321 Stainless Steel Sheet

Nov 28, 2025

Leave a message

321 stainless steel sheet is a titanium-stabilized material with corrosion resistance comparable to 304/304L stainless steel. SS 321 material is commonly used in high-temperature applications ranging from 800 to 1500°F. Additionally, 1.4541 stainless steel incorporates titanium to inhibit chromium carbide formation, delivering excellent intergranular corrosion resistance. Our supplier-manufacturer maintains stock of 321 sheet in various dimensions, certified to AMS 5510 and ASTM A240.

 

321 stainless steel sheet

 

Contact us for further details and price!

 

321 Stainless Steel Data Sheet Specification

 

Specification

ASTM A240 / ASME SA240 / AMS 5510

Manufacturing

Hot Rolled (HR) / Cold Rolled (CR)

Thickness

0.6 MM TO 80 MM THICKNESS

Width

1250 MM / 1500 MM / 2000 MM

Length

2400 MM / 2420 MM / 6000 MM

Surface Finish

2B, 2D, BA, No.4, No.5, HR, CR, No.8, Mirror, Hairline

Testing

NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test, Charpy Impact Test, Macro, Grain Size, Hardness, etc.

Certificate

Manufacturer Test Certificate As Per EN10204 3.1, 3.2
Under Third Party Inspection SGS, TUV, DNV, LLOYDS, ABS
ISO9001

 

1.4541 AISI 321 Stainless Steel Composition

 

Element

Chromium

Nickel

Carbon

Manganese

Phosphorus

Sulfur

Silicon

Titanium

Nitrogen

Iron

321

17.00 min.-19.00 max.

9.00 min.-12.00 max.

0.08

2

0.045

0.03

0.75

5 x (C + N) min.-0.70 max.

0.1

Balance

 

321 ASME SA 240 Plate Mechanical Properties

 

Property

Density

Yield Strength, min. (ksi)

Tensile Strength, min. (ksi)

Elongation, min. (%)

Hardness, max. (Rb)

321

7.920 g/cm3

30

75

40

95

 

1.4541 Material Equivalent

 

Grade

UNS

Old British

Euronorm

Swedish SS

Japanese JIS

BS

En

No

Name

321

S32100

321S31

58B, 58C

1.4541

X6CrNiTi18-10

2337

SUS 321

 

Thickness Of Stainless Steel Sheet Metal

 

Thickness Range: 0.1mm – 6.0mm

 

Width & Length: 1000×2000mm, 1220×2440mm (4'×8'), 1220×3050mm, 1500×3000mm, 1500×6000mm

 

Ams 5510 321 Cres Sheet Applications

 

Aerospace, Aircraft Exhaust Manifolds

 

Industrial Furnaces

 

Heat Exchanger Components

 

Thermal Oxidizer Assemblies

 

Chemical Processing

 

Expansion Joints

 

Furnace Components

 

Heat Exchangers

 

SS 321 Stainless Steel Weldability

 

SS 321 Stainless Steel Weldability

 

321 SS has excellent weldability and does not require post-weld solution annealing. Use ER321 or ER347 filler metal.

 

Manual Metal Arc Welding (SMAW)

 

Gas Metal Arc Welding (GMAW/MIG)

 

Gas Tungsten Arc Welding (GTAW/TIG)

 

Submerged Arc Welding (SAW)

 

Plasma Arc Welding (PAW)

 

AISI 321 Stainless Steel Machinability

 

321 ss sheet has moderate machinability, slightly inferior to 304. It exhibits a high tendency for work hardening.

 

Customer Purchase Cases

 

Please provide your best price and availability for the below requirement.

 

Material grade: ALloy 321 / 1.4541 / s32100

 

Specification: 100 sheets of 3mm thickness

 

Specification: 200 sheet of 6mm thickness

 

Please also share the delivery time and relevant Mill Test Certificates (MTC) for verification.

 

Stainless Steel 321 Vs 304

 

321 stainless steel has added Ti and is designed for high temperatures; while 304 stainless steel is suitable for medium-temperature environments and is less expensive.

 

1.4571 vs 1.4541

 

1.4571 (316Ti) contains Mo and is more resistant to chloride and acidic environments. 1.4541 (321), while, is more suitable for environments with lower corrosiveness.

 