Inconel 625 Characteristics
Inconel Alloy 625 (UNS designation N06625) is a nickel-based superalloy that possesses high strength properties and resistance to elevated temperatures. It also demonstrates remarkable protection against corrosion and oxidation. Its ability to withstand high stress and a wide range of temperatures, both in and out of water.Inconel 625 was developed in the 1960s with the purpose of creating a material that could be used for steam-line piping. Some modifications were made to its original composition that have enabled it to be even more creep-resistant and weldable.
Inconel 625 Chemical Composition, %
|
Grade |
C≤ |
Mn≤ |
Si≤ |
S≤ |
Fe≤ |
Ni≥ |
Cr |
Co≤ |
Mo |
Cr+Ta |
P≤ |
Al≤ |
Ti≤ |
|
Inconel 625 |
0.10 |
0.50 |
0.5 |
0.015 |
5.0 |
58.0 |
20.0-23.0 |
1.0 |
8.0-10.0 |
3.15-4.15 |
0.015 |
0.4 |
0.4 |
Alloy 625 Mechanical Properties
|
Mechanical properties |
Tensile, min, ksi[MPa] |
Yield, min, ksi[MPa] |
Elongation, %(min) |
|
Alloy 625 |
100[690] |
40[276] |
30 |
Alloy 625 Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
|
Inconel 625 |
2.4856 |
N06625 |
NCF 625 |
NA 21 |
ХН75МБТЮ |
NC22DNB4M |
NiCr22Mo9Nb |
ASTM Specifications
|
Form |
Bar |
Sheet/Plate |
Tube |
Pipe |
Fitting |
Forging |
|
Standard |
ASTM B466 AMS 5666 BS3076 |
ASTM B443 AMS 5599 Din 17750 |
ASTM B444 |
ASTM B705 |
ASTM B366 |
ASTM B564 Din 17754 |
Alloy 625 Application
1. Components of organic chemical processes containing chlorides, especially where acid chloride catalysts are used.
2. Digesters and bleaching tanks for the pulp and paper industry.
3. Absorption tower, reheater, flue gas inlet baffle, fan (humid), agitator, deflector and flue in flue gas desulfurization system.
4. For the manufacture of equipment and components for use in sour gas environments. For example Acetic acid and acetic anhydride reaction generator.
5. Sulfuric acid condenser.
Hot Tags: inconel 625 / uns n06625 / 2.4856, China inconel 625 / uns n06625 / 2.4856 manufacturers, suppliers, inconel application, inconel industry, inconel usage, inconel local market, inconel field, inconel sector