Nickel 200 plate

 

JN Alloy is largest Stockiest of Nickel 200 Plate supplier with huge inventory of Alloy 200 Hot Rolled Plate, ASTM B162 UNS N02200 Polished Plate and Nickel 200 Cold Rolled Plate. We offer Din 2.4066/2.4060 Coils in various sizes at best price. We are leading manufacturer of Nickel alloy 200 strip & Nickel 200 Sheet.

 

Nickel 200 Sheet / Plate can operate at temperatures above 315 degrees Celsius. The material is a commercially pure nickel grade with 99% nickel in the composition along with sulfur, phosphorus, manganese, silicon and carbon and provides numerous beneficial qualities including excellent corrosion resistance, good mechanical properties, and high thermal and electrical conductivities. Nickel 200 plate is a ferromagnetic alloy which moderates strength in extensive high temperature. It has desirable mechanical properties, excellent resistance against corrosion, and oxidation in high heat. It is suitable in all temperature environments and also offers exceptional corrosion resistance. Outstanding resistance to reducing chemicals, alkaline mediums, and good electrical conductivity, oxidation resistance, pitting strength, stress crack corrosion resistance, excellent toughness are the few most beneficial properties of Nickel 200 plate.

 

JN Alloys is a leading manufacturer and supplier of these sheets and plates in larger quantities. The uns n02200 sheet is thinner with less than 4mm in thickness where the plates are thicker up to 75mm in thickness. The material is highly dense with 8.89 grams per centimeter cube density. The Alloy 200 Sheet also has high strength with up to 275MPa minimum yield strength and 550MPa minimum tensile strength and 45-73 Brinell hardness score.

 

There are different types of productions such as hot rolling and cold rolling. The nickel 200 hot rolled plate is used in the making of storage containers, tankers, panels and platforms for highly corrosive applications. We choose the highest quality alloy for the manufacturing of Plates and Sheets by testing it strictly. JN Alloys is your trusted source for premium Nickel 200 Sheet and Plate materials. Contact us for more information regarding our Nickel 200 Plates and Sheets options and we will gladly speak with you regarding your project's exact specifications.

 

Nickel 200 Sheets & Plates Specifications

 

Specifications

ASTM / ASME SB 168

Size

1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Thickness

0.1mm to 12 mm Thk

Form

Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

Nickel 200 Chequered Plates Chemical Composition

 

Grade

C

Mn

Si

Cu

S

Ni

Fe

Nickel 200

0.15 max

0.35 max

0.1 max

0.25 max

0.01 max

99.0 min

0.4 max

 

Nickel 200 Plate Mechanical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Nickel 200

8.9 g/cm3

1446 °C (2635 °F)

Psi – 67000 , MPa – 462

Psi – 21500 , MPa – 148

45 %

 

Nickel 200 plate Equivalent Grades

 

STANDARD

WERKSTOFF.NR.

UNS

JIS

BS

GOST

AFNOR

EN

Ni200

2.4066/2.4060

N02200

NW 2200

NA 11

HП-2

N-100M

Ni 99.2

 

Nickel 200 plate Applications Industry

 

Our wide-ranging inventory of Nickel 200 Plates is available in different sizes and specifications in order to meet all need of various industries like in petroleum, chemical, power, gas, metallurgy, shipbuilding, construction, and so on.

Pharmaceutical Equipment

Off-Shore Oil Drilling Companies

Chemical Equipment

Power Generation

Sea Water Equipment

Petrochemicals

Heat Exchangers

Gas Processing

Condensers

Specialty Chemicals

Pulp and Paper Industry Pharmaceuticals

 

Come To Us
And Start Your RFQs Now.
contact us