Stainless Steel 321 features

 

Grades 321 and 347 are the basic austenitic 18/8 steel (Grade 304) stabilized by Titanium (321) or Niobium (347) additions. These grades are used because they are not sensitive to intergranular corrosion after heating within the carbide precipitation range of 425-850 °C. Grade 321 is the grade of choice for applications in the temperature range of up to about 900 °C, combining high strength, resistance to scaling and phase stability with resistance to subsequent aqueous corrosion.

 

SS 321 Chemical Composition

 

Grade

UNS

C≤

Mn

P≤

S≤

Si≤

Cr

Mo

Ni

321

S32100

0.08

2

0.045

0.03

0.75

17.0-19.0

-

9.0-12.0

 

Mechanical Properties of SS 321

 

Grade

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Hardness, HB(max)

321H

75【515】

30【205】

40

217

 

SS 321 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

EN

321

1.4541

S32100

SUS321

X6CrNiTi18-10

 

ASTM SPECIFICATION

 

Pipe,
SMLS& Welded

Tube,
SMLS& Welded

Tube ,
Seamless

Sheet/Plate

Bar /Rod

Forging /Flange

BW Fittings

ASTM A312

ASTM A269

ASTM A213

ASTM A240

ASTM A276/A479

ASTM A182

ASTM A403

 

Applications of SS 321

 

  • Annealing covers
  • High-temp tempering equipment
  • Chemical processing equipment
  • Automotive exhaust systems
  • Firewalls
  • Boiler casings
  • Aircraft exhaust stacks and manifolds
  • Superheaters
  • Gas and oil refinery equipment

 