Stainless Steel 304l Plate
JN Alloy is largest Stockiest of Stainless steel 304L Plate supplier with huge inventory of AISI 304L Hot Rolled Plate, ASTM A240 UNS S30403 Polished Plate and 304L steel Cold Rolled Sheets. We offer Din 1.4306/1.4307 Coils in various sizes at best price. We are leading manufacturer of 304L steel strip & SS 304L Sheet.
Stainless Steel 304L plates are a specific type of stainless steel product that is commonly used in various industries and applications. Stainless Steel 304L is an austenitic stainless steel, which means it contains high levels of chromium and nickel. The composition typically includes approximately 18% chromium and 8% nickel. It also contains a low carbon content, usually around 0.03% or lower, which helps prevent sensitization and subsequent corrosion issues. Stainless Steel 304L is highly resistant to corrosion and oxidation in various environments, including atmospheric conditions, freshwater, mild acids, and alkaline solutions. However, it may be susceptible to localized corrosion in certain aggressive environments, such as chloride-rich environments. Stainless Steel 304L exhibits excellent mechanical properties, including high tensile strength, good formability, and excellent toughness. It has a density of around 8 g/cm³ and a melting point of approximately 1400-1450°C (2550-2650°F). Overall, Stainless Steel 304L plates offer a combination of corrosion resistance, mechanical properties, and fabricability, making them a popular choice for many industrial applications. It is important to consult with manufacturers and suppliers to ensure the specific grade and plate dimensions meet your requirements.
JN Alloy have a wide variety of Stainless Steel 304L Sheets/ Plates, and our manufactured plates are known for their quality, long service life, and dimensional accuracy. The plates that we produce have excellent welding characteristics such as forming, drawing, flexibility, and spinning properties. Stainless Steel 304L plates find extensive use in many industries, including chemical processing, food processing, pharmaceuticals, petroleum refining, and various other applications requiring resistance to corrosion.
Standard Specification Of ASTM A240 Type 304L Plate
|
Thickness |
0.3-200mm |
|
Length: |
2000mm, 2438mm, 3000mm, 5800mm, 6000mm,12000mm, etc |
|
Width |
40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
|
Standard: |
ASTM,AISI,JIS,GB, DIN,EN |
|
Surface: |
BA,2B,NO.1,NO.4,4K,HL,8K |
|
Certification: |
ISO, SGS,BV |
|
Technique: |
Cold Rolled Hot Rolled |
|
Edge: |
Mill Edge \ Slit Edge |
UNS S30403 Plate Chemical Composition
|
Element |
% by Weight |
|
C |
0.030 |
|
Mn |
2.00 |
|
P |
0.045 |
|
Sulfur |
0.030 |
|
S |
0.75 |
|
Cr |
18.00 20.00 |
|
Ni |
8.0 12.00 |
|
Nitrogen (N) |
0.10 |
ASME SA 240 304L Plate Mechanical Properties
|
SS |
Melting Point |
Psi / Mpa - Tensile Stress |
Density |
Psi / Mpa - Yield Stress (0.2%Offset) |
% Elongation |
|
304L |
1400 °C (2550 °F) |
515 75000 |
8.0 g/cm3 |
205 30000 |
35 % |
Stainless steel 304L Plate Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
|
304L |
1.4306/1.4307 |
S30403 |
SUS304L |
304S11 |
03Х18Н11 |
Z3CN18‐10 |
X2CrNi18-9 / X2CrNi19-11 |
Applications of stainless steel 304L Plate
Chemical process vessels
Marine
Architectural
Pharmaceutical equipment
Food Processing and handling
Conveyors
Heat exchangers