Nickel 201 Plate

 

JN Alloy is largest Stockiest of Nickel 201 Plate supplier with huge inventory of Alloy 201 Hot Rolled Plate, ASTM B162 UNS N02201 Polished Plate and Nickel 201 Cold Rolled Plate. We offer Din 2.4061/2.4068 Coils in various sizes at best price. We are leading manufacturer of Nickel Alloy 201 strip & Nickel 201 Sheet.

 

The Nickel 201 Plate shows excellent corrosion resistance properties and can operate in temperatures up to 600 degrees F. The lower carbon content protects these plates against graphitization, making them less susceptible to embrittlement. Apart from this, the plates show excellent resistance to caustic alkalis and varying acid systems to give these modules enhanced oxidation resistance in stress-induced environments. Nickel Alloy 201 Sheet & Plate is also known from the grade name UNS N022001. These sheet plates are nonferrous metals plates that include nickel alloy and other additional contents. This grade of sheet and plates enhances superior toughness and strength. As well as it also shows outstanding resistance at elevated temperature applications. These nickel alloy plates oppose acidic attacks and get unaffected by the weak base of ammonium hydroxide at high-temperature situations. Furthermore, these plates expose strong base to sodium hydroxide.

 

JN Alloys is having the very experienced team and staff members in our organization who are maintaining quality standard higher. Our high-grade Nickel 2.4068 Sheets and Plates has excellent strength. Our team is working to bring efficiency and effectiveness to the organization. Our team and staff members always work to reduce the cost of production by ensuring the fuller utilization of resources and raw materials. Our skilled professionals are doing check the quality standards from time to time and produce the products according to the need and demands of the clients and maintain the quality standards. We do strict quality testing of the Nickel 201 Sheets and Plates at various stages of production. Our team member performs so many tests to check the quality of the products. We pack Nickel 201 Sheets and Plates in suitable packing material, and by choosing a fast shipping way, we deliver orders within the decided time. At reasonable rates, we are offering excellent quality and durable Sheets and Plates to our esteem clients.

 

Nickel 201 Sheets & Plates Specifications

 

Grade

Nickel 201 - UNS N02201

Type

Clad Plate, Rolling Plate, Flat Shim, Plain Sheet, Rolling Sheet Rolls, Foils, Coils, Plate, Strip, Sheet, Flats, Blank (Circle), ,Flat Sheet, Shim Sheet, soft annealed, descaled, sheared, annealed, Checker Plate, tread plate

ASTM B162 Alloy 201 Plate surface

Hot rolled plate (HR), Cold rolled sheet (CR), No.1 finish hot rolled ASTM B162 Alloy 201 Plate, BA, No.3, No.4, No.6, No.1, No. 2D, No. 2B, BA NO(8), No.7, 2B, 2D, SATIN (Met with Plastic Coated), 2B, 1D, No.4, 8K, BA, hairline, brush, satin, mirror etc.

ASTM B162 Alloy 201 Plate Length

0-12mm or as required

Alloy Nickel 201 Plate Thickness

0.3 to 1200 mm or as required

201 Nickel Plate Width

0-2500mm or as required

UNS N02201 Nickel 201 Plate Process

Hot/ Cold Rolled

 

Nickel 201 Chequered Plates Chemical Composition

 

Grade

C

Mn

Si

Cu

S

Mg

Ni

Ti

Fe

Nickel 201

0.02 max

0.35 max

0.2 max

0.25 max

0.01 max

0.15 max

99.0 min

0.1 max

0.4 max

 

Nickel 201 Plate Mechanical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Nickel 201

8.9 g/cm3

1446 °C (2635 °F)

Psi – 67000 , MPa – 462

Psi – 21500 , MPa – 148

45 %

 

Nickel 201 plate Equivalent Grades

 

STANDARD

WERKSTOFF.NR.

UNS

JIS

BS

GOST

EN

Ni201

2.4061/2.4068

N02201

NW 2201

NA 12

HП-2

LC-Ni 99

 

Nickel 201 Plate Applications Industry

 

Nickel 201 Plate is a versatile and high-performance material that finds numerous industrial applications due to its excellent corrosion resistance, mechanical strength, and thermal and electrical conductivity. Some common applications of Nickel 201 Plate include:

 

1. Chemical processing equipment: Nickel 201 Plate is often used in the manufacture of equipment for the production and processing of chemicals, including reactors, heat exchangers, and storage tanks.

 

2. Aerospace and defense: Nickel 201 Plate is used in the aerospace and defense industries due to its ability to withstand high temperatures and its corrosion resistance. It is commonly used in the production of jet engine components, rocket parts, and missiles.

 

3. Electrical and electronic equipment: Nickel 201 Plate has good electrical conductivity, making it an excellent material for use in electrical and electronic equipment. It is often used in the production of electrical contacts, switchgear, and connectors.

 

4. Marine engineering: Nickel 201 Plate's excellent resistance to corrosion makes it ideal for use in marine environments. It is commonly used in the manufacture of marine valves, pumps, and heat exchangers.

 

5. Oil and gas industry: Nickel 201 Plate is used in the oil and gas industry due to its excellent resistance to corrosive environments. It is often used in the manufacture of pipes, fittings, and other equipment for oil and gas exploration and production.

Come To Us
And Start Your RFQs Now.