the core specification for austenitic stainless steel pipe in pressure and general industrial service. It covers three manufacturing types: Seamless (SMLS), Welded (WLD - which includes ERW pipe), and Heavily Cold Worked (HCW). For welded pipe under A312, automatic welding without filler metal addition is required. This is the ERW production method.
Key A312 data points for ERW stainless pipe:
- Diameter range: NPS 1/8" to NPS 30" (per ASME B36.19M)
- Wall thickness: SCH 5S through SCH 80S (with SCH 10S and 40S most common)
- Grades: TP304, TP304L, TP316, TP316L, TP321, TP347, TP310S, and others
- Delivery condition: Annealed and Pickled (AP) or Bright Annealed (BA)
- Testing: Hydrostatic test OR Non-Destructive Electric Test (ECT) at manufacturer's option
- Joint efficiency: 0.85 for welded pipe with radiographic examination (ASME B31.3)
ASTM A358 / ASME SA358
ASTM A358 governs electric-fusion-welded (EFW) austenitic stainless steel pipe - the SAW/LSAW pipe used in large-diameter and high-pressure applications. Unlike A312, A358 pipe uses filler metal and generally applies plate (ASTM A240) rather than coil as the starting material. A358 specifies five classes that define increasingly rigorous welding and inspection requirements:
|
Class |
Welding method |
Radiographic testing |
Joint efficiency (E) |
|
Class 1 |
Double-welded, filler metal in all passes |
100% RT (complete) |
1.00 |
|
Class 2 |
Double-welded, filler metal in all passes |
None required |
0.85 |
|
Class 3 |
Single-welded, filler metal in all passes |
100% RT (complete) |
0.90 |
|
Class 4 |
Single-welded; inside pass may be without filler |
100% RT (complete) |
0.85 |
|
Class 5 |
Double-welded, filler metal in all passes |
Spot RT only |
0.80 |
Table 3: ASTM A358 Class Definitions and Joint Efficiency Factors. Source: ASTM A358/A358M (official specification); ASME B31.3 Section 302.3.5.
For engineering design calculations under ASME B31.3 (Process Piping), the joint efficiency E directly affects the allowable internal pressure a pipe can sustain. Specifying A358 Class 1 (E = 1.00) can allow smaller wall thickness for the same pressure rating compared to Class 5 (E = 0.80), which directly reduces material cost on large-diameter orders - a key procurement lever.
Size range under A358: ASTM A358 is particularly suited to larger diameter pipes, typically from NPS 8" to NPS 72" and beyond, with wall thickness from 3 mm to 60 mm. These dimensions are not achievable via ERW production, which is the fundamental reason A358 EFW/SAW pipe exists.
Performance Comparison: Five Critical Dimensions
The most fundamental performance difference between ERW and SAW pipe lies in weld metallurgy. ERW pipe relies on forge bonding - the parent metal is heated and pressed together without any filler. The result is a narrow, flush weld seam with low residual stress. Studies confirm that ERW pipe typically exhibits lower residual stress than SAW pipe because the continuous roll forming and subsequent sizing operations (oval-to-circle deformation sequences) relieve internal stresses progressively.
SAW pipe, by contrast, uses a consumable filler wire and flux. This enables the weld chemistry to be engineered: by selecting specific wire/flux combinations, a skilled manufacturer can formulate a weld deposit that matches - or actually exceeds - the mechanical properties and corrosion resistance of the parent stainless grade. This is why SAW is the only viable process for critical-service, heavy-wall pipe. An engineer specifying API 5L X65 or an austenitic stainless grade for a high-pressure chemical line needs confidence that the weld seam will not be the weakest link - SAW provides that assurance.
Surface Quality and Dimensional Accuracy
ERW pipe has a clear advantage in surface finish. Because no filler metal is deposited, the ERW weld seam is flat, smooth, and nearly flush with the pipe surface. Post-weld bead removal produces a seam that is difficult to detect visually, which is important for sanitary applications (food, pharmaceutical, bioprocessing) where internal surface cleanliness matters.
SAW pipe, particularly LSAW, has internal and external weld reinforcement (weld bead crown) that extends above the plate surface. Standards specify maximum weld crown heights, but the reinforcement is inherent to the fusion process. For fluid-carrying applications, the internal reinforcement may need to be ground flush if flow characteristics or cleanliness are critical - adding cost and lead time.
On dimensional accuracy, ERW pipe produced from precision-rolled coil typically achieves tighter outside diameter tolerances and better roundness than plate-formed LSAW pipe. This translates to easier fit-up and better gasket sealing at flanged connections.
Pressure Rating and Wall Thickness Capability
Pressure rating is the most decisive factor in the ERW vs SAW choice for process engineers. ERW pipe, being produced from coiled strip and without filler metal, is limited in achievable wall thickness. In stainless grades, ERW is practical up to approximately SCH 80S; beyond that, the process becomes uneconomical or technically constrained.
SAW pipe, starting from heavy plate, can achieve wall thicknesses of 60 mm and beyond, and diameters up to NPS 72" (LSAW) or larger (SSAW). Combined with the engineered weld metallurgy and full RT inspection at Class 1, A358 SAW pipe can achieve a joint efficiency of 1.00, making it equal to seamless pipe for pressure calculations. This is why SAW pipe is the standard choice for large-diameter pressure vessel nozzles, bulk chemical transfer headers, power plant steam lines, and similar demanding services.
Defect Types and Non-Destructive Examination (NDE)
ERW pipe has fewer defect modes than SAW pipe. ERW weld defects are limited to straight weld defects and wire-line defects - both of which lie along the weld seam and are highly amenable to ultrasonic testing (UT) and eddy-current testing (ECT). The defect geometry in ERW is straightforward, and modern online UT systems can scan the full weld seam at production speeds.
SAW pipe has a broader potential defect spectrum: in addition to wire-line and straight weld defects, the flux deposit introduces risk of slag inclusions, porosity, and other volumetric defects. However, the flux shield itself provides significant protection against atmospheric contamination - which is why SAW produces consistently high-quality welds despite the richer defect vocabulary. NDE for SAW pipe under A358 is correspondingly more thorough, with 100% RT required at Classes 1 and 3.
Bottom line for the engineer: if you specify A358 Class 1 SAW pipe with 100% RT, you receive a pipe whose entire weld seam has been radiographically verified - a higher assurance level than standard ERW under A312.
Corrosion Performance
Both ERW and SAW stainless steel pipe benefit from the full corrosion resistance of the parent austenitic stainless grade when properly solution-annealed and passivated. However, there are important distinctions to keep in mind:
ERW pipe (A312 WLD): No filler metal is added, so the HAZ composition is identical to the parent strip. After proper annealing and pickling, the passive film is restored uniformly. The low residual stress profile of ERW pipe reduces susceptibility to stress corrosion cracking (SCC) in chloride-containing environments.
SAW pipe (A358 EFW): The filler wire must be selected to match or exceed the parent metal's corrosion resistance. For grades like TP316L or duplex 2205, matching filler chemistry is critical - under-alloyed filler can create a galvanic corrosion path at the weld seam. Reputable SAW manufacturers specify filler wire chemistry per AWS A5.9 and subject it to corrosion testing per ASTM A262.
Sensitization risk: In both pipe types, the low-carbon 'L' variants (304L, 316L) are preferred for welded construction to minimise carbide precipitation at grain boundaries and reduce sensitization-related intergranular corrosion.
Grade Suitability by Process
Not every stainless grade is equally well-suited to both ERW and SAW production. The table below summarises grade suitability and typical application pairing.
|
Grade |
ERW (A312) |
SAW (A358) |
Key property |
Typical application |
|
TP304/304L |
✓ Primary |
✓ |
18Cr-8Ni; general corrosion resistance |
General process, food/beverage, architectural, HVAC |
|
TP316/316L |
✓ Primary |
✓ |
16Cr-10Ni-2Mo; chloride and pitting resistance |
Marine, pharmaceutical, chemical processing, coastal infrastructure |
|
TP321 / TP347 |
✓ |
✓ |
Ti/Nb stabilised; high-temperature service |
Exhaust systems, heat exchangers, petrochemical furnaces |
|
TP317L |
Limited |
✓ Preferred |
3–4% Mo; superior chloride and acid resistance |
Pulp/paper, strong acid chemical service |
|
904L |
Niche |
✓ Preferred |
High alloy; sulfuric acid resistance |
Sulfuric acid plants, phosphoric acid, seawater desalination |
|
2205 Duplex |
Possible |
✓ Standard |
~2× yield strength vs 316L; SCC resistant |
Offshore oil/gas, desalination, chemical tankers |
|
2507 Super Duplex |
Rare |
✓ Standard |
PREN ~42; extreme chloride resistance |
Subsea pipelines, FPSO, deep desalination |
|
TP310S / TP310H |
Limited |
✓ Preferred |
25Cr-20Ni; high-temperature oxidation |
Furnace liners, heat treatment equipment, ethylene cracking |
Table 4: Stainless Steel Grade Suitability for ERW vs SAW Production. Source: ASTM A312, ASTM A358, ASTM A240.
Application Selection Guide
The right pipe type depends on four primary variables: required diameter, operating pressure, media aggressiveness, and budget. The following matrix provides clear guidance.
|
Application context |
Recommended pipe type |
Standard & notes |
|
Pharmaceutical / bioprocess / food sanitary lines (small-medium diameter, clean surfaces) |
ERW (A312 WLD) |
Smooth weld seam; easy electropolishing; ASTM A312 TP316L 10Ra finish achievable |
|
HVAC, general utilities, potable water (NPS 2"–12", low pressure) |
ERW (A312 WLD) |
Cost-effective; ASTM A312 TP304L / TP316L; adequate for ambient-temperature service |
|
Chemical processing - moderate pressure, standard corrosive media (acids, alkalis) |
ERW up to NPS 12"; SAW for larger |
A312 for smaller sizes; A358 Class 3/4 for larger diameter headers; TP316L typical |
|
Petrochemical / refinery bulk headers and process lines (NPS 12"–48", elevated pressure) |
LSAW (A358 EFW) |
A358 Class 1 (100% RT) recommended; TP321H or TP347H for high-temperature service |
|
Power generation - steam lines and heat exchanger connections |
LSAW (A358 EFW) for large lines; ERW (A312) for smaller branches |
Class 1 joint efficiency (E=1.0) maximises pressure allowance; TP321H/347H common |
|
Offshore oil and gas, subsea flowlines (duplex/super duplex) |
LSAW (ASTM A928) |
ASTM A928 for duplex/super duplex welded pipe; 2205 or 2507; NACE MR0175 compliance |
|
Low-pressure large-diameter infrastructure (water transmission, piling, marine structures) |
SSAW (ASTM A358 or A778) |
Most economical for NPS 24"+ at low pressure; helix seam distributes primary stress |
|
Architectural / structural (handrails, cladding, decorative) |
ERW (ASTM A554) |
ASTM A554 for mechanical/structural tubing; polished or satin finishes available |
Table 5: Application Selection Matrix - ERW vs SAW Stainless Steel Pipe. Source: ASTM A312, A358, A554, A928; ASME B31.3; EETA application guidance.
Quality Assurance and Inspection Requirements

Stainless steel welded pipe is subject to rigorous quality inspection under both ASTM standards. The following tests are applicable:
|
Test / Inspection |
ERW (A312 WLD) |
SAW (A358 EFW) |
|
Chemical analysis |
Required per grade (heat analysis + product analysis) |
Required; filler wire also tested per AWS A5.9 |
|
Tensile test |
Mandatory; transverse weld specimen |
Mandatory; all-weld-metal and transverse specimens |
|
Flattening test |
Mandatory (crush test of weld integrity) |
Mandatory |
|
Hydrostatic test |
Required OR ECT (manufacturer option) |
Required; pressure per formula; holds specified time |
|
Non-destructive electric test (ECT/UT) |
Standard online UT or ECT of weld seam |
UT per applicable ASME Section V procedures |
|
Radiographic testing (RT) |
Not required under base A312 (purchaser can request) |
100% RT (Class 1/3); spot RT (Class 2/5); none (Class 2 without RT) |
|
Intergranular corrosion test |
ASTM A262 Practice E (purchaser specified) |
ASTM A262 (by agreement; common for TP316L) |
|
Dimensional inspection |
OD, wall, length, straightness per ASME B36.19M |
OD, wall ±10%, ovality, weld crown height; per A358 |
|
Material test certificate (MTC) |
EN 10204 3.1 or 3.2 as specified |
EN 10204 3.1 or 3.2; includes RT report for Class 1/3 |
Table 6: Quality Inspection Requirements - ERW vs SAW Stainless Steel Pipe. Source: ASTM A312, ASTM A358, ASME Section V, EN 10204; EETA quality framework.
Frequently Asked Questions
ERW stainless steel pipe is not equivalent to seamless pipe in terms of pressure integrity, but for many applications it is entirely adequate. Under ASME B31.3, welded pipe produced to ASTM A312 (WLD) carries a joint efficiency of 0.85 when radiographically examined, meaning the allowable stress must be derated by 15% versus a seamless equivalent. For low-to-moderate pressure services - which represents the vast majority of applications - this derate is easily accommodated by standard schedule selections. Seamless pipe is generally specified only for high-pressure, critical-service, or very high-temperature applications where the extra cost (20–40% premium over ERW) is justified.
Q2: What is the difference between ERW, EFW, and SAW pipe?
ERW (Electric Resistance Welded) is a forge weld - the pipe edges are heated by high-frequency current and pressed together without filler metal. EFW (Electric Fusion Welded) is the broader category of arc fusion welding processes. SAW (Submerged Arc Welding) is the most common and advanced EFW method, using a wire electrode and granular flux to produce a full-penetration fusion weld. In everyday specification language, SAW pipe (LSAW or SSAW) is a sub-type of EFW pipe and is covered by ASTM A358.
Q3: Can I use ERW pipe for stainless steel pharmaceutical applications?
Yes - ERW stainless steel pipe is the standard choice for pharmaceutical and bioprocessing piping. The flush, smooth ERW weld seam lends itself to internal electropolishing, and ASTM A312 TP316L (or TP316) in SCH 10S is the industry-standard material form for sterile process lines. After electropolishing, the internal surface can achieve Ra values well below 0.5 micron, meeting the tightest hygienic standards. ERW pipe under ASTM A270 (Sanitary Tubing standard) is specifically produced for food, dairy, and pharmaceutical applications.
Q4: What does ASTM A358 Class 1 mean, and when should I specify it?
ASTM A358 Class 1 means the SAW pipe is double-welded (inside and outside passes), all weld passes use filler metal, and 100% radiographic testing (RT) is performed on the complete weld seam. Class 1 achieves a joint efficiency of 1.00 under ASME B31.3, equivalent to seamless pipe for pressure calculations. Specify Class 1 whenever: (a) the pipe is in critical pressure service (above 50% of allowable stress), (b) the service involves hydrogen, toxic fluids, or lethal service per B31.3 Category M, or (c) you wish to achieve the thinnest possible wall for a given pressure rating on large-diameter pipe.
Q5: Is LSAW or SSAW better for large diameter stainless steel pipe?
For most industrial service where pressure integrity and weld quality are paramount, LSAW (Longitudinal SAW) is preferred. The straight seam is shorter than SSAW's helical seam, resulting in fewer total weld metres to inspect, easier radiographic examination, and lower total weld volume to defect-free status. SSAW pipe is a cost-effective choice for low-pressure applications - such as water transmission mains, piling, or marine outfall pipes - at very large diameters (above NPS 36") where LSAW plate sizes become limiting or uneconomical.
Q6: What is the maximum diameter and wall thickness available in ERW stainless steel pipe?
ERW stainless steel pipe is commercially available up to approximately NPS 24" (610 mm OD) in standard grades, with wall thickness from SCH 5S (very thin) up to SCH 80S. Above NPS 16"–20", the ERW process becomes technically demanding and less economical for stainless grades, and most specifications at these sizes transition to LSAW/A358 EFW pipe. For sizes above NPS 24", SAW is the standard welded process.
Q7: How do I specify stainless steel ERW or SAW pipe correctly on a purchase order?
A complete specification for stainless steel welded pipe should include: (1) ASTM standard and edition (e.g., ASTM A312-23 or ASTM A358-21); (2) Grade (e.g., TP316L); (3) NPS and schedule (e.g., NPS 8" SCH 40S) or OD × wall thickness; (4) length (random, double random, or cut length); (5) pipe type: seamless, welded (A312), or EFW class (A358 Class 1–5); (6) finish (AP, BA, No. 4 polish, etc.); (7) inspection and test requirements (hydrostatic test, ECT, RT level, ASTM A262 if required); (8) material test certificate (EN 10204 3.1 or 3.2); and (9) any supplementary requirements (impact testing, PMI, hardness testing).
Conclusion
The choice between ERW and SAW stainless steel welded pipe is not a matter of one being superior to the other - it is a matter of matching the right manufacturing process to the right application requirements.
ERW pipe (ASTM A312 WLD) is the workhorse of everyday industrial piping: cost-effective, dimensionally precise, readily available, and entirely suitable for the vast majority of general process, sanitary, architectural, and utility applications up to NPS 24". Its flush weld seam, low residual stress profile, and compatibility with electropolishing and hygienic finishing make it the preferred choice for pharmaceutical, food, and beverage services.
SAW pipe - LSAW and SSAW under ASTM A358 - is the engineering solution when scale, pressure, or service severity exceeds what ERW can deliver. Its fusion weld metallurgy, engineered filler chemistry, double-pass weld integrity, and 100% RT capability (Class 1) make it the standard for large-diameter pressure headers, petrochemical process lines, power generation infrastructure, and offshore/subsea applications where a weld-seam failure is not an option.
In practice, many projects use both pipe types: SAW for the large-diameter main headers and ERW for the smaller branch connections, instrumentation take-offs, and utility lines - each fulfilling its design function at optimum cost. Understanding the technical distinction between these two pipe types is the foundation of sound piping engineering.
Need ERW or SAW stainless steel pipe for your project?
JN Alloys / Jinie Technology (Jiangsu) Co., Ltd | www.jnalloys.com
ASTM A312 | ASTM A358 | TP304L | TP316L | TP321 | 2205 | 2507 | 904L