Nickel 200 pipe
JN Alloy is a distributor and manufacturer of nickel 200 Pipe, UNS N02200 Tube, nickel 200 Tube, 2.4066/2.4060 nickel 200 Tube, nickel 200 Material, nickel 200 Tubing and nickel 200 Seamless Tubing.
Nickel Alloy 200 Tube also known as Commercially Pure Nickel Tube and Low Alloy Nickel Tube. This alloy tube is 99.6 % pure wrought nickel and suitable for a wide range of applications. Nickel has superior toughness and offers resistance against corrosive and caustic environments whether operating in-house or outdoors. Both hot working and cold working practices can be utilized when shaping UNS N02200 Tubing. Hot working temperatures of Nickel 200 rectangular Tubes should be between 1200 Degree F and 2250 Degree F with heavy forming to be performed at temperatures above 1600 Degree F. Annealing in Nickel 200 Round Exhaust Tubes should be performed at a temperature between 1300 Degree F and 1600 Degree F. Care should be taken when choosing the anneal temperature and time at temperature in Nickel 200 welded Tubes. This can greatly influence the mechanical properties and structure of the material so they have good mechanical properties. When operating temperatures are expected to exceed 600 Degree F, carbon content in ASTM B161 Nickel 200 Seamless tubing becomes critical. The lower carbon content of Nickel 200 Electro-polish Tubes makes the material resistant to graphitization and therefore less subject to embrittlement.
Jinie Technology (Jiangsu) Co., LTD an ISO 9001: 2015 guaranteed organization, that offer advancement, quality and administration bundled into a tough item that epitomizes magnificence.We are a maker, broker, stockist, provider, and exporter of ASTM B725 Nickel 200 Pipes that are designed by giving extraordinary concentration to creating channels that thought on testing conditions, giving elite at sensible cost. We give UNS N02200 Nickel ERW Pipes to the warm power and rural industry, which has high deformability and quality, with great imperviousness to destructive environment. Our 2.4066 Nickel Rectangular Pipes have high imperviousness to dry gasses, chlorine and dry chloride and also dry fluorine, subsequently utilized as a segment in the gas business. We keep a tab on showcase patterns and requests, to create new, reasonable and prudent items fit for experiencing customization. We have assembled a comprehensive arrangement of value items over the traverse of 25 years. Our items are completely guaranteed and 100% strong. Also visit out copper nickel pipes section for range of products.
Nickel Alloy 200 Seamless Pipe Material Specification
|
ASTM Specification |
ASME SB-161, ASME SB-829, ASME SB-775, ASME SB-725 |
|
Standard |
ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB |
|
ASTM B161 Nickel 200 Seamless Pipe Size |
4 to 219mm W. T.: 0.5 to 20mm |
|
DIN 17740 UNS N02200 Welded Pipe Size |
5.0 - 1219.2 mm |
|
Nickel WERKSTOFF NR. 2.4066 EFW Pipe size |
5.0 - 1219.2 mm |
|
Swg & Bwg |
12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg., |
|
BS 3075 200 Nickel Pipe Schedule |
XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160 |
|
BS 3074 Nickel 200 pipe Length |
Double Random, Single Random, Standard & Cut length Pipe |
|
Finish |
Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc |
|
Form |
Nickel 200 are available in form of Round, Square, Hollow, Rectangular, Hydraulic, Coiled, Straight Pipes, "U" Shape, Pan Cake Coils etc. |
|
Type of BS 3073 200 Alloy Pipe |
Seamless / ERW/ EFW / Welded / Fabricated / CDW / DOM / CEW nickel 200 |
|
Nickel 200 pipe End |
Plain End, Beveled End, Threaded Pipe, Screwed ends |
|
Marking on ASME SB-725 Alloy 200 Pipe |
All ASTM B161 Nickel 200 Pipes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.) |
|
Application of BS 3076 Nickel 200 pipe |
Dairy Pipe, Oil Pipe, Gas Pipe, Fluid Pipe, Boiler Pipe for Chemical Industry |
|
Value Added Service |
Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc. |
|
Specialize in |
Large Diameter Nickel 200 pipe |
|
NA11 DIN 17740 Nickel 200 pipe manufacturing Technique |
Cold drawn, hot drawn, bright annealed, solid solution, hot extruding |
Nickel ASTM B161 Custom Pipe Chemical Equation
|
Nickel 200 |
Ni |
C |
Mo |
Mn |
Si |
Fe |
P |
S |
Cu |
Cr |
|
99.0 min |
0.15 max |
– |
0.35 max |
0.1 max |
0.4 max |
– |
0.01 max |
0.25 max |
– |
Nickel 2200 4 inch Pipe Mechanical Behaviour
|
Density |
Melting Point |
Yield Strength (0.2%Offset) |
Tensile Strength |
Elongation |
|
8.9 g/cm3 |
1446 °C (2635 °F) |
Psi – 21500 , MPa – 148 |
Psi – 67000 , MPa – 462 |
45 % |
Nickel 200 Pipe Equivalent Grades
|
STANDARD |
WERKSTOFF.NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
|
Ni200 |
2.4066/2.4060 |
N02200 |
NW 2200 |
NA 11 |
HП-2 |
N-100M |
Ni 99.2 |
DIN 2.4066 tubing applications
Pharmaceutical Equipment
Chemical Equipment
Sea Water Equipment
Heat Exchangers
Condensers
Pulp and Paper Industry
Off-Shore Oil Drilling Companies
Power Generation
Petrochemicals
Gas Processing
Specialty Chemicals
Pharmaceuticals