Stainless steel AL6XN Characteristics
AL6XN (UNS N08367) is a super austenitic stainless steel with outstanding resistance to chloride pitting, crevice corrosion and stress corrosion cracking. AL6XN is a 6 moly alloy that was developed for and is used in highly aggressive environments. It has high nickel (24%), molybdenum (6.3%), nitrogen and chromium contents that give it excellent resistance to chloride stress corrosion cracking, chloride pitting, and exceptional general corrosion resistance. AL6XN is primarily used for its improved pitting and crevice corrosion resistance in chlorides. It is a formable and weldable stainless steel.
AL6XN Super austenitic Stainless Steel Chemical Analysis, %
|
Grade |
C≤ |
Mn≤ |
P≤ |
S≤ |
Si≤ |
Cr |
Ni |
Mo |
Cu≤ |
N |
|
AL6XN |
0.03 |
2.0 |
0.04 |
0.03 |
1.0 |
20.0- 22.0 |
23.5- 25.5 |
6.0- 7.0 |
0.75 |
0.18- 0.25 |
Stainless steel AL6XN Mechanical Properties
|
Grade |
Tensile, min, ksi[MPa] |
Yield, min, ksi[MPa] |
Elongation, %(min) |
Hardness, HB(max) |
|
AL6XN |
100【690】 |
45【310】 |
30 |
241 |
Physical properties
Density: 8.1 g/cm3
Stainless steel AL6XN Equivalent Grades
|
STANDARD |
UNS |
|
AL6XN |
N08367 |
ASTM Specifications
|
Pipe |
Tube |
Tube |
Sheet/Plate |
Bar |
Forging |
Fitting |
|
ASTM A312 |
ASTM A213/ ASTM A269 |
ASTM A269 |
ASTM A240 |
ASTM A479/ ASTM A276 |
ASTM A182 |
ASTM A403 |
AL-6XN Applications
1.FGD (Flue gas desulfurization) scrubbers.
2.Reverse osmosis desalination.
3.Distillation columns.
4.Heat exchangers.
5.Biopharm tanks and fermenters.
6.Pressure vessels.
7.Agitators and mixers.
8.Seawater coolers in nuclear plants.
Hot Tags: stainless steel al6xn / uns n08367 / 1.4529, China stainless steel al6xn / uns n08367 / 1.4529 manufacturers, suppliers, alloy feedback, alloy keynote speech, alloy continuous casting, alloy breakthrough alloy, alloy delivery, alloy investment opportunity