Stainless Steel 316H features
Stainless Steel Grade 316H is a higher carbon variation of 316 making the steel more suitable for use in applications where high temperatures are available. Balanced Grade 316Ti offers comparable qualities. The expanded carbon content delivers a greater tensile and yield strength. The austenitic structure of the material also gives this grade excellent toughness, even down to cryogenic temperatures.
316H is very suitable for use at high temperatures, has excellent corrosion resistance when exposed to various corrosive environments and media, and has good machinability and good weldability.
Stainless steel 316H Chemical Composition,%
|
Grade |
C |
Si≤ |
Mn≤ |
P≤ |
S≤ |
Cr |
Mo |
Ni |
|
316H |
0.04--0.10 |
0.75 |
2.00 |
0.045 |
0.030 |
16.00--18.00 |
2.00--3.00 |
10.00--14.00 |
Stainless steel 316H Mechanical Properties
|
Grade |
Yield |
Tensile Strength |
Elongation |
Hardness Max,HB |
|
316H |
205 |
515 |
40 |
217 |
Physical properties
Density: 7.98 g/cm3
Stainless steel 316H Equivalent Grades
|
STANDARD |
UNS |
EN |
WERKSTOFF NR. |
|
316H |
S31609 |
X6CrNiMO17-13 |
1.4919 |
ASTM SPECIFICATION
|
Pipe, |
Tube , |
Sheet/Plate |
Bar /Rod |
Forging /Flange |
BW Fittings |
|
ASTM A312 |
ASTM A213/ASTM A269 |
ASTM A240 |
ASTM A276/A479 |
ASTM A182 |
ASTM A403 |
SS 316H Application
- Food preparation equipment, especially in chloride environments
- Chemical processing, equipment
- Laboratory benches and equipment
- Rubber, plastics, pulp & paper machinery
- Pollution control equipment
- Boat fittings, value and pump trim
- Heat exchangers
- Pharmaceutical and textile industries
- Condensers, evaporators and tanks
Hot Tags: stainless steel 316h / uns 31609 / 1.4919, China stainless steel 316h / uns 31609 / 1.4919 manufacturers, suppliers, alloy inventory, alloy price, alloy specialized alloy, alloy innovative alloy, alloy growth opportunity, alloy sand casting