Products Description
JN Alloy is largest Stockiest of Stainless steel 316h Plate supplier with huge inventory of AISI 316h Hot Rolled Plate, ASTM A240 UNS S31609 Polished Plate and 316h steel Cold Rolled Sheets. We offer Din 1.4919 Coils in various sizes at best price. We are leading manufacturer of 316h steel strip & SS 316h Sheet.
Stainless Steel 316H Sheets & Plates are designed to work in corrosive conditions having mechanical properties like excellent formability, non-magnetic, excellent strength to prefer in high-temperature applications, etc. SS 316H Sheets & Plates also resists the carbide precipitation in high temperature media, appropriate to use in a saline environment. SS 316H Sheets & Plates have a wide range of applications because of their availability in different forms and finishes like mechanically brushed finishes to mill finishes. A high carbon variant of alloy 316 called 316H was created for use in higher temperatures service. The alloy is used for structural and pressure vessel applications at temperatures above 932°F (500°C) because it has greater strength at high temperatures.
JN Alloy is one of the leading suppliers and stockists of the premium quality range of ANSI/ASME 316H Stainless Steel Plates. We are a highly experienced company in supplying Stainless Steel Plates in customized sizes, various materials, and in numerous dimensions. Products are visually checked for conformity to ASTM, DIN, ASME, MSS, EN, and JIS codes and standards. Upon demand, official certified Inspection organizations can be called in to witness the material reports, dimensions and quality conformity of products. We offer these 316H Stainless Steel Plates in different lengths, shapes, sizes, dimensions, diameters, thicknesses, forms, standards, finishes, types, specifications, etc. and available like hot rolled plates, cold rolled plates, polished plates, etc. We provide the best packing facility like wooden box, bundle, plastic wrap, carton box according to the packing requirements of clients.
Stainless Steel 316H Plate Specifications
|
Description |
ASTM A240 / ASME SA240 Stainless Steel Plates, ASTM A240 Hot Rolled Stainless Steel Plates |
|
Standard |
ASTM, ASME, BS, DIN, EN |
|
Specification |
Cold rolled: 1219mm * 2438mm (4′ x 8′), 1219mm * 3048mm (4′ x 10′), 1220mm * 2440mm, 1250mm * 2500mm or as your requirement. Hot rolled: 1500mm * 2000mm, 1000mm * 3000mm, 1500mm * 4000mm, 1500m * 6000mm or as your requiremnt. |
|
Technique |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
|
Form |
Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Etc. |
|
Surface |
2B, 2D, BA, NO. 1, NO. 4, NO.8, 8K, Mirror, Checkered, Embossed, Hair Line, Sand Blast, Brush, Etching |
|
Thickness |
0.25-200mm, 0.3mm to 120mm |
|
Width |
1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm |
|
Length |
2000mm, 2440mm, 3000mm, 5800mm, 6000mm, 12000mm |
|
Package |
Standard Export Seaworthy Package, or as required. |
|
Value Added Services |
Cladding,Heat Treatment,Annealed, Pickling, Polish,Rolling,Cutting,Bending,Forging,Minor Fabrication Etc. |
|
MTC |
Mill Test Certificate, Available as per EN 10204 3.1 |
316H Stainless Steel Plate Chemical Compostion and Properties
|
Grade |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
|
|
316H |
Min |
0.04 |
0.04 |
0 |
- |
- |
16.0 |
2.00 |
10.0 |
|
max |
0.10 |
0.10 |
0.75 |
0.045 |
0.03 |
18.0 |
3.00 |
14.0 |
316H Stainless Steel Plate Mechanical and Physical Properties
|
Grade |
Tensile Str (MPa) min |
Yield Str 0.2% Proof (MPa) min |
Elong (% in 50mm) min |
Hardness |
|
|
Rockwell B (HR B) max |
Brinell (HB) max |
||||
|
316H |
515 |
205 |
40 |
95 |
217 |
316H Stainless Steel Plates Physical Properties
|
Grade |
Density (kg/m3) |
Elastic Modulus (GPa) |
Mean Co-eff of Thermal Expansion (µm/m/°C) |
Thermal Conductivity (W/m.K) |
Specific Heat 0-100°C (J/kg.K) |
Elec Resistivity (nΩ.m) |
|||
|
0-100°C |
0-315°C |
0-538°C |
At 100°C |
At 500°C |
|||||
|
316H |
8000 |
193 |
15.9 |
16.2 |
17.5 |
16.3 |
21.5 |
500 |
740 |
Stainless steel 316H Plates Equivalent Grades
|
STANDARD |
UNS |
EN |
WERKSTOFF NR. |
|
316H |
S31609 |
X6CrNiMO17-13 |
1.4919 |
ASTM A240 UNS S31609 Plates Application
We regularly supply these Stainless Steel 316H Plates to many leading industrial units and industries like chemical engineering, cement industries, refinery plants, oil & gas industries, petro-chemical industries, power generation industries, natural gas industries, water disposal industries, etc.
SS 316H Sheets & Plates also widely used in manufacturing of sinks, splash backs, medical appliances, cookware, kitchen appliances. The sheets are often used in the manufacturing of food processing units, dairy and also breweries. These SS 316H Sheets & Plates are used in press frame, interior decoration, hospitals, solar plates, machine base, sheaves and for a load of purpose in column base. 316H Stainless Steel Plates finds applications in chemical and petrochemical companies, pharmaceutical companies, fertilizers, pulp, and paper companies, oil and gas companies, etc. Our products are preferred by our clients due to their unique features including durability, reliability, reasonable price, dimensional accuracy, high-end finishing, etc.