JN ALLOY supplies Stainless Steel 904L Buttweld Cap Manufacturer, SS 904L End Pipe Cap Suppliers, 904L Stainless Steel Welded End Caps, Stainless Steel 904L Pipe Cap, ASTM A403 366 WP904L Stainless Steel End Caps for Pipes, 904L Stainless Steel End Cap, UNS N08904 Weld on Pipe Caps, SS 904L Pipe Cap Exporters, 904L Stainless Steel End Cap, Stainless Steel 904L Cap, Din 1.4539 Pipe Cap Stockist in China.
904L Stainless Steel Buttweld Cap come under the ASTM B366 specification with ASME B16.9 and B16.28 standards. These standards and specification specify pipes of nominal bore sizes ranging from 1/8 inches to 48 inches in diameter for high temperature and corrosion resistant services. 904L Stainless Steel Cap can be seamless and 100% x-ray welded or fabricated. Our excellent quality Stainless Steel 904L Cap is the high alloy austenitic stainless steel which is known for its corrosion properties. These Caps have the application where the corrosion properties of stainless steel are not adequate. These Stainless Steel Caps are having austenitic low- carbon variety of stainless steel with the addition of molybdenum and copper.
Jinie Technology (Jiangsu) Co., LTD is a well-known company that makes, sells, and exports Stainless Steel 904L Pipe Fittings that can be used in many different ways and last for a very long time. Buttweld pipe fittings like the Stainless Steel 904L Buttweld Cap are known for being strong and long-lasting and are often used in violent situations. The Stainless Steel 904L pipe Cap is an excellent choice for structural applications because the chromium-nickel stainless steel and titanium in it resist corrosion between the grains. End Cap fittings of stainless steel 904L resist a wide range of corrosive media and have a lower general corrosion rate than those of stainless steel 904. At temperatures up to 1550 degrees Fahrenheit, the Stainless Steel 904L pipe Cap is very resistant to oxidation. However, it shouldn't be used at temperatures above 1600 degrees Fahrenheit. The corrosion resistance of Stainless Steel 904L End Cap is not as good as that of 18–8 chromium–nickel steels, and the fact that carbides can form when it is welded limits its use in several situations. Stainless Steel 904L Cap Pipe Fittings are very resistant to the damage that chlorine and warm saltwater can cause. Alloy 904L Butt Weld Cap are recommended for use in places with a lot of corrosion. SS 904L Caps are often affected by their loss of strength at high temperatures, caused by over-tempering, and their inflexibility at frigid temperatures.
904L Stainless Steel Pipe Cap Specification
|
Trade name |
Stainless Steel 904L Pipe Cap |
|
Stainless Steel 904L Pipe Cap Standard |
ASTM A403 / ASME SA403 |
|
904L Stainless Steel Pipe Cap Dimensions |
ANSI B16.9, B16.25, B16.28, MSS-SP-43, MSS-SP-48, MSS-SP-59 |
|
SS 904L Pipe Cap Size Range |
1/2″ (15 NB) to 48″ (1200NB) |
|
SS 904L Pipe Cap Schedule |
SCH 5S, 10S, 10, 20, 40S, 40, STD, 60, 80S, 80, XS, 100, 120, 140, 160 & XXS |
|
SA 403 Gr 904L Stainless Steel Pipe Cap Marking |
All Fittings are marked as follows: Grade, Standard, Thickness, Heat No. (Or according to the customer's request.) |
|
Delivery Time |
7-15 working days as usual, It will based on the detailed order quantity. |
|
Payment Terms |
Paypal, Western Union, T/T (Telegraphic Transfer or Wire Transfer), L/C or Trade Assurance 30% deposit & balance before shipping |
|
UNS N08904 Stainless Steel Pipe Cap testing reports |
EN 10204/3.1B NACE 3.1 Certification Mill Test Certification ISO 17025 Standards by a Government of India approved Laboratory Raw Materials Certificate 100% Radiography Test Report Third Party Inspection Report and others as required Positive Material Identification is done on all raw material procured at Priminox Overseas |
ASME SA403 WP904L Stainless Steel Pipe Cap Price
ASTM A403 WP 904L Stainless Steel Pipe Cap : FOB Price US $800.00-$3,500.00 / Ton
904L Stainless Steel Pipe End Cap : FOB Price US $900.00-$5,200.00/ Ton
Stainless Steel 904L Seamless Cap : FOB Price US $700.00-$5,000.00/ Ton
ASTM A403 WP904L Stainless Steel Welded Pipe Cap : FOB Price US $1,199.00-$2,999.00/ Ton
ASME SA403 WP 904L Stainless Steel Buttweld End Cap : FOB Price US $950.00-$4,200.00/ Ton
|
SS UNS N08904 End Cap |
ASTM A403 WP904L Stainless Steel 2" sch40s pipe cap |
|
SA 403 904L Pipe Caps For Pipe End |
Stainless Steel ASTM B366 904LH Pipe Cap |
|
Grade WP904L Stainless Steel 24" pipe end cap |
SS Grade WP904L B16.9 Buttweld Cap |
|
SS 904L End Cap |
DN100 Stainless Steel 904L S40 Weld On Pipe Cap |
|
SA 403 Gr 904L seamless butt weld pipe cap |
SS WP904L Pipe Cap |
|
904L SS pipe end caps |
ASME B16.9 904L Stainless Steel End Cap |
|
Werkstoff No 1.4539 SS Buttwelded Pipe Cap |
ANSI B16.9 Stainless Steel 904L SCH40 Cap Butt Weld Cap |
|
SA 403 WP 904L End Cap |
SA 403 WP 904L Buttweld end seamless pipe cap |
ASME B16.9 Stainless Steel Butt Weld Cap Dimensions Tolerance
|
Nominal Pipe Size |
1/2 to 2.1/2 |
3 to 3.1/2 |
4 |
5 to 8 |
|
Outside Diameter |
1.6 |
1.6 |
1.6 |
2.4 |
|
at Bevel (D) |
-0.8 |
-1.6 |
||
|
Inside Diameter at End |
0.8 |
1.6 |
1.6 |
1.6 |
|
Overall Length (H) |
3 |
3 |
3 |
6 |
|
Nominal Pipe Size |
10 to 18 |
20 to 24 |
26 to 30 |
32 to 48 |
|
Outside Diameter |
4 |
6.4 |
6.4 |
6.4 |
|
at Bevel (D) |
-3.2 |
-4.8 |
-4.8 |
-4.8 |
|
Inside Diameter at End |
3.2 |
4.8 |
6.4 |
6.4 |
|
-4.8 |
-4.8 |
|||
|
Overall Length (H) |
6 |
6 |
10 |
10 |
|
Wall Thickness (t) |
Not less than 87.5% of Nominal Wall Thickness |
|||
Stainless Steel 904L Butt weld Cap Application Industries
Our ASTM A403 WP904L Stainless Steel Butt weld Pipe Cap are used in a wide range of applications and various industries. Below are a few of them:
Petrochemical Industry
Oil and Gas Industry
Chemical Industry
Power Plant Industry
Energy Industry
Pharmaceuticals Industry
Pulp & Paper Indusry
Food Processing Industry
Aerospace Industry
Refining Industry