JN Alloy is largest Stockiest of Stainless steel 17-4ph Plate supplier with huge inventory of 17-4ph Steel Hot Rolled Plate, ASTM A693 UNS S17400 Polished Plate and 17-4ph Cold Rolled Sheets. We offer Din 1.4542 Coils in various sizes at best price. We are leading manufacturer of 17-4ph Plates & SS 17-4ph Sheet.

 

Characteristics Of Stainless Steel 17-4ph Plate

 

Additions of copper and carbon in Stainless Steel 17-4H Sheets give it distinct characteristics, with the copper serving as a strengthening agent against corrosive acids. Type 17-4 PH Stainless steel is the most widely used of all of the precipitation- hardening stainless steels. Its valuable combination of properties gives designers opportunities to add reliability to their products while simplifying fabrication and offen reducing costs. Type 17-4 PH is a martensitic precipitation-hardening stainless steel that provides an outstanding combination of high strength, good corrosion resistance, and good mechanical properties at temperatures up to 600o F (316oC). Its unique combination of properties make this alloy an effective solution to many design and production problems.

 

JN Alloy is a renowed manufacturer, exporter & supplier of wide range of high quality Stainless Steel 17-4H Sheets, Plates & Coils, which is an austenitic stainless steel determination offering moderate to high erosion resistance. Our provided Stainless Steel 17-4H Coils is magnetic, readily welded, and has good fabricating characteristics, though it will lose some toughness at higher temperatures. We provide our customers with a variety of Stainless Steel 17-4H Perforated Coils in stock shapes under the high quality standards.

 

Stainless steel 17-4ph plate Specification

 

Grade

Stainless Steel 17-4 PH | UNS S17400

Standard

ASTM B625 / ASME SB625

Thickness

0.1mm To 100 mm

Length

2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Width

1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Surface

2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sand blast, Brush, etching, etc

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form

Sheets, Plates, Coils, Slatting Coils, Perforated Coils

 

Stainless steel 17-4ph plate Chemical Composition, %

 

Element

Percent By Weight Type 17-4ph

C

Carbon

0.07 maximum

Mn

Manganese

1.00 maximum

P

Phosphorus

0.04 maximum

S

Sulfur

0.03 maximum

Si

Silicon

1.00 maximum

Cr

Chromium

15.00 - 17.50

Ni

Nickel

3.00 - 5.00

Cu

Copper

3.00 - 5.00

Nb

Ta

Columbium

plus Tantalum

0.15 - 0.45

 

Mechanical Properties and Yield Strength 17-4PH Stainless Steel

 

Ultimate Tensile Strength Ksi (MPa): 160 (1103)

0.2% Tensile Yield Strength Ksi (MPa): 145 (1000)

Elongation % in 2" (50mm): 5.0

Hardness Rockwell C: 35

 

17-4ph Stainless Steel Plate Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

17-4PH

1.4542

S17400

SUS630

 

Applications of 17-4PH Stainless Steel Plate

 

Off-Shore Oil Drilling Companies

Pharmaceutical Equipment

Power Generation

Chemical Equipment

Petrochemicals

Sea Water Equipment

Gas Processing

Heat Exchangers

Specialty Chemicals

Condensers

Pharmaceuticals

Pulp and Paper Industry

 

Come To Us
And Start Your RFQs Now.
contact us