ASTM A182 Alloy 17-4PH Forged Socket Weld Half Coupling, ASME SA 182 Stainless Steel 17-4PH Socket Weld Half Coupling, Stainless Steel DIN 1.4542 Half Coupling, Manufacturer Of ASTM A705 Stainless Steel 17-4PH Forged Half Coupling, UNS S17400 Stainless Steel Forged Socket Weld Half Coupling.
One of the most widely used and most well-liked stainless chromium-nickel alloy steels is 17-4PH, which has a martensitic structure and a copper addition. It is precipitation hardened. It exhibits excellent hardness and high strength qualities while exhibiting great corrosion resistance. Stainless Steel UNS S17400 Coupling, precipitation-hardening stainless steel formulated for primary forming into wrought products. Stainless Steel 17-4 PH Coupling are martensitic stainless steels that are precipitation hardened to achieve excellent mechanical properties. Like martensitic grades, 17-4 PH Stainless Steel Coupling are known for their ability to gain high strength through heat treatment. Alloy 17-4PH Coupling is a steel product from the family of improved machinability and precipitation-hardened stainless steel. Stainless Steel DIN 1.4542 Coupling has good mechanical properties at temperatures up to 600 Degrees F (316 Degrees C) and good toughness in both base metal and welds. The valuable combination of high strength, good corrosion resistance, and toughness of Stainless Steel 17-4 PH Coupling in both base metals and welds give designers opportunities to add reliability to their products while simplifying fabrication and often reducing costs.
The chemical mixture of SS 17-4 PH Coupling offers many benefits, including safety, ease of construction, flexibility, and the capacity to weld. The strength and toughness of the material may be affected by the temperature range maintained throughout the heat treatment process. Heat treatment further improves SS 17-4 PH Coupling mechanical properties, including high flexibility and exceptional tensile and yield strengths. Forged stainless steel 17-4 PH Couplings are designed to endure severe weights and come with a warranty on their respective items. These stainless steel 17-4 PH Couplings maintain a remarkable blend of high strength, excellent corrosion resistance, and strong mechanical properties at temperatures as high as 600 degrees Fahrenheit (316°C). The pipe fitting maintains its oxidation resistance even when exposed to an oxidising atmosphere. This alloy's unique combination of characteristics enables it to solve various design and manufacturing challenges effectively.
Specification of Stainless Steel 17-4PH Forged Socket Weld Half Coupling
|
Standard |
ASTM A182 / ASME SA 182 |
|
Dimension |
ANSI/ASME B16.11 |
|
Grade |
Stainless Steel 17-4PH (UNS NO. S17400) |
|
Size |
1/2"NB TO 4"NB IN |
|
Class |
2000LBS, 3000LBS, 6000LBS, 9000LBS, etc. |
|
Types |
Socket Weld (S/W) & SCREWED (SCRD) – NPT, BSP, BSPT, Threaded Fittings |
Chemical Composition and Properties of Stainless Steel 17-4PH Coupling
17-4PH stainless steel, also known as SAE Type 630 or UNS S17400, is a high-strength, corrosion-resistant alloy with a specific chemical composition. The primary elements in 17-4PH stainless steel and their typical concentrations are: Chromium (15.0-17.5%), Nickel (3.0-5.0%), Copper (3.0-5.0%), Carbon (0.07% max), Manganese (1.0% max), Phosphorus (0.04% max), Sulfur (0.03% max), Silicon (1.0% max), and Columbium + Tantalum (0.15-0.45%). These elements combine to give 17-4PH its unique properties, such as high strength, hardness, and corrosion resistance.
Mechanical Properties of Stainless Steel 17-4PH Coupling
Stainless Steel 17-4PH Coupling can be significantly enhanced through heat treatment, achieving an ultimate tensile strength of up to 190,000 psi (1,300 MPa), yield strength up to 160,000 psi (1,100 MPa), and hardness of approximately 44 Rockwell C (Rc). It typically has an elongation of around 5% in 2 inches (51 mm). These properties make 17-4PH suitable for demanding applications requiring high strength and durability.
Corrosion Resistance of Stainless Steel 17-4PH Coupling
Stainless Steel 17-4PH Coupling offers excellent corrosion resistance, comparable to austenitic 304 stainless steel. It performs well in various environments but can be susceptible to crevice corrosion in stagnant saltwater and stress corrosion cracking when aged at lower temperatures. This makes it ideal for use in various industries, though it is important to consider the specific conditions in which it will be used.
Physical Characteristics of Stainless Steel 17-4PH Coupling
The physical characteristics of 17-4PH stainless steel Coupling include a density of approximately 0.282 lb/in³ (7,800-7,900 kg/m³), a melting range of 2560-2625°F (1404-1440°C), thermal conductivity between 17.9-22.6 W/m·K, and a linear coefficient of thermal expansion around 10.8-11.2 μm/m·°C (6-6.3 in/in/°F·10^6). These characteristics are crucial for understanding how the material behaves under different thermal and mechanical conditions.
Types of Stainless Steel 17-4PH Couplings
SS 17-4PH Couplings Stockist
ASTM A182 F17-4PH Stainless Steel Couplings
ASME SA 182 F17-4PH SS Couplings
17-4PH Stainless Steel Couplings Exporter
UNS S17400 Forged Socket Weld Couplings
SS 17-4PH Half Couplings
SS 17-4PH Forged Couplings
Stainless Steel 17-4PH Couplings
SS 17-4PH Couplings
SS 17-4PH Socket Weld Couplings
SS 1.4542 Couplings Supplier
Stainless Steel 17-4PH Couplings
ANSI B16.11 Stainless Steel 17-4PH Couplings
Size Of B16.11 ASME Half Coupling Forged fitting
|
NPS |
End To End |
Thread Minimum Length |
O.D. |
|||
|
Inches |
ASME B16.11 Full Coupling |
ASME B16.11 Half Coupling |
|
|
# 3000 |
# 6000 |
|
|
A |
A/2 |
B |
C |
D |
D |
|
1/8 |
32 |
A/2 |
6.7 |
6.4 |
16 |
22 |
|
1/4 |
35 |
A/2 |
10.2 |
8.1 |
19 |
25 |
|
3/8 |
38 |
A/2 |
10.4 |
9.1 |
22 |
32 |
|
1/2 |
48 |
A/2 |
13.6 |
10.9 |
28 |
38 |
|
3/4 |
51 |
A/2 |
13.9 |
12.7 |
35 |
44 |
|
1 |
60 |
A/2 |
17.3 |
14.7 |
44 |
57 |
|
1 1/4 |
67 |
A/2 |
18 |
17 |
57 |
64 |
|
1 1/2 |
79 |
A/2 |
18.4 |
17.8 |
64 |
76 |
|
2 |
86 |
A/2 |
19.2 |
19 |
76 |
92 |
|
2 1/2 |
92 |
A/2 |
28.9 |
23.6 |
92 |
108 |
|
3 |
108 |
A/2 |
30.5 |
25.9 |
108 |
127 |
|
4 |
121 |
A/2 |
33 |
27.7 |
140 |
159 |
Stainless Steel 17-4 PH Forged Coupling Uses
Oil and Gas Industries: 17-4 PH Coupling lattice fittings are commonly used in offshore drilling rigs, subsea equipment and pipelines where corrosion resistance and strength are required, especially in harsh environments
Aerospace Applications: Aerospace applications, including structural components, landing gear, and engine components, require lightweight, high-strength materials with excellent corrosion resistance
Chemical Applications: 17-4 pH Coupling mesh fittings are used in pipelines, valves and fittings handling corrosive chemicals and high-pressure water in chemical plants and refineries
Marine Applications: Because of Stainless Steel 17-4 PH Forged Coupling resistance to seawater and salt spray, these materials are used in marine equipment such as boat hulls, propeller shafts and marine pump components