Inconel 601 plate

 

JN Alloy is largest Stockiest of Inconel 601 Plate supplier with huge inventory of Alloy 601 Hot Rolled Plate, ASTM B168 UNS N06601 Polished Plate and Inconel 601 Cold Rolled Plate. We offer Din 2.4851 Coils in various sizes at best price. We are leading manufacturer of Inconel alloy 601 strip & Inconel 601 Sheet.

 

Inconel 600 Sheets is a nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high temperature corrosion. The maximum significant material is its brilliant resistance to extraordinary temperature oxidization even under recurring heating and refrigeration. Inconel 601 Sheet offer good oxidation and corrosion resistance at a very high temperature range. It is nonmagnetic and has excellent mechanical properties. Inconel 601 Sheet has high strength properties, good workability and weldability. It is heat treatable. It exhibits excellent resistance to alkaline solutions and chloride-ion stress cracking due to its high nickel content and high resistance to sulfur compounds due to its chromium content. Inconel 601 plate is also resistant to steam, steam/air mixtures and carbon dioxide. It has good workability and is weldable. The Inconel Alloy 601 Sheet exhibits excellent mechanical properties and superior hardness. These sheets possess a minimum tensile strength of 650Mpa and minimum yield strength of 300Mpa. They can be elongated by 30% and still possess good workability. UNS N06601 Sheet is used in various industries where strength and precision are very important.

 

JN Alloys offers an extensive collection of Inconel 601 plate, which are extensively appropriate for dissimilar purposes in dissimilar industries. We are committed in offering the best qualities on their products that are highly appreciated by the buyers. Unique features such as high end finishing, accurate dimensions, excellent durability and timely delivery of the product are some of the services offered. While manufacturing the Inconel 601 sheets and plates, the industry use efficient quality of raw materials that are procured form reliable market vendors which are further quality tested by the industry professionals. Apart from this, they use modern machinery and other inventory technology in their fabrication process in order to enhance the productivity of the product. Besides, buyers can buy the Inconel grade sheets and plates in customization specification varying in size and shapes as per their necessity. The industry professionals conduct relevant material tests on Inconel 601 Sheet & Plate in order to ensure the strict quality and efficiency before finally delivering it to the buyers.

 

Specification Table Of Inconel 601 Plate

 

Grade

Inconel 601 | UNS N06601

Standard

ASTM B168 / ASME SB168

Thickness

0.1mm To 100 mm

Size

1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form

Sheets, Plates, Coils, Slatting Coils, Perforated Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

Chemical Composition of Inconel Alloy 601 Sheet & Plate

 

Grade

C

Mn

Si

S

Cu

Fe

Ni

Cr

Inconel 601

0.10 max

1.00 max

0.5 max

0.015 max

1 max

Bal

58 – 63

21 – 25

 

Mechanical Properties of Inconel 601 Sheet & Plates

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

8.1 g/cm3

1411 °C (2571 °F)

Psi – 80,000 , MPa – 550

Psi – 30,000 , MPa – 205

30 %

 

Inconel 601 Sheet & Plates Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

Inconel 601

2.4851

N06601

NCF 601

NA 49

Xp0BT

NC23FeA

NiCr23Fe

 

Inconel 601 plate Application Industries

 

Chemical industry

Food processing

Aerospace

Nuclear Engineering

Heat treating industry

Gas turbine components

Pulp and paper industry

 