ASTM B366 Inconel Alloy 601 Elbow, ASME SB366 Inconel 601 90 deg Elbow, UNS N06601 45 deg Elbow, 2.4851 180 Deg Buttweld Elbow, Nickel Alloy 601 Seamless Pipe Elbow Exporter, ANSI B16.9 Inconel 601 Buttweld Elbow Supplier, Inconel 601 Welded Elbow Manufacturer in China.
Jinie Technology (Jiangsu) Co., LTD offers a wide range of Inconel 601 Butt Weld Pipe Fittings which is manufactured at par with the international quality standards by making use of high-grade metals and alloys. The outstanding characteristic of these Inconel UNS N06601 Elbow is its resistance to high-temperature oxidation. Our Inconel 601 Long Radius Elbow Butt Weld Pipe Fittings retains its ductility after long service exposure and are quite popular known as an engineering material. These Inconel 601 Short Radius Elbow Butt Weld Pipe Fittings is construction alloy for heat treat furnace fixtures and components such as annealing tubes, muffles, and flame shields. Our Inconel 601 Butt Weld Elbow are used in petrochemical and other process equipment. High – speed operations such as grinding, milling or turning, are performed in these Inconel 601 Elbow using water-based coolants.
Inconel 601 Buttweld Elbow Specifications
|
Specifications |
ASTM B366 / ASME SB366 |
|
Size |
Seamless Butt Weld Fittings: 1/2″ – 10″, Welded Butt Weld Fittings: 1/2″ – 48″ |
|
Standards |
ASME/ANSI B16.9, ASME B16.28, MSS-SP-43 |
|
Thickness |
5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
|
Type |
Seamless / Welded / Fabricated |
Types of UNS N06601 Inconel Alloy 601 Buttweld Elbow and other Fittings
|
Available Size – 1/4" NB TO 32" NB. (Seamless & Welded) |
||
|
Inconel Alloy 601 Reducers |
Inconel Alloy 601 Concentric Reducers |
Inconel Alloy 601 Tees |
|
Inconel Alloy 601 Pipe Nipples |
Inconel 601 Stub end |
Alloy 601 Fitting Tees |
|
Inconel Alloy 601 Elbows |
601 Alloy 3D Elbow |
Inconel Alloy 601 Stub Ends |
|
UNS N06601 Inconel End Caps |
Inconel 601 5D Elbow |
601 Alloy 180° SR Return Bends |
|
Inconel 601 Long Radius Elbow |
Alloy 601 Eccentric Reducers |
Inconel Alloy 601 Reducing Crosses |
|
Inconel Alloy 601 Elbows |
601 Inconel Alloy Crosses |
Inconel Alloy 601 Couplings |
|
Inconel 601 Short Radius Elbow |
601 Alloy ASME B16.9 Pipe Bends |
601 Inconel 45° Elbows |
|
Inconel Alloy 601 Reducing Elbow |
601 Inconel Alloy Piggable Bends |
601 Alloy 180° LR Return Bends |
|
UNS N06601 Inconel Welded Fittings |
Inconel 601 Seamless Fittings |
601 ASTM A366 Butt weld Fittings |
|
Inconel 601 Pipe Fittings |
Inconel Alloy 601 Pipe Fittings |
Alloy 601 Welded Pipe Fittings |
Dimensions of Inconel 601 Pipe Elbows
|
Nominal |
Outside |
90° Elbows |
45° Elbows |
180° Returns |
||||
|
(inches) |
Long Radius |
Short Radius |
Long Radius |
Long Radius |
||||
|
(mm) |
(inches) |
Center to Face |
Center to Face |
Center to Face |
Radius |
Center to Center |
Back to face |
|
|
1/2 |
21.3 |
0.840 |
1 1/2 |
– |
5/8 |
2 |
1 7/8 |
|
|
3/4 |
26.7 |
1.050 |
1 1/8 |
– |
7/16 |
2 1/4 |
1 11/16 |
|
|
1 |
33.4 |
1.315 |
1 1/2 |
1 |
7/8 |
3 |
2 3/16 |
|
|
1 1/4 |
42.2 |
1.660 |
1 7/8 |
1 1/4 |
1 |
3 3/4 |
2 3/4 |
|
|
1 1/2 |
48.3 |
1.900 |
2 1/4 |
1 1/2 |
1 1/8 |
3 |
4 1/2 |
3 1/4 |
|
2 |
60.3 |
2.375 |
3 |
2 |
1 3/8 |
4 |
6 |
4 3/16 |
|
2 1/2 |
73.0 |
2.875 |
3 3/4 |
2 1/2 |
1 3/4 |
5 |
7 1/2 |
5 3/16 |
|
3 |
88.9 |
3.500 |
4 1/2 |
3 |
2 |
6 |
9 |
6 1/4 |
|
3 1/2 |
101.6 |
4.000 |
5 1/4 |
3 1/2 |
2 1/4 |
7 |
10 1/2 |
7 1/4 |
|
4 |
114.3 |
4.500 |
6 |
4 |
2 1/2 |
8 |
12 |
8 1/4 |
|
5 |
141.3 |
5.563 |
7 1/2 |
5 |
3 1/8 |
10 |
15 |
10 5/16 |
|
6 |
168.3 |
6.625 |
9 |
6 |
3 3/4 |
12 |
18 |
12 5/16 |
|
8 |
219.1 |
8.625 |
12 |
8 |
5 |
12 |
24 |
16 5/16 |
|
10 |
273.1 |
10.750 |
15 |
10 |
6 1/4 |
15 |
30 |
20 3/8 |
|
12 |
323.9 |
12.750 |
18 |
12 |
7 1/2 |
18 |
36 |
24 3/8 |
Industrial Applications of Inconel 601 Elbow
Industrial Heating and Thermal Processing
Inconel 601 Pipe Elbow is extensively used in industrial heating and thermal processing due to its excellent high-temperature properties. Components include radiant tubes, muffles, retorts, flame shields, strand-annealing tubes, baskets, trays, and fixtures. These components are crucial in processes like annealing, carburizing, carbonitriding, and nitriding, where materials are handled at elevated temperatures.
Chemical Processing
Inconel 601 Elbow resistance to corrosion and high temperatures makes it ideal for chemical processing applications, including process heaters, condenser tubes, insulating cans in ammonia reformers, catalyst regenerators, and air preheaters. These components are essential in processes like sour-water stripping and high-density polyethylene production, where high-temperature stability is critical.
Aerospace
The aerospace industry relies on Inconel 601 for high-performance parts like jet engine components, including combustor parts and turbine blades, as well as gas turbine components. These parts must withstand extreme thermal and mechanical stresses, making the alloy's durability and resistance to high temperatures invaluable.
Oil and Gas
Inconel 601 Elbow are crucial in oil and gas exploration and processing, particularly in high-temperature and high-pressure environments. Their strength and corrosion resistance make them suitable for refineries, offshore platforms, and subsea pipelines.
Marine Engineering
Marine environments are especially harsh, with challenges like saltwater corrosion and extreme pressure. Inconel 601 Elbow are used in seawater applications, such as desalination plants and offshore structures, for their exceptional resistance to chloride-induced corrosion.