347 stainless steel is a columbium/tantalum stabilized austenitic chromium-nickel stainless steel. Type 347 has excellent intergranular corrosion resistance and oxidation resistance. at high temperatures. This material is stabilized against chromium carbide formation by the addition of columbium and tantalum. Since these elements have a stronger affinity for carbon than chromium, columbium-tantalum carbides precipitate within the grains instead of forming at the grain boundaries. 347 should be considered for applications requiring intermittent heating between 800ºF (427ºC) and 1650ºF (899ºC) or for welding under conditions which prevent a post-weld anneal. 347 is non-magnetic.
Stainless Steel 347 features
1) It features excellent corrosion resistance comparable to 304 stainless steel.
2) It restrains chromium carbide formation, resists sensitization, and has good intergranular corrosion resistance between 427°C and 816°C.
3) It exhibits certain strength of creep resistance even in strong oxidizing environment at high temperature of 816°C.
4) It is easy to form and weld.
5) It has good low temperature toughness.
Overall, 347 has similar performance like 321 (304 plus Ti) but is superior to 321.
Stainless steel 347 Chemical Composition, %
|
Grade |
C≤ |
Mn |
P≤ |
S≤ |
Si≤ |
Cr |
Ni |
Nb |
|
347 |
0.08 |
2.0 |
0.045 |
0.03 |
0.75 |
17.0-19.0 |
9.0-13.0 |
10*C-1.0 |
Stainless steel 347 Mechanical Properties
|
Grade |
Tensile, min, ksi[MPa] |
Yield, min, ksi[MPa] |
Elongation, %(min) |
Hardness, HB(max) |
|
347 |
75【515】 |
30【205】 |
40 |
201 |
Physical properties
Density: 7.9 g/cm3
Stainless steel 347 Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
GOST |
EN |
|
347 |
1.4550 |
S34700 |
SUS347 |
08Ch18N12B |
X6CrNiNb18-10 |
ASTM SPECIFICATION
|
Pipe, |
Tube, |
Pipe , |
Sheet/Plate |
Bar /Rod |
Forging /Flange |
BW Fittings |
|
ASTM A312 |
ASTM A269 |
ASTM A213 |
ASTM A240 |
ASTM A276/A479 |
ASTM A182 |
ASTM A403 |
Stainless steel 347 Application
1) Petrochemical, food, paper, etc.;
2) Exhaust manifold and branch pipe of aero engine;
3) Turbine compressor hot gas pipeline;
4) Aircraft collector rings;
5)Aircraft exhaust stacks;
6)Boiler casings;
Hot Tags: stainless steel 347 / uns s34700 / 1.4550, China stainless steel 347 / uns s34700 / 1.4550 manufacturers, suppliers, ,