Our company has built a reputation for excellence through innovative manufacturing processes, stringent quality controls, and a customer-focused approach. We specialize in producing high-performance alloys that withstand extreme environments, and our Inconel 600 flanges exemplify this commitment. Certified under ISO 9001, ISO 14001, OHSAS 18001, and PED 97/23/EC, we ensure every product delivers unmatched reliability, durability, and value.

In this article, we explore the attributes that position our Inconel 600 flanges as the best in the market.
Inconel 600, designated as UNS N06600 or Alloy 600, is a nickel-chromium-iron superalloy engineered for exceptional resistance to oxidation, corrosion, and high-temperature.
Features and Benefits of Our Inconel 600 Flanges
Inconel 600 flange's high nickel content (minimum 72%) imparts outstanding resistance to reducing and oxidizing atmospheres, while chromium enhances oxidation resistance up to 2000°F (1093°C). These flanges maintain dimensional stability across cryogenic to elevated temperatures, preventing warping or failure in cyclic heating conditions.
Compelling benefits include:
Superior Corrosion Resistance: Excels in harsh chemical environments, resisting pitting, crevice corrosion, and intergranular attacks.
High-Temperature Strength: Retains mechanical integrity in extreme heat, ideal for furnaces and heat exchangers.
Ease of Fabrication: Welds readily without special treatments, facilitating quick assembly and repairs.
Longevity and Cost-Effectiveness: Minimizes downtime and replacement needs, offering a lower total cost of ownership.
By selecting our flanges, clients gain a persuasive edge in performance, supported by our expertise in alloy optimization and custom solutions.
Types of Inconel 600 Flanges We Manufacture
We offer an extensive portfolio of Inconel 600 flange types, each designed for specific operational demands and compliant with ASTM B564 / ASME SB564 standards. Our range ensures versatility for any piping configuration:

Weld Neck Flanges (WNRF): Provide excellent stress distribution for high-pressure systems.
Slip-On Flanges (SORF): Economical and easy to install for moderate-pressure applications.
Blind Flanges (BLRF): Seal pipe ends securely for isolation or testing.
Socket Weld Flanges (SWRF): Ensure leak-proof connections in small-diameter, high-pressure lines.
Threaded Flanges: Suitable for non-welded setups in low-pressure environments.
Lap Joint Flanges: Allow for easy alignment and disassembly.
Orifice Flanges: Facilitate accurate flow measurement.
Ring Type Joint Flanges (RTJ): Offer high-integrity sealing in critical services.
Spectacle Blind Flanges: Enable quick pipeline isolation during maintenance.
Reducing Flanges: Adapt to varying pipe sizes efficiently.
Long Weld Neck Flanges: Ideal for vessels and equipment nozzles.
Expander Flanges: Transition to larger pipe diameters seamlessly.
High Hub Blind Flanges: Enhanced for high-pressure blind applications.
Groove & Tongue Flanges: Provide precise mating for specialized joints.
Square Flanges: Custom for unique structural needs.
Spades Ring Spacers Flanges: Support maintenance in large systems.
Flat Flanges: Simple and effective for low-pressure uses.
Loose Flanges: Flexible for rotating equipment.
We also produce forged, screwed, and weldo/nipo flanges, available in sizes from 1/2" NB to 48" NB, with custom options to match precise requirements.
Inconel 600 Specifications and Standards

Our Inconel 600 flanges adhere to global benchmarks for quality and interoperability:
Standards: ASTM B564 / ASME SB564, ANSI/ASME B16.5, B16.47 Series A & B, B16.48, BS4504, BS 10, EN-1092, DIN.
Pressure Ratings: Class 150# to 2500#, PN6 to PN64.
Flange Face Types: Flat Face (FF), Raised Face (RF), Ring Type Joint (RTJ).
Size Range: 1/2" (15 NB) to 48" (1200 NB).
These specifications ensure seamless integration into diverse systems, from ASME B16.36 orifice designs to API 6A high-pressure applications.
Inconel 600 Chemical Composition
The alloy's composition is finely tuned for peak performance:
|
Element |
Content (%) |
|
Nickel (Ni) |
72.00 min |
|
Chromium (Cr) |
14.00 - 17.00 |
|
Iron (Fe) |
6.00 - 10.00 |
|
Carbon (C) |
0.15 max |
|
Manganese (Mn) |
1.00 max |
|
Silicon (Si) |
0.50 max |
|
Sulfur (S) |
0.015 max |
|
Copper (Cu) |
0.50 max |
This balance delivers exceptional resistance to environmental degradation.
Inconel 600 Mechanical Properties
Inconel 600 flanges boast impressive mechanical attributes:
|
Property |
Value |
|
Density |
8.47 g/cm³ |
|
Melting Point |
1413°C (2580°F) |
|
Tensile Strength |
655 MPa (95,000 psi) |
|
Yield Strength (0.2% Offset) |
310 MPa (45,000 psi) |
|
Elongation |
40% |
These properties guarantee resilience in high-stress scenarios.
Inconel 600 Pressure Ratings
Our flanges maintain integrity across temperature ranges, as shown in this pressure rating table (in psi):
|
Temp (°F) |
150# |
300# |
400# |
600# |
900# |
1500# |
2500# |
|
-20 to 100 |
275 |
720 |
960 |
1440 |
2160 |
3600 |
6000 |
|
200 |
230 |
600 |
800 |
1200 |
1800 |
3000 |
5000 |
|
400 |
190 |
495 |
660 |
995 |
1490 |
2485 |
4140 |
|
600 |
140 |
435 |
580 |
875 |
1310 |
2185 |
3640 |
|
800 |
80 |
405 |
540 |
805 |
1210 |
2015 |
3360 |
|
1000 |
20 |
320 |
430 |
640 |
965 |
1605 |
2675 |
|
1200 |
20 |
155 |
205 |
310 |
465 |
770 |
1285 |
|
1400 |
20 |
50 |
65 |
95 |
145 |
240 |
400 |
This data underscores their suitability for high-pressure operations.
Inconel 600 Equivalent Grades
For international compatibility:
|
Standard |
Designation |
|
UNS |
N06600 |
|
Werkstoff Nr. |
2.4816 |
|
EN |
NiCr15Fe |
|
JIS |
NCF 600 |
|
BS |
NA 13 |
|
GOST |
МНЖМц 28-2,5-1,5 |
|
AFNOR |
NC15FE11M |
These equivalents facilitate global sourcing without compromise
Inconel 600 Flange Applications

Our Inconel 600 flanges excel in industries such as:
Chemical and Petrochemical: Resisting corrosive fluids in processing plants.
Aerospace: Components for jet engines and airframes.
Oil and Gas: Pipelines and wellheads in harsh offshore environments.
Power Generation: Nuclear reactors and heat exchangers.
Marine Engineering: Seawater-resistant fittings.
Pulp and Paper: Handling aggressive chemicals.
Food Processing: Maintaining hygiene in acidic conditions.
Heat Treating: Furnace parts like retorts and muffles.
Proven in real-world scenarios, they enhance safety and efficiency across sectors.
Quality Assurance and Certifications
Quality is paramount at Jinie Products. Each flange undergoes comprehensive testing, including radiography, ultrasonic inspection, and third-party verification. We provide EN 10204 3.1/3.2 certificates, material test reports, and NABL-approved lab results.
Products are marked with essential details and packaged securely for worldwide shipment, with HS Code 75072000 for efficient customs clearance.