Inconel 718 / UNS N07718 / 2.4668

Inconel 718 / UNS N07718 / 2.4668
Product Introduction:
Type:
Pipes
Plates
Bars
Fittings
Forgings
Flanges
Prefabrication
We are Inconel 718 manufacturer and supplier, top quality, competitive price, professional distribution and after-sales service team.
Send Inquiry
Description
Technical Parameters

Inconel 718 Characteristics

 

INCONEL® alloy 718 (UNS N07718/W.Nr. 2.4668) is a high-strength, corrosion-resistant nickel chromium material used at -423° to 1300°F. Age hardenable and may be welded in fully aged condition, Excellent oxidation resistance up to 1800 degrees F (980 degrees C). Typically sold in the solution annealed temper, but can be ordered aged, cold worked, or cold worked & aged.

 

Inconel 718 Chemical Composition, %

 

Grade

C≤

Mn≤

Si≤

S≤

Cu≤

Ni

Cr

Co≤

Mo

Ti

Al

Fe

Nb+Ta

P≤

B≤

Ti

Inconel 718

0.08

0.35

0.35

0.015

0.30

50.0-55.0

17.0-21.0

1.0

2.8-3.3

0.65-1.15

0.2-0.8

Remainder

4.75-5.5

0.015

0.006

0.65-1.15

 

Alloy 718 Mechanical Properties

 

Mechanical properties

Tensile, min, ksi[MPa]

Yield, min, ksi[MPa]

Elongation, %(min)

Alloy 718

185[1275]

150[1034]

12

 

Alloy 718 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

Inconel 718

2.4668

N07718

NCF 718

 

UNS N07718 Specifications

 

Form

Bar

Plate&Sheet

Tube

Pipe

Forging

Standard

ASTM B637/AMS 5662/AMS 5663/AMS 5664/PWA 1009/PWA 1010/GE B50TF15

ASTM B670/AMS 5596/AMS 5597/ ASTM B637

AMS 5589/ AMS 5590

AMS 5589/ AMS 5590

ASTM B637 /AMS 5562 /AMS 5663 /AMS 5664 /PWA 1009 /PWA 1010 /GE B50TF15

 

Alloy 718 Application

 

1.Cryogenic engineering
2.Acid environment
3.Nuclear Engineering
4.Steam turbine
5.Liquid fuel rocket

 

Hot Tags: inconel 718 / uns n07718 / 2.4668, China inconel 718 / uns n07718 / 2.4668 manufacturers, suppliers, inconel sector, inconel usage, inconel industry, inconel application, inconel local market, inconel field

Send Inquiry
Come To Us
And Start Your RFQs Now.
contact us