Monel K500 Flange

 

JN ALLOY supplies Monel K500 SO flanges, Monel K500 WN flanges, UNS N05500 blind flanges, 2.4375 Monel K500 plain flanges, ASTM B564 UNS N05500 SW flanges, Monel K500 spectacle blind flanges, Monel K500 threaded flanges, 2.4375 spacer ring, UNS N05500 paddle blind/blank, Monel K500 bleed/test/drip ring, Monel K500 reducing flange.

 

MONEL 400/K500 FLANGES SPECIFICATION

 

Material: ASTM B564 Standard Specification for Nickel Alloy Forgings

Standard: ASME B16.5, ASME B16.47, DIN, EN, BS, JIS

Size: 1/2"-48", DN6-DN400

Class: 150#,300#,400#,600#,900#,1500#,2500#

 

ASTM B564 flanges are a type of weld neck flange made from corrosion-resistant nickel alloy containing copper and iron. This alloy offers superior resistance to freshwater, brine, and steam environments and excellent strength and hardness in temperatures up to 1000°F (538°C). Additionally, it is more resistant to stress corrosion cracking than many other alloys. Monel K500 weld neck flanges boast superior ductility and formability compared to most alloys, making them the ideal option for welding operations involving complex shapes or tight spaces. Monel K500 flanges offer a unique combination of high strength with similar corrosion resistance to Monel 400 and improved resistance to a sour-gas environments. Stronger than 400, alloy K500 even retains this strength in corrosive conditions, resisting both pure and salt water, as well as non-oxidizing mineral acids, salts, alkalis, and sour gas. The exception being that Monel K500 flanges can be more prone to stress-corrosion cracking in some environments than Monel 400. In addition, stagnant or slow-moving sea water can cause fouling which is followed by pitting, but pitting typically slows after initial attack.

 

Jinie Technology (Jiangsu) Co., LTD is a leading manufacturer, stockiest, and exporter of premium quality of Monel K500 Flanges in the global market. Monel K500 is a Nickel-Copper alloy that provides excellent corrosion resistance towards oxidizing salt, nitric acid, nitrates, and other oxidizing agents. This alloy has a higher strength and hardness. Monel K500 Flanges have excellent resistance in harsh environments offering crevice corrosion, pitting, stress corrosion cracking, and inter-granular corrosion. Additionally, compared to other metals like steel or stainless steel, Monel K500 Flanges have a few advantages. Due to their extremely low thermal expansion coefficient, they resist buckling and warping under stress. Because of this, Monel K500 Flanges are resistant to thermal shock and fatigue during stress cycles, which helps to prevent internal components from being damaged or may even cause the flanges to break off in some locations depending on how much force is exerted along their length. Monel K500 Flanges can sustain more stress without cracking or breaking than most other alloys because of their high yield strength. Additionally, they are more resistant to wear and pressure corrosion cracks because of their high yield strength. These flanges are available in various sizes, shapes, types, dimensions, and customized specifications as per the demands of our esteem customers.

 

Types Of Monel K500 Flanges

 

Products

Size

Monel K500 Slip On Flanges

Monel K500 Weld Neck Flanges

Sizes 1/8″ – 36″
Raised Face or Flat Face

Monel K500 Blind Flanges

Monel K500 Lap Joint Flanges

Monel K500 Threaded Flanges

Monel K500 Socket Weld Flanges

Monel K500 Plate Flanges

Monel K500 Ring Joint Type Face (RTJ) Flanges

Monel K500 Spectacle Blind Flanges

Monel K500 High Hub Blind Flanges

Monel K500 Orifice Flanges

Monel K500 Reducing Flanges

Monel K500 Square Flanges

Monel K500 Groove & Tongue Flanges

Monel K500 Long Neck Weld Flanges

Monel K500 Spades and Ring Spacers Flanges

Monel K500 Weldo / Nipo Flanges

Monel K500 Expander Flanges

 

Monel Alloy K500 Pipe Flanges Chemical Composition

 

Grade

 

C

Mn

Si

S

Cu

Fe

Ni

Monel K500

 

0.25 max

1.5 max

0.5 max

0.010 max

27.00 – 33.00

0.5 – 2

63.00 min

 

Monel K500 Plate Flanges Mechanical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Monel K500

8.44 g/cm3

1350 °C (2460 °F)

Psi – 160000 , MPa – 1100

Psi – 115000 , MPa – 790

20%

 

Monel K500 Flanges Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Monel K500

2.4375

N05500

 

Weight Of 65mm (2 1/2") Monel K500 UNS N05500 Flange

 

Standard

Class

Diameter

Bolt Circle Diameter

Number of Bolts

Bolt Size

Diameter of Bolt Hole

AS 4087 Flanges

PN14 Flanges

165

127

4

M16

18

PN16 Flanges

165

127

4

M16

18

 

PN21 Flanges

185

146

8

M16

18

 

PN35 Flanges

185

146

8

M16

18

 

AS 2129 Flanges

Table C Flanges

165

127

4

16

18

Table D Flanges

165

127

4

16

18

Table E Flanges

165

127

4

16

18

Table F Flanges

185

146

8

16

18

Table H Flanges

185

146

8

16

18

Table J Flanges

185

146

8

19

22

ANSI B16.5 Flanges

ANSI 150 Flanges

178

140

4

16

19

ANSI 300 Flanges

191

149

8

19

22

ANSI 600 Flanges

191

149

8

19

22

ANSI 900 Flanges

244

191

8

22

25

ANSI 1500 Flanges

244

191

8

25

29

ISO 7005 (DIN) Flanges

PN6 Flanges

160

130

4

M12

14

PN10 Flanges

185

145

4

M16

18

PN16 Flanges

185

145

4

M16

18

PN20 Flanges

180

139.5

4

M16

18

PN25 Flanges

185

145

8

M16

18

PN40 Flanges

185

145

8

M16

18

 

Monel K500 Flanges ApplicationChemical Industry

 

Petrochemical industry

Marine & Power Transmission industry

Power plants

Energy industries

Furniture

Pharmaceutical processing industry

Modern architecture

Home appliances

Water waste projects

Synthetic fiber

Heat exchanger

Fluid piping

Dairy and food processing

 

Come To Us
And Start Your RFQs Now.
contact us