Stainless steel 304L Pipe Spools
JN ALLOY supplies 304L Stainless Steel Pipe Spools, 304L Stainless Steel Pipe Prefabrication, 304L Stainless Steel Seamless Pipe & Flange, 304L Stainless Steel Piping Fabrication , SS 304L Pre-fabricated Pipe Spools, UNS S30400 Piping System, 1.4301 Stainless Steel Pipes Spools manufacturer.
304L is a low carbon version of the original, and it is commonly used in heavy-gauge components for greater weldability. This lower carbon content reduces carbide precipitation during welding. Because of this reduced carbon content, 304L stainless steel pipe spool can be used in its as-welded state even in the most corrosive environments. Annealed 304L stainless steel Pipe Spools are more heat and corrosion-resistant. These stainless steel 304L Pipe Spools are a low-carbon variant of type 304 that doesn't need to be annealed after the welding and is frequently used in heavy gauge components. Kitchen benches, equipment, appliances, sinks, troughs, and other items frequently use our SS 304L Pipe Spools. These Alloy 304L Pipe Spools exhibit remarkable strength and toughness at cryogenic temperatures. Our Grade 304L Pipe Spools provide superior forming, drawing, and spinning capabilities and higher ductility and corrosion resistance than Grade 302.
Jinie Technology (Jiangsu) Co., LTD is one of the most well-known producers and exporters of SS 304L Pipe Spools. Our SS 304L Pipe Spools are incredibly strong and adaptable. We can also provide custom sizes for SS 304L Pipe Spools based on the customer's needs. Power plants, high-temperature uses, oil and gas, major engineering industries, shipbuilding, atomic force, marine applications, heat pumps, furnaces, superheaters, transportation liquids, etc., all employ stainless steel 304L spool fittings.
Stainless Steel 304L Pipe Spools Specification
| Specifications | ASTM A403 / ASME SA403 |
| Dimensions | ASTM, ASME and API |
| Thickness | 4.0mm-100mm |
| Size | 1000 mm x 2000mm, 1220mm x 2440mm, 4′ x 8′, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm |
| Range | 5mm To 150mm |
| Specialize | Shim Sheet, Perforated Sheet, B. Q. Profile |
| Form | Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
| End | Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
304L Stainless Steel Pipe Spool Length
|
To suit pipework NB |
PTFE liner Thickness |
Length Min. |
Length Max. |
|
|
Inches |
millimeter |
millimeter |
millimeter |
millimeter |
|
1/2" |
15 |
2.8 |
90 |
6000 |
|
3/4" |
20 |
3.3 |
90 |
6000 |
|
1" |
25 |
3.3 |
90 |
6000 |
|
1.1/2" |
40 |
3.3 |
95 |
6000 |
|
2" |
50 |
3.3 |
110 |
6000 |
|
3" |
80 |
3.3 |
120 |
6000 |
|
4" |
100 |
4.5 |
125 |
6000 |
|
6" |
150 |
5.5 |
140 |
6000 |
|
8" |
200 |
8 or 4.5 |
150 |
3000 |
|
10" |
250 |
9 or 5 |
165 |
3000 |
|
12" |
300 |
9 or 5 |
170 |
3000 |
Common 304L Stainless Pipe Spools Applications
304L stainless is ideal for both commercial and at-home applications. Some specific examples of uses for this grade of steel can include:
Aerospace and automotive structures
Architectural paneling, molding, trim and other details
Braces
Chemical containers to be used for transport
Cooking tools (such as pots and pans)
Construction material for buildings
Dyeing
Food processing equipment (such as wine, beer brewing, and milk)
Heat exchangers
Kitchen equipment (such as sinks or appliances)
Marine environment equipment (such as nuts, screws or bolts)
Railing and trim
Springs
Threaded fasteners
Welded or woven water filtration screens