What is F316 Material?
F316 (UNS S31600) is an austenitic stainless steel containing 16-18% chromium, 10-14% nickel, and 2-3% molybdenum. This "marine-grade" alloy delivers superior corrosion resistance vs. standard 304/304L, especially against:
- Chlorides (seawater, brine)
- Sulfuric/phosphoric acids
- Pitting/crevice corrosion
F316 pipe fittings comply with ASTM A403 and dimensional standards ASME B16.9/B16.11.


Why Choose F316 Pipe Fittings?
|
Property |
F316 Advantage |
Industry Application |
|
Corrosion Resistance |
2-3% Mo boosts PREN① to 24.5+ |
Seawater cooling, desalination plants |
|
High-Temp Strength |
Retains strength to 870°C (1600°F) |
Refinery piping, exhaust systems |
|
Fabricability |
Excellent weldability (TIG/MIG/SAW) |
Custom manifolds, skid modules |
|
Cost Efficiency |
20-30% cheaper than duplex/super-austenitic alloys |
Chemical processing, food & pharma |
Technical Specifications
Composition & Mechanical Properties
|
Element |
Cr |
Ni |
Mo |
C (max) |
Yield Strength |
Tensile Strength |
|
% Range |
16-18 |
10-14 |
2-3 |
0.08 |
≥30 ksi (205 MPa) |
≥75 ksi (515 MPa) |
Pressure-Temperature Ratings
|
Pipe Size |
Sch 40S @ 100°C |
Sch 80S @ 200°C |
Max Pressure (ANSI 300#) |
|
2" |
290 psi |
750 psi |
720 psi @ 38°C |
F316 vs. Competing Alloys
|
Alloy |
Mo Content |
PREN |
Chloride Limit |
Cost vs F316 |
|
F316 |
2-3% |
24.5 |
500 ppm |
Baseline |
|
F304 |
0% |
18.5 |
200 ppm |
15% lower |
|
Duplex 2205 |
3-3.5% |
35+ |
5,000 ppm |
40% higher |
|
Alloy 625 |
8-10% |
50+ |
Unlimited |
300% higher |
F316 vs. F316L: Which to Choose?
- F316L (UNS S31603) has ≤0.03% carbon - essential for:
- Welded assemblies >400°C (prevents carbide precipitation)
- Oxalic acid/Caustic services
- Standard F316 preferred for:
- High-temperature strength (>500°C)
- Non-welded fittings (flanges, threaded couplings)
FAQ
Q: Can F316 fittings handle seawater?
A: Yes, up to 30°C with flow >1.5 m/s. For stagnant/severe service, upgrade to super duplex.
Q: Are F316 fittings magnetic?
A: Minimally (permeability <1.02) due to austenitic structure. Cold working may increase magnetism.
Q: What's the lead time for custom F316 fittings?
A: 4-8 weeks for non-stock sizes; specify NDE requirements (RT/UT/PT) upfront.