ASME B16.11 Hastelloy B2 Union

Jul 05, 2025

Leave a message

ASME B16.11 Hastelloy B2 Union, Hastelloy Alloy B2 Union, Hastelloy UNS 10665 Socket Weld Union, Hastelloy Din204617 Forged Socket Weld Union, Hastelloy Alloy B2 High Pressure Forged Union, Hastelloy B2 Screwed Union, Hastelloy Alloy Threaded Union, ASTM B564 B2 Hastelloy Forged Union Manufacturer in China.

 

Hastelloy B2 Union (UNS N10665) is a nickel – molybdenum alloy with significant resistance to reducing environments, such as hydrogen chloride gas and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element in Hastelloy B2 Union which provides significant corrosion resistance to reducing environments. Hastelloy B2 Union controls other alloying elements such as iron and chromium solved other issues concerning fabricability. Additionally, Hastelloy B2 Union has good stress corrosion cracking and pitting resistance as well. Reliable, cost effective and practical solutions to corrosion weld problems involve the use of Alloy B2 Union filler metal. Alloy B2 Union Tube Fittings suffered unusually severe base metal, weld metal, and heat affected zone attack in this particular environment. Alloy B2 Union is generally stiffer than the austenitic stainless steels, and therefore, more energy is required during cold forming. Meanwhile, there was minimal corrosion attack on the sample of Alloy B2 Union.

 

Jinie Technology (Jiangsu) Co., LTD is a prominent manufacturing firm that produces and supplies the highest quality Hastelloy B2 Union. We have earned name and fame in the field of manufacturing and supply product to the client from the domestic and global market. For the production of Hastelloy B2 Union, we take the guidance and valuable insights from our experts. We manufacture and supply the Hastelloy B2 Union by using supreme quality raw material in the form of Hastelloy. For the production of products, we have a team of skilled manufacturing experts, designers, and quality analysts. They ensure product superiority, quality and desired quantity of Hastelloy B2 Union to match the demand of our client.

 

Hastelloy B2 Union Specifications

Standards

ASTM B564 / ASME SB564

Size Range

1/16″OD to 2″OD, 2mm OD to 50mm OD

Thread

NPT, BSP, BSPT, UNF, ISO, SAE etc.

End

Threaded, Welding, JIC

Pressure Rating

1000 Psi, 3000 Psi, 6000 Psi, 10000 Psi

Type

Single Ferrule tube fitting, Double Ferrule tube fitting, Hydraulic tube fitting, Instrumentation tube fitting

 

Types of Hastelloy B2 Union

Hastelloy B2 Union Tee

Hastelloy Alloy B2 Union Tee
B2 Hastelloy Alloy Union Tee
Hastelloy B2 Union Tee
B2 Hastelloy Alloy Parker Union Tee
Hastelloy Alloy UNS N10665 Union Tee
B2 Hastelloy Alloy Swagelok Union Tee
Hastelloy WERKSTOFF NR. 2.4617 Union Tee
ASME SB564 B2 Alloy Union Tee

Hastelloy B2 Reducing Union

Hastelloy Alloy B2 Reducing Union
B2 Hastelloy Alloy Reducing Union
Hastelloy B2 Reducing Union
Hastelloy B2 Swagelok Reducing Union
Hastelloy Alloy UNS N10665 Reducing Union
B2 Hastelloy Alloy Parker Reducing Union
Hastelloy WERKSTOFF NR. 2.4617 Reducing Union
ASTM B564 B2 Alloy Reducing Union

Hastelloy B2 Bulkhead Union

Hastelloy Alloy B2 Bulkhead Union
B2 Hastelloy Alloy Bulkhead Union
Hastelloy B2 Bulkhead Union
B2 Hastelloy Alloy Swagelok Bulkhead Union
Hastelloy B2 Parker Bulkhead Union
Hastelloy Alloy UNS N10665 Bulkhead Union
Hastelloy WERKSTOFF NR. 2.4617 Bulkhead Union
ASTM B564 B2 Alloy Bulkhead Union

Hastelloy B2 Tube to Union

Hastelloy Alloy B2 Tube to Union
B2 Hastelloy Alloy Tube to Union
Hastelloy B2 Tube to Union similar to parker and swagelok
Hastelloy Alloy UNS N10665 Tube to Union
Hastelloy WERKSTOFF NR. 2.4617 Tube to Union
B2 ASME SB564 Alloy Tube to Union

Hastelloy B2 Union Elbow

Hastelloy Alloy B2 Union Elbow
Hastelloy B2 Union Elbow
B2 Hastelloy Union Elbow
Hastelloy Alloy UNS N10665 Union Elbow
Hastelloy B2 Swagelok Union Elbow
Hastelloy WERKSTOFF NR. 2.4617 Union Elbow
ASTM B564 B2 Alloy Union Elbow

Hastelloy B2 Union Cross

Hastelloy Alloy B2 Union Cross
B2 Hastelloy Alloy Union Cross
Hastelloy B2 Union Cross
Hastelloy Alloy UNS N10665 Union Cross
Hastelloy WERKSTOFF NR. 2.4617 Union Cross
ASTM B564 Alloy Union Cross

 

Hastelloy B2 Union Price List

B2 Hastelloy Alloy Tube To Union

US $1-5 / Piece (FOB Price)

Hastelloy Alloy B2 Union Tee

US $0.07 / Piece

Hastelloy B2 Union Elbow

US $0.01-3 / Piece (FOB Price)

ASTM B366 B2 Hastelloy Reducing Union

US $0.1-0.2 / Piece (FOB Price)

ASME SB366 Alloy B2 Bulkhead Union

US $0.01-2 / Piece (FOB Price)

Hastelloy UNS N10665 Union Cross

US $0.02-4 / Piece (FOB Price)

DIN 2.4617 Hastelloy Alloy Bulkhead Union

US $2-6 / Piece (FOB Price)

 

Hastelloy Alloy B2 Union Application Industries

Off-Shore Oil Drilling Companies

Power Generation

Petrochemicals

Gas Processing

Specialty Chemicals

Pharmaceuticals

Pharmaceutical Equipment

Chemical Equipment

Sea Water Equipment

Heat Exchangers

Condensers

Pulp and Paper Industry

 

Send Inquiry
Come To Us
And Start Your RFQs Now.
contact us