JN Alloy is a distributor and manufacturer of Monel 400 Pipe, UNS N04400 Tube, Monel 400 Tube, 2.4360 Monel 400 Tube, Monel 400 Material, Monel 400 Tubing and Monel 400 Seamless Tubing.
A solid solution alloy, Monel 400 is an alloy that exhibits superior resistance to the marine environment. This is an alloy which can only be strengthened by cold working. Cold worked Alloy 400 Pipe produced under specification ASTM B165, is available in both a seamless or welded construction. The corrosion resistance to acids such as hydrochloric acid or hydrofluoric acid in a deaerated condition, of the Monel 400 Seamless Pipe is what makes them suitable for use in non-oxidizing chloride based solutions. In an annealed condition, the strength of a Monel 400 EFW Pipe is relatively low. This can be remedied by the use of various tempers, which can result in an increase in strength. The Monel 400 Welded Pipe can be used at temperatures as high as about 1000° F down to cryogenic temperatures. Apart from having good resistance to alkalis, the ASTM B725 UNS N04400 demonstrates excellent resistance when exposed to solutions containing neutral and alkaline salts.
Jinie Technology (Jiangsu) Co., LTD an ISO 9001: 2015 certified company, that offer innovation, quality and service packaged into a durable product that embodies excellence. We, at Amco, are dedicated to the highest degree of quality and standard, offering premium goods and services for challenging industries. We deliver products that guarantee customer satisfaction. We produce and provide WNR 2.4361 Monel Seamless Pipes have an excellent surface condition and uniform hardness, are resistant to seawaters and brine waters flowing at higher speeds and can equally withstand alkalis and sulfuric acids.ASTM B725 UNS N04400 pipes come in different standards. The seamless pipes and tubes are in SB 165, the welded pipes come in SB725 standards. The Alloy 400 Welded Pipe is produced through welding procedures. These welded from either a strip or plate of the same material grade. Seamless pipes are drawn from a single piece of material therefore there is no seam and the absolute roughness is very less. We supply all kinds of DIN 2.4360 Alloy 400 Pipe products and you can contact us for further details.
ASME SB165 Monel 400 pipe tube specifications
|
Specifications |
ASTM B165 |
|
|
ASTM B165 400 Monel Seamless Pipes size |
4 to 219mm W. T.: 0.5 to 20mm |
|
|
Nickel Alloy 400 Welded Pipes size |
|
|
|
UNS N04400 EFW Pipes size |
5.0 -1219.2 mm |
|
|
Specialized in |
Large Diameter Size |
|
|
Alloy 400 Pipes Schedule |
SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
|
|
ASTM B165 UNS N04400 Pipes Condition |
Hot-Finished, Annealed, Cold-Drawn, Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
|
|
2.4360 Alloy 400 Pipes Form |
Square, Straight, Rectangular, Round, Hollow, Hydraulic, |
|
|
ASTM B165 Monel 400 Pipes Length |
Single Random, Double Random & Cut Length. |
|
|
End |
Plain End, Beveled End, Threaded. |
|
|
Marking |
All Monel Alloy 400 Pipes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.) |
|
|
Material Test Certificates (MTC) |
Material Test Certificates (MTC) as per EN 10204 3.1 and EN 10204 3.2 |
ASTM B165 UNS N04400 Pipe Chemical Composition
|
Grade |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
|
Monel 400 |
0.30 max |
2.00 max |
0.50 max |
0.24max |
28.0-34.0 |
2.50 max |
63.00 min |
2.4360 Alloy 400 Pipe Mechanical Properties
|
Element |
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
Monel 400 |
8.8 g/cm3 |
1350 °C (2460 °F) |
Psi – 80,000 , MPa – 550 |
Psi – 35,000 , MPa – 240 |
40 % |
Equivalent Grades for ASTM B165 Monel 400 Pipes
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
|
Monel 400 |
2.4360 |
N04400 |
NW 4400 |
NA 13 |
МНЖМц 28-2,5-1,5 |
NU-30M |
NiCu30Fe |
UNS N04400 Tubing applications
Textile machinery
Oil and gas industry
Pulp and paper industry
Power plants
Energy industries
Furniture
Pharmaceutical processing industry
Modern architecture
Home appliances
Water waste projects
Synthetic fiber
Heat exchanger
Fluid piping
Dairy and food processing