Hastelloy B2 characteristics

 

Hastelloy B2 (UNS N10665/W.Nr. 2.4617) is a solid solution strengthened nickel molybdenum alloy that exhibits significant resistance to reducing environments such as hydrogen chloride gas, sulfuric acid, acetic acid and phosphoric acid. Molybdenum is a major alloying element that provides significant corrosion resistance in reducing environments. This nickel alloy can be used in the as-welded condition because it resists the formation of grain boundary carbide deposits in the weld heat-affected zone.

Hastelloy B2 nickel alloy has excellent salt and acid resistance at various concentrations and temperatures. In addition, Hastelloy B2 has excellent resistance to pitting corrosion, stress corrosion cracking, and knife line and heat-affected zone attacks. Hastelloy B2 supports resistance to pure sulfuric acid and many non-oxidizing acids.

Hastelloy B2 is suitable for most chemical process applications in the as-welded state. Ideal for equipment that handles hydrochloric acid of various concentrations and temperatures. Resistant to hydrogen chloride gas and sulfuric acid, acetic acid and phosphoric acid. The main high temperature applications are those requiring a low coefficient of thermal expansion. Exposure to temperatures between 540 and 815°C (1000-1500°F) should be avoided as the ductility of the alloy decreases. In oxidizing gases such as air, Hastelloy B2 can be used at temperatures up to 540°C (1000°F). In reducing gas or vacuum, the alloy can be used at 815°C (1500°F) to higher temperatures. When hydrochloric acid comes into contact with iron or copper, iron or copper salts may be formed, therefore Hastelloy B2 should not be used with copper or iron piping in systems containing hydrochloric acid.
 

Hastelloy B2 Chemical Composition, %

 

Grade

Mo

Fe≤

C≤

Co≤

Cr≤

Mn≤

Si≤

P≤

S≤

Ni

Hastelloy B2

26.0-30.0

2.00

0.02

1.00

1.00

1.00

0.10

0.04

0.03

Remainder

 

Hastelloy B2 Mechanical Properties

 

Grade

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Hastelloy B2

110[760]

51[350]

40

 

Hastelloy B2 Typical Physical Properties

 

Grade

Density Room Temp.

Melting Range

Specific Heat 68°F

Elastic Modulus 68°F

Thermal Conductivity 68°F

Hastelloy B2

0.333lb/in3

2430°F to 2520°F

0.090Btu/lb. °F

31.4*106psi

64Btu/ft.h.°F

 

Hastelloy B2 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

EN

Hastelloy B2

2.4617

N10665

NiMo28

 

Hastelloy B2 Specifications

 

Bar

Sheet & Plate

Welded Pipe

Seamless Pipe & Tube

Welded Tube

Fittings

Forgings

ASTM B335

ASTM B333, A480

ASTM B619, B775

ASTM B622

ASTM B626

ASTM B366

ASTM B564

 

Hastelloy B2 Application

 

- Food Processing Industry

- Fabrication Industry

- Oil and Gas Industry

- Chemical Industry

- Plumbing

- General Purpose Applications

- Water supply Systems

- Power Plant

- Paper & Pulp Industry

 

Hot Tags: hastelloy b2 / uns n10665 / 2.4617, China hastelloy b2 / uns n10665 / 2.4617 manufacturers, suppliers, ,

Send Inquiry
Come To Us
And Start Your RFQs Now.
contact us