Monel 400 Nipple

Jul 01, 2025

Leave a message

Monel 400 One End Threaded Nipple, Monel UNS N04400 Both End Threaded Nipple Exporter, Monel 400 Nipple, Monel WERKSTOFF NR. 2.4360 Nipple Exporter in China. ASTM B564 Monel 400 Nipple, ANSI B16.11 Monel 400 Hexagon Reducing Nipple, 400 Monel Hexagoan Nipple Supplier and Manufacturer.


Jinie Technology (Jiangsu) Co., LTD is one of the pioneer supplier and manufacturer of quality Monel Alloy 400 Nipple, where we provide these products at very competitive price to our clients. Offered Monel 400 Hexagon Reducing Nipple is manufactured using optimum quality stainless steel and latest technology by vendors' skilled professionals. Besides, Monel 400 Hexagon Nipple is made available in various sizes and shapes. Monel 400 One End Threaded Nipple is highly appreciated among our clients for their precise design and durability. As would be expected from its high copper content, Monel 400 Concentric Swaged Nipple is rapidly attacked by nitric acid and ammonia systems. Monel 400 Eccentric Swaged Nipple is a precipitation – hardenable nickel – copper alloy that combines the excellent corrosion resistance characteristic with the added advantage of hardness and greater strength. These amplified properties of strength and hardness in Alloy 400 Hexagon Reducing Nipple is obtained by adding titanium and aluminium to the nickel – copper base and by a thermal processing used to effect precipitation, typically called age hardening or aging. Our Alloy 400 One End Threaded Nipple can be further strengthened by cold working prior to precipitation hardening.

 

Monel 400 Forged Nipple Specification

Specifications

ASTM B564/ ASME SB564

Dimension Specification

ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799

Monel 400 Forged Fittings Thread

NPT, BSPT, BSPP

Monel 400 FittingsType

DN15-DN1200

End

Threaded, Welding, JIC

Monel 400 Forged Fittings Pressure Rating

Threaded end-2000lb/ 3000lb/ 6000lbs Pipe Fittings
Socket-weld end-3000/ 6000/ 9000lbs Pipe Fittings

Connection

Welding

Bending Radius

R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom Pipe Fittings

Size Range

½" NB to 24" NB in Sch 10s, 40s, 80s, 160s, XXS. (DN6~DN100)

Manufacturing process

Push, Press, Forge, Cast, etc.

Monel 400 Threaded Fittings Test Certificates

EN 10204/3.1B
Raw Materials Certificate
100% Radiography Test Report
Third Party Inspection Report, etc

Key markets and industries for Monel 400 Forged Fittings

Bitumen upgraders.

Heavy oil refineries.

Nuclear power (mostly seamless).

Petrochemicals and acids.

Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2, Test Certificates certifying NACE MR0103, NACE MR0175

 

Monel 400 Nipple Price List

Alloy 400 Nipple

US $0.2-25 / Piece (FOB Price)

Monel 400 Nipple

US $0.2-25 / Piece (FOB Price)

Monel Nipple

US $0.2-25 / Piece (FOB Price)

ASTM B366 Monel 400 Nipple

US $0.2-25 / Piece (FOB Price)

 

ASME B16.11 Monel Alloy 400 Size Chart

Pipe Nipple Size Chart

Nom.Pipe
Size (in)

0.D.

Average
I.D.

Min.
Wall

Nominal
Wt./Ft.

Maximum
W.P.PSI*

1/8

0.405

0.249

0.068

0.051

810

1/4

0.540

0.344

0.088

0.086

780

3/8

0.675

0.473

0.091

0.115

620

1/2

0.840

0.602

0.109

0.170

600

3/4

1.050

0.804

0.113

0.226

480

1

1.315

1.029

0.133

0.333

450

1-1/4

1.660

1.360

0.140

0.450

370

1-1/2

1.900

1.590

0.145

0.537

330

2

2.375

2.047

0.154

0.720

280

2-1/2

2.875

2.445

0.203

1.136

300

3

3.500

3.042

0.216

1.488

260

3-1/2

4.000

3.521

0.226

1.789

240

4

4.500

3.998

0.237

2.118

220

5

5.563

5.016

0.258

2.874

190

6

6.625

6.031

0.280

3.733

180

8

8.625

7.942

0.322

5.619

160

10

10.750

9.976

0.365

7.966

140

12

12.750

11.889

0.406

10.534

130

14

14.000

13.073

0.437

12.462

130

16

16.000

14.940

0.500

16.286

130

18

18.000

16.809

0.562

20.587

130

20

20.000

18.743

0.593

24.183

120

24

24.000

22.544

0.687

33.652

120

 

Application of Monel 400 Pipe Nipple

Monel 400 Pipe nipples are used in different settings. Here's where you'll typically find them:

Plumbing: The most common area where Monel 400 pipe nipples are found is plumbing in a residential or commercial building. Such nipples work as connectors for pipe systems that service water supply, waste removal, or other similar functions requiring dependable and leak-free connections.

Industrial Pipelines: In industrial settings, Monel 400 pipe nipples are used to connect industrial pipelinescarrying either chemical, gas, or liquid. They are strong and durable, so it is very important in these venues where it is expected that the pipe fittings will be under extremely high pressure and subjected to harsh materials.

 

Electrical Boxes: Monel 400 Pipe nipples electrically connect conduit pipes to electrical boxesor panels in electrical installation. Its purpose is to serve as a bridge between the electrical conduit pipe and the box.

 

Kitchen Tap Pipes: One major area of application is in kitchen plumbing as part of the processes established to connect water pipes to kitchen tap pipes. The work of a Monel 400 pipe nipple in aplumbing system includes making sure that the water flows accordingly to faucets or other fixtures. Those are a few examples; however, Monel 400 pipe nipples can be found somewhere almost everywhere systems connect pipes. They are very comprehensive and flexible and constitute a good need in most industries.

 