Inconel 625 plate
JN Alloy is largest Stockiest of Inconel 625 Plate supplier with huge inventory of Alloy 625 Hot Rolled Plate, ASTM B443 UNS N06625 Polished Plate and Inconel 625 Cold Rolled Plate. We offer Din 2.4856 Coils in various sizes at best price. We are leading manufacturer of Inconel alloy 625 strip & Inconel 625 Sheet.
Inconel 625 (AMS 5599, UNS N06625) plate is a nickel-based superalloy with excellent resistance to oxidation and corrosion. The nickel-chromium matrix of this material is reinforced by the addition of molybdenum and niobium, which is alloyed through solid solution strengthening. This process allows alloy Inconel 625 plate to maintain high strength and toughness at temperatures ranging from cryogenic up to 1800°F (982°C). It is non-magnetic, austenitic, and displays high tensile strength, fabricability, and brazeability. Inconel 625 Sheet / Plate is a high alloy high temperature resistant metallic sheet or plate that can operate at temperatures up to 1093 degrees Celsius. This superalloy is made up of nickel, chromium and molybdenum and is stabilized by niobium. Inconel 625 sheets are nickel-based and can withstand temperatures ranging from cryogenic extreme freezes to 1000 degrees Celsius/2000 degrees Fahrenheit. They are nickel-based and use columbium and molybdenum as refractory metals. ASTM B443 UNS N06625 Strip has a minimum yield strength of 430MPa and a minimum tensile strength of 940MPa due to the nickel chromium framework, molybdenum material, and strong solution strengthening.
JN Alloys is a supplier of these plates and sheets in various sizes and scales. The Inconel 625 plate is resistant to saline and sea water. This is because the Alloy 625 sheet has high nickel content. The high corrosion allows the plates and sheets to be used in marine applications and equipment. Inconel 625 Sheet Plate are one of the most demanded products from our inventory. We are producing the highest quality Inconel 625 Sheet Plate, which has excellent toughness and strength across a wide range of operating temperatures. We ensure to offer excellent quality Inconel 625 Sheet Plate to our esteem customers at reasonable rates. Our high-grade Plates have excellent resistance to oxidation and stress-corrosion cracking. Our high-quality Inconel 625 Sheet Plate has high tensile strength, high durability, excellent performance, and low maintenance. By following all the industrial and international specifications while designing these Plates, we are delivering suitable and durable Plates to our clients.
ASTM B168 Inconel 625 Sheets, Plates Specification
|
ASTM Specification |
ASTM A240 / ASME SA240 |
|
Standard |
MSRR, AMS, BS, ASTM A240 / ASME SA240 |
|
Length & Sizes |
1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 2m, 2.44m, 3m, 36" X 120" or 48" X 144", 4' x 8', Cut to size available |
|
Thickness |
0.1mm to 100 mm Thk |
|
Width |
10-2500mm |
|
Hardness |
Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
|
Temper |
Annealed |
|
Condition |
Polished on both sides |
|
Finish |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
|
Stock in form of |
Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate |
|
Value Added Service |
Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc. |
Inconel 625 Cold Rolled Sheets Chemical Composition
|
Grade |
C |
Mn |
Si |
P |
S |
Ni |
Cr |
Fe |
Mo |
Co |
Al |
Ti |
Nb + Ta |
|
Inconel 625 |
0.10 max |
0.50 max |
0.50 max |
0.015 max |
0.015 max |
58.0 min |
20.0 – 23.0 |
5.0 max |
8.0 – 10.0 |
1.0 max |
0.40 max |
0.40 max |
3.15 – 4.15 |
Alloy 625 Polished Cold Drawn Plates Mechanical Properties
|
Grade |
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
Inconel 625 |
8.4 g/cm3 |
1350 °C (2460 °F) |
Psi – 135,000 , MPa – 930 |
Psi – 75,000 , MPa – 517 |
42.5 % |
Alloy 625 plate Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
|
Inconel 625 |
2.4856 |
N06625 |
NCF 625 |
NA 21 |
ХН75МБТЮ |
NC22DNB4M |
NiCr22Mo9Nb |
ASME SB443 UNS N06625 APPLICATIONS INDUSTRY
Motor racing exhaust systems
Chemical Processing
Aerospace equipment
Jet Engine exhaust systems
Chimney Linings
Sour gas production tubes
Nuclear waste reprocessing equipment