Jinie Technology (Jiangsu) Co., LTD produce tees in all grades of stainless steel. There are different types of pipe fittings in use and stainless steel 347 tee is one the most common fittings. The ANSI B16.9 SS 347 Threaded Tee belongs to a standard governing fittings and pipes of nominal size ½ inches to 48 inches. The threaded tee has threads instead of sockets. So it is easy to fit with threaded pipes. We produce Stainless Steel 347 Buttweld Unequal Tee which has differently sized ends. This allows differently sized pipes to be connected in one joint. A tee allows 3 pipe endings to be connected together in one joint. The equal tee is used to connect pipes of the same size. We manufacture fittings in grade steel as well. The SS 347 Buttweld Equal Tee manufactured by us is easy to weld with. It has the buttweld which provides extra grip to the welding. The ASME B16.9 Lateral Tee Dimensions differ with schedules and nominal sizes. The nominal sizes change according to standards. Also, the reducing tee can reduce the size of pipeline at the joint. The ASTM A403 Stainless Steel Flanged Reducing Tee is made up of a forged and rolled austenitic SS material. It can be used interchangeably with the SS Reducing Tee or the Stainless Steel Threaded Reducing Tee.

 

We manufacture Forged Fittings in grade steel as well. We vast inventory housing all types of machinery and tools that cut bent and manufacturer ASTM A182 F347 Stainless Steel Forged Socket Weld Tee with accuracy. Grade 347 Stainless Steel Forged Tee has an excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800 to 1500°F (427 to 816°C). SS 347 Socketweld Tee advantageous for high temperature service because of its good mechanical properties. These ASME SA182 F347 Forged Tee are utilized in various industrial application like in chemical industries, ship buildings, fats and fertiliser industries.Customers can contact us for further details.

 

Specification of Werkstoff No 1.4550 Stainless Steel 347 Tee

 

Specifications

ASTM A182 & ASME SA182, ASTM A403 & ASME SA403

Stainless Steel Forged Pipe Fittings size

1/8" NB to 4" NB (Socketweld & Screwed-Threaded)

Werkstoff No 1.4550 SS 347 Thread Fittings

NPT , BSPT, BSPP

ASTM A182 F347 Fittings Dimensions

ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799

ASME SA182 F347H FittingsType

DN15-DN1200

347 Forged Fittings Pressure Rating

2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS

End

Threaded, Welding, JIC

Connection

Welding

Bending Radius

R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom Pipe Fittings

Thickness

Schedule 5S, 10S, 20S, S10, S20, S30, STD, 40S, S40, S60, XS, 80S, S80, S100, S120, S140, S160, XXS and etc.

 

ASTM A403 Equal Tee Price List

 

Description

Price Per Piece in INR

Price Per Piece in USA $

Price Per Piece in UAE Dirham

Stainless Steel 347 Reducing Tee Dn 20 R 15

INR 94

USA $ 1.25

AED 4.60

Ss Equal Tee Dn 25

INR 126

USA $ 1.68

AED 6.17

2x2x1-1/2 Nb Ss Sch40 Reducing Tee

INR 367

USA $ 4.89

AED 17.96

Stainless Steel 347 Dn40, sch 10s, equal Tee

INR 468

USA $ 6.23

AED 22.90

ASME Sa 403 Gr Dn 50x40, sch 10s, unequal Tee

INR 414

USA $ 5.51

AED 20.26

 

Dimension Tolerances of ss 347 Tee fittings

 

Nominal Pipe Size

1/2 to 2½

3 to 3½

4

5 to 8

10 to 18

20 to 24

26 to 30

32 to 48

Outside Dia
at Bevel (D)

+1.6
-0.8

1.6

1.6

+2.4
-1.6

+4
-3.2

+6.4
-4.8

+6.4
-4.8

+6.4
-4.8

Inside Dia at End

0.8

1.6

1.6

1.6

3.2

4.8

+6.4
-4.8

+6.4
-4.8

Center to End (C / M)

2

2

2

2

2

2

3

5

Wall Thk (t)

Not less than 87.5% of Nominal Wall Thickness

 

Application of SS 347 Tee

 

Seawater cooling devices

Oil refinery components

Gas scrubbing plants

Pulp and paper processing industries

offshore process equipment

chemical industry

 

Come To Us
And Start Your RFQs Now.
contact us