Nickel 200 Round Bar
JN ALLOY supplies Nickel 200 Bars,Nickel 200 Rods,UNS N02200 Bars Rods, 2.4066/2.4060 Nickel 200 Solid Bars, ASTM B160 UNS N02200 Bars.
Nickel N02200 Round Bars are extensively preferred due to their exceptional corrosion resistant property. It has a pretty low electrical conductivity.
They are available for different applications like from low to high-temperature application purpose. They conduct oxidation resistant and have high strength and can be preferred in the high-temperature environment. Jinie Technology (Jiangsu) Co., LTD offers an extensive collection of Nickel Alloy 200 Round Bars to the valued clienteles, which is quickly fancied by commonplace industrial procedures. Nickel 200 Square Bars is a commercially unalloyed nickel that displays exceptional corrosion resistance and has pretty low electrical resistivity. Nickel 200 Flat Bars are reinforced wrought materials, and is a commercially pure material that shows excellent corrosion resistance. Meanwhile, these Nickel 200 Threaded Bars are also being offered in different sizes and shapes to our customers. Hot forming in Nickel 200 Hollow Bars should be performed within a temperature range between 1600 Degree F and 2250 Degree F (870 Degree C – 1230 Degree C) with heavier sections heated to a minimum of 2000 Degree F before forming. Ganpat Industrial Corporation is one of the pioneer supplier and dealer of quality Nickel 200 Hexagonal Bars, which may be welded victimization all of the common attachment processes. Nickel 200 Triangular Bars is associate solid solution heat resistant alloy with wonderful resistance to oxidization underneath gently cyclic conditions through 2000 Degree F. Alloy 200 Square Bars is compared to steel, where in fact unsullied steels that are harder and have a tendency to figure harden speedily. Alloy 200 Flat Bars is a heat resisting stainless – steel with high resistance to oxidization scaling and has high strength at elevated temperatures. Alloy 200 Threaded Bars is also available in custom made sizes and shapes to our clients at reasonable price.
Types of Nickel 200 Bars
|
Nickel 200 Bright Bar Supplier |
Nickel 200 Hex Bar Exporter in India |
|
Nickel 200 Flat Bar |
Nickel 200 Black Bar Stockists |
|
ASTM B160 Nickel 200 Forged Round Bar |
Nickel 200 Hot Rolled Round Bar |
|
N02200 Nickel Round Bars Manufacturers |
Nickel 200 Black Bar Stockholder |
|
High Quality Nickel 200 Rods |
Industrial Nickel 200 Rectangular Bars |
|
Nickel® Alloy 200 Square Bars Dealer in India |
Alloy 200 Forged Bar Distributor in Mumbai |
|
Nickel 200 Threaded Round Bar Trader in India |
Nickel 200 Hot Rolled Bars |
Chemical Composition and Performance of Nickel Alloy 200
Nickel Alloy 200 is a pure alloy designed for superior performance in various industries. Its carefully balanced chemical composition ensures exceptional durability, corrosion resistance, and adaptability in demanding environments. Each element plays a critical role in enhancing the alloy's overall functionality.
Key Elements and Their Roles
Nickel (Ni): Nickel is the backbone of the alloy, providing exceptional resistance to corrosion and excellent thermal and electrical conductivity. With a minimum content of 99.0%, nickel ensures the alloy's reliability in harsh conditions.
Carbon (C): The low carbon content (maximum 0.15%) enhances toughness and prevents damage at high temperatures, making the alloy suitable for extended use in extreme environments.
Manganese (Mn): Manganese, present at a maximum of 0.35%, boosts resistance to sulfur compounds and strengthens the alloy, contributing to its structural integrity.
Iron (Fe): Though minimal (maximum 0.40%), iron strengthens the alloy without sacrificing its corrosion resistance, ensuring a balance between durability and chemical stability.
Copper (Cu): Copper (maximum 0.25%) helps the alloy resist certain acids and alkalis, enhancing its ability to perform in chemically aggressive settings.
Silicon (Si): With a maximum content of 0.35%, silicon improves the alloy's resistance to high-temperature oxidation, ensuring longevity in elevated-temperature applications.
Sulfur (S): Low sulfur content (maximum 0.01%) ensures easy fabrication and welding, making the alloy versatile for various manufacturing processes.
Nickel 200 round bar Specification
|
Grade |
Nickel 200 – UNS N02200 |
|
Specification |
ASTM B160 UNS N02200 |
|
Nickel 200 Round bar size |
Diameter: 3mm~800mm |
|
Nickel 200 Angle bar size |
3mm*20mm*20mm~12mm*100mm*100mm |
|
Nickel 200 Square bar size |
4mm*4mm~100mm*100mm |
|
Nickel 200 Flat bar size |
Thickness: 2mm~100mm |
|
Width: 10mm~500mm |
|
|
Nickel 200 Hex Bar size |
2mm~100mm |
|
Nickel 200 Billet Size |
1/2" to 495mm Diameter |
|
Nickel 200 Rectangles Size |
33mm x 30mm to 295mm x 1066mm |
|
LENGTHS |
12 RANDOM LENGTHS AND LONG BARS:15 20 RANDOM LENGTHS |
|
Finish |
Bright, Polish, Bright, Rough Turned, Grinding, Centreless Ground & Black |
|
Tolerance |
H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements |
|
Surface |
Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline |
|
Condition |
Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished, Annealed round bar |
|
Technique |
Nickel 200 Hot Rolled, Cold Rolled, Cold Drawn, Forged Round Bar, Rod |
|
Form |
Round, Rod, Precision Ground Bar, Square, Round Rod, Hollow, Hex (A/F), Triangle, Rectangle, Threaded, T-Bar, Half Round Bar, Flat Bar, Rings, Blocks, Billet, Ingot, I/H Bar, Angle, Channel Bar, Profiles, Forging Etc. |
|
Our Nickel 200 round bar conforms to NACE MR0175/ISO 15156 |
|
Nickel Alloy 200 Rods Manufacturing Process
Nickel 200 belongs to a wrought pure nickel commercial grade. The Nickel 200 Round Bar is an age-hardenable material that has above 99% nickel with some other constituting alloys. The versatile Alloy 200 Round Bar is designed with a circular cross-sectional area and can be easily machined and welded in place following standard welding procedures. DIN 2.4066 Hollow Bar has a density of 8.9 g/cm3 and showcases a minimum tensile strength of 462mpa with a minimum yield strength of 148mpa. The robust modules can be easily elongated by 45% in the system. The 2.4066 Nickel 200 Cold Rolled Bar is processed soon after the hot rolling process. These bars have enhanced strength coupled with good tolerance and have a melting point of 1446 degrees C.
The ASTM B160 Nickel 200 flat Bar is a common type of bar that is designed with a rectangular cross-sectional area. These bars typically have a hardness between 70 to 90 Rockwell B. Alloy 200 Flat Bar is commonly seen in use in structural applications where modules require good strength at the same time are lightweight. These bars generally have a thickness between 2mm up to 100mm and have widths from 10mm to 500mm. The ASTM B160 UNS N02200 Hex Rod is a non-pressurized grade designed possessing 6 sides. The rods offer good stability to subsequent components and can be easily rotated or moved within the system. The UNS N02200 Threaded Bar is designed with threads that align to subsequent modules. The bars don't require any welding procedures to fix them in place. The 200 Nickel Alloy Bright Bar is an aesthetically appealing grade that is designed with a smooth surface. These bars are generally designed in an array of shapes and sizes, allowing them to be used in different applications. For more information on the line of products or its pricing, contact us for more information.
Alloy 200 Round Bar Sizes
|
Size & Dimensions of Nickel 200 round bar |
|||||||
|
Metric |
US Bar |
ASTM/ Canadian |
Japanese |
||||
|
Bar Size |
Diam. (mm) |
Bar Size |
Diam. (Inch) |
Bar Size |
Diam. (mm2) |
Bar Size |
Diam. (mm) |
|
5 |
5 |
#2 |
0.250 |
10M |
100 |
6 |
6 |
|
5.5 |
5.5 |
#3 |
0.375 |
15M |
200 |
10 |
10 |
|
6 |
6 |
#4 |
0.500 |
20M |
300 |
13 |
13 |
|
7 |
7 |
#5 |
0.601 |
25M |
500 |
16 |
16 |
|
8 |
8 |
#6 |
0.750 |
30M |
700 |
19 |
19 |
|
9 |
9 |
#7 |
0.875 |
35M |
1000 |
22 |
22 |
|
10 |
10 |
#8 |
1.000 |
45M |
1500 |
25 |
25 |
|
11 |
11 |
#9 |
1.125 |
55M |
2500 |
29 |
29 |
|
12 |
12 |
#10 |
1.250 |
32 |
32 |
||
|
14 |
14 |
#11 |
1.375 |
35 |
35 |
||
|
16 |
16 |
#12 |
1.500 |
38 |
38 |
||
|
18 |
18 |
#13 |
1.601 |
41 |
41 |
||
|
20 |
20 |
#14 |
1.750 |
44 |
44 |
||
|
22 |
22 |
#15 |
1.875 |
48 |
48 |
||
|
25 |
25 |
#16 |
2.000 |
51 |
51 |
||
|
28 |
28 |
#18 |
2.250 |
57 |
57 |
||
|
32 |
32 |
||||||
|
36 |
36 |
||||||
|
40 |
40 |
||||||
|
44 |
44 |
||||||
|
50 |
50 |
||||||
Nickel 200 Bar Applications
Successful Implementation in Marine Environments
In marine environments, Nickel Alloy 200 round bars have been effectively implemented in offshore oil and gas platforms, which operate under harsh conditions with exposure to seawater, inducing severe corrosion. Nickel Alloy 200 was selected for its superior resistance to chloride-induced stress corrosion cracking. The round bars maintained their integrity and performance, ensuring the structural safety of the platforms and minimizing the risk of environmental contamination due to fastener failure.
Application in Chemical Processing Plants
For instance, in a hydrofluoric acid production plant, these Nickel Alloy 200 round bars successfully resisted extremely corrosive conditions. The alloy's ability to resist chemical attack and maintain its mechanical properties ensured the continuous and safe operation of the plant's equipment, demonstrating the material's suitability for such demanding applications.
Aerospace and Petrochemical Industry Applications
The aerospace industry has also embraced Nickel Alloy 200 round bars, primarily for their purity and resistance to reducing chemicals. For example, in aircraft engines, these round bars endured high temperatures and pressures, maintaining peak performance. Similarly, in the petrochemical sector, these round bars have been employed in environments containing caustic solutions, providing long-lasting resistance to corrosion and contributing to the safe operation of processing facilities.
Versatile Use in Oil and Gas Industries
The oil and gas, mining, and cement industries have widely adopted Nickel Alloy 200 round bars due to their high strength and toughness. In the oil and gas sector, they are used in equipment exposed to high pressures and corrosive conditions, such as drilling rigs and pipelines. In mining and cement production, the bolts withstand abrasive environments, contributing to the durability and longevity of machinery and infrastructure. These case studies highlight the versatility and dependability of Nickel Alloy 200 round bars across diverse industrial applications.