Stainless Steel 310s Plate
JN Alloy is largest Stockiest of Stainless steel 310S Plate supplier with huge inventory of AISI 310S Hot Rolled Plate, ASTM A240 UNS S31008 Polished Plate and 310S steel Cold Rolled Sheets. We offer Din 1.4845 Coils in various sizes at best price. We are leading manufacturer of 310S steel strip & SS 310S Sheet.
310S stainless steel plates are a form of commercially available chromium-nickel-based alloy. As such, they have a unique composition that gives them an optimal balance of strength, elasticity, and corrosion resistance. In addition, the density of 310S stainless steel plates is 8.0 g/cm3 or 0.289 lb/in3, making them relatively light compared to other metals with similar properties. AISI 310S stainless steel sheets must also remain dimensional stability during hardening and tempering processes. SUS 310S Stainless Steel Plate have strong carbide formers like tungsten, molybdenums, vanadium and chromium in various combinations to enhance high-temperature performance often with cobalt or nickel. Stainless Steel 310S sheets are generally made up of either flat or long products, which both have a hot rolled or cold formed surface or a covered surface. Although they may not be the lightest materials on the market, their low density allows them to be easily formed into complex shapes and sizes while still offering superior performance in most applications.
Grade 310s Stainless Steel Plate are one of the products from our inventory. JN Alloy is one of the largest Manufacturer and suppliers of high quality 310S stainless steel sheets. Our firm is known in the industry for 310S Stainless Steel Sheets, UNS S31008, ASTM A240 stainless steel 310S sheets, which is available in the market in diverse structures. By considering the needs and demands of clients, we are producing these Plates in a variety of sizes, thicknesses, grades, specifications, and dimensions. These products are enormously admired in the market for their precision engineering. To check the performance, experts check these products on diverse industry norms. We are providing the entire range to our patrons at reasonable rates.
Stainless Steel 310s Plate Specification
|
Item |
Stainless Steel 310s sheet(Hot rolled, cold rolled) |
|
Thickness |
0.3mm~200mm |
|
Width |
1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
|
Length |
2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc |
|
Standard |
JIS, AISI, ASTM, GB, DIN, EN, etc |
|
Surface |
the surface and finish of stainless steel 310s sheet: |
|
Brand: |
Indian Origin, European Origin, Japanese Origin, US Origin, Korea Origin, Thailand Origin, |
|
Package |
Shrink-wrapped ,Carton boxes,Wooden pallets,Wooden boxes ,Wooden crates Etc. |
|
Export to |
India, Indonesia, Malaysia, Singapore, Saudi Arabia, Qatar, UAE, Iran, Iraq, Oman, South Africa, Nigeria, Kenya, Italy, UK, Brazil, Russia , Egypt , Kuwait, Australia |
SS 310S Plates Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Ni | |
| 310S | 0.08 | 2 | 1.5 | 0.045 | 0.03 | 26 | 22 | |
Stainless Steel 310s Plate Mechanical Properties
|
Grade |
Tensile Strength (MPa) min |
Yield Strength 0.2% Proof (MPa) min |
Elongation (% in 50mm) min |
Hardness |
|
|
Rockwell B (HR B) max |
Brinell (HB) |
||||
|
310S |
515 |
205 |
40 |
95 |
217 |
Stainless steel 310S Plate Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
GOST |
EN |
BS |
|
310S |
1.4845 |
S31008 |
SUS310S |
20Ch23N18 |
X8CrNi25-21 |
310S16 |
ASTM A240 310s Plate Applications
Widely used in high temperature and electrical industry, medical equipment construction, chemical, food industry, agriculture and ship parts, food and beverage packaging,Kitchen supplies, trains, airplanes, conveyor belts, vehicles, bolts, nuts, springs and screens, etc.