Super Duplex steel S32760 plate
JN Alloy is largest Stockiest of Super Duplex steel S32760 Plate supplier with huge inventory of Super Duplex Steel S32760 Hot Rolled Plate, ASTM A240 UNS S32760 Polished Plate and Duplex S32760 Cold Rolled Sheets. We offer Din 1.4501 Coils in various sizes at best price. We are leading manufacturer of S32760 steel strip & S32760 stainless steel Sheet.
ASTM A240 UNS S32760 Plate is a super duplex grade stainless steel alloy made for specific applications. Super duplex is a grading of duplex steel which is a combination of ferrite and austenitic steel types. By combining the structures of ferrite and austenite steels, a remarkable corrosion resistance along with high tensile strength is achieved. Super duplex steels S32760 enable their users to capitalize on their many strengths or characteristics. With a yield strength valued at 600 MPa, the Super Duplex Grade S32760 Sheet possesses high mechanical strength. A combination of its strength and satisfactory ductility with its outstanding corrosion resistance properties have led suppliers and manufacturers to dub the UNS S32760 F55 Coil as a super duplex alloy. Super Duplex S32760 plate retains its mechanical and corrosion-resistant properties across a wide range of temperatures. It performs reliably in sub-zero conditions and maintains its structural integrity even in moderately high-temperature environments, ensuring consistent performance in challenging conditions.
JN Alloy is one of the best manufacturers, suppliers, stockiest, and exporters of Super Duplex Steel 32760 Sheets and plates. It is highly resistant to chloride stress corrosion cracking. It is mostly used in high elevated and severe temperatures. The Chemical composition of the Duplex Stainless Steel 32760 Sheet includes chromium content of up to 26%, Nickel content of up to 8%, and molybdenum content of up to 5%. It possesses high tensile strength and toughness. Super Duplex Steel UNS 32760 Plates are highly durable and rust-resistant. It has the best corrosion resistance to many organic and inorganic acids. We are supplying the best quality products that can be used in several manufacturing applications. We used the manufacture of the Super Duplex steel UNS32760 Sheets and Plates in the different shapes and sizes. We manufacture the product according to national and international quality standards. Our organization focuses on customer satisfaction by providing better quality customized as well as non-customized Sheets and Plates in reasonable rates.
Duplex Steel steel S32760 Sheet, Plate & Coil Specifications
|
ASTM A240 UNS S32760 Plate Standards |
ASTM A240 / ASME SA240 - UNS S32760 |
|
Material |
Super Duplex Steel UNS S32760 Plate |
|
Duplex S32760 Plate Specification |
ASTM A240 / ASME SA240 |
|
Width |
1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
|
SA-240 Duplex Steel S32760 Plate Thickness |
4mm-100mm |
|
SA 240 Type S32760 Plate Length |
2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc |
|
SA 240 GR S32760 Plate Finish |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated). |
|
SA 240 TP S32760 Plate Hardness |
Quarter Hard, Half Hard,Spring Hard, Soft, Hard, Super Duplex 2507 Sheet suppliers |
|
Stock available in form of |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) etc |
|
Surface |
2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sand blast, Brush, etching, etc. |
Chemical Composition of ASTM A240 UNS S32760 Super Duplex Stainless Steel Plates
|
Elements |
C |
Cr |
Cu |
Fe |
Mo |
Mn |
N |
Ni |
P |
S |
Si |
W |
|
Minimum |
- |
24.0 |
0.5 |
REMAINDER |
3.0 |
- |
0.20 |
6.00 |
- |
- |
- |
0.50 |
|
Maximum |
0.030 |
26.00 |
1.0 |
- |
4.0 |
1.0 |
0.30 |
8.00 |
0.030 |
0.010 |
1.00 |
1.00 |
ASME SA 240 UNS S32760 Plate Tensile & Yield Strength
|
Tensile |
Yield |
Elongation |
Hardness |
|
MPa min |
MPa min |
% min |
Brinell max |
|
750 |
550 |
25 |
270 |
Super Duplex stainless steel S32760 Plate Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
EN |
|
Super Duplex S32760 |
1.4501 |
S32760 |
X2CrNiMoCuWN25-7-4 |
Super Duplex stainless steel S32760 Plate Application:Pharmaceutical Equipment
Chemical Equipment
Power Generation
Sea Water Equipment
Petrochemicals
Heat Exchangers
Gas Processing
Condensers
Specialty Chemicals
Pulp and Paper Industry
Pharmaceuticals
Off-Shore Oil Drilling Companies