What is ASTM A105 Flange?
ASTM A105 flanges, forged from carbon steel, are suitable for industrial high-pressure and high-temperature environments. Carbon steel flange dimensions are specified by standards such as ASME B16.5/ASME B16.47. Jinie is a manufacturer and supplier of A105N flanges. We can customize sizes according to customer requirements.

Factory A105 Carbon Steel Flanges Manufacturers, A105 Forged Steel Flanges Suppliers, Contact us to get price list, Customized Sizes & Free Sample!
Types of A105 Flanges
Weld Neck Flange (WN)
Slip-On Flange (SO)
Blind Flange (BL)
Socket Weld Flange (SW)
Lap Joint Flange (LJ)
Threaded Flange (THD)
Orifice Flanges
Spectacle Blind Flanges
A105N Flange Specifications
|
Specifications |
ASTM A105, ASTM A105N, ASME SA105 |
|
Size |
1/2″ to 60″, DN6-DN4000 |
|
Standards |
ANSI B16.47 Series A & B, ANSI B16.5 |
|
Pressure Ratings |
Class 150, Class 300, Class 400, Class 600, Class 900, Class 1500, Class 2500 |
|
Flange Face Type |
Flate Face, Raised Face, Ring Type Joint |
|
Coating/Surface Treatment |
Oil Black Paint, Anti-rust Paint, Cold and Hot Dip Galvanized, Zinc Plated. |
ASTM A105 Pipe Flanges Chemical Composition
|
Element |
Carbon (C) |
Manganese (Mn) |
Phosphorus (P) |
Sulfur (S) |
Silicon (Si) |
Copper (Cu) |
Nickel (Ni) |
Chromium (Cr) |
Molybdenum (Mo) |
Vanadium (V) |
|
Composition (%) |
0.35 max |
0.60 - 1.05 |
0.035 max |
0.040 max |
0.10 - 0.35 |
0.40 max |
0.40 max |
0.30 max |
0.12 max |
0.08 max |
ASTM A105N Mechanical Properties Flanges
|
Tensile Strength |
Yield Strength |
Elongation |
Reduction of Area |
Hardness (Brinell) |
|
70 ksi (485 MPa) min |
36 ksi (250 MPa) min |
22% min (in 2in / 50mm) |
30% min |
187 HB max |
ASTM A105 Flange Pressure-Temperature Ratings
|
Temp. °C |
Working Pressure by Classes, bar |
||||||
|
150 |
300 |
400 |
600 |
900 |
1500 |
2500 |
|
|
-29 ~ 38 |
19.6 |
51.1 |
68.1 |
102.1 |
153.2 |
255.3 |
425.5 |
|
50 |
19.2 |
50.1 |
66.8 |
100.2 |
150.4 |
250.6 |
417.7 |
|
100 |
17.7 |
46.6 |
62.1 |
93.2 |
139.8 |
233 |
388.3 |
|
150 |
15.8 |
45.1 |
60.1 |
90.2 |
135.2 |
225.4 |
375.6 |
|
200 |
13.8 |
43.8 |
58.4 |
87.6 |
131.4 |
219 |
365 |
|
250 |
12.1 |
41.9 |
55.9 |
83.9 |
125.8 |
209.7 |
349.5 |
|
300 |
10.2 |
39.8 |
53.1 |
79.6 |
119.5 |
199.1 |
331.8 |
|
325 |
9.3 |
38.7 |
51.6 |
77.4 |
116.1 |
193.6 |
322.6 |
|
350 |
8.4 |
37.6 |
50.1 |
75.1 |
112.7 |
187.8 |
313 |
|
375 |
7.4 |
36.4 |
48.5 |
72.7 |
109.1 |
181.8 |
303.1 |
|
400 |
6.5 |
34.7 |
46.3 |
69.4 |
104.2 |
173.6 |
289.3 |
|
425 |
5.5 |
28.8 |
38.4 |
57.5 |
86.3 |
143.8 |
239.7 |
|
450 |
4.6 |
23 |
30.7 |
46 |
69 |
115 |
191.7 |
|
475 |
3.7 |
17.4 |
23.2 |
34.9 |
52.3 |
87.2 |
145.3 |
|
500 |
2.8 |
11.8 |
15.7 |
23.5 |
35.3 |
58.8 |
97.9 |
|
538 |
1.4 |
5.9 |
7.9 |
11.8 |
17.7 |
29.5 |
49.2 |
Advantages of A105 Carbon Flanges

High Strength and Durability
High Temperature Resistance: Operates from -29°C to 425°C
Corrosion Resistance: A105 flanges can withstand corrosion through coatings or linings.
Low Cost: Carbon steel raw materials (iron and carbon) are significantly less expensive than stainless steel or nickel alloys.
ASTM A105 VS ASTM A350 LF2
A350 LF2 is a carbon steel alloy suitable for low-temperature environments (down to -46°C / -50°F).
A105 is suitable for environments ranging from ambient to high-temperature, high-pressure environments.
Carbon Steel Flanges Manufacturers Fabrication
Raw materials → Heating → Forging → Heat treatment → Machining → Surface treatment → Inspection and testing → Marking and packaging
A105 Carbon Steel Flanges Testing
Dimensional inspection
Materials chemical analysis using spectrometers
Tensile and impact testing
Magnetic particle inspection
Ultrasonic testing
ASTM A105 Flange Manufacturer
Jinie is a well-known stockist and exporter. We are a carbon steel material supplier with 20+ export experience. We not only provide pipes, plates, round bars, but also pipe fittings, flanges, etc.
Contact us for more information and prices for free.