Inconel 600 plate

 

JN Alloy is largest Stockiest of Inconel 600 Plate supplier with huge inventory of Alloy 600 Hot Rolled Plate, ASTM B168 UNS N06600 Polished Plate and Inconel 600 Cold Rolled Plate. We offer Din 2.4816 Coils in various sizes at best price. We are leading manufacturer of Inconel alloy 600 strip & Inconel 600 Sheet.

 

Inconel 600 plate is a commonly used chromium and nickel austenitic steel alloy plate, which is non-magnetic in nature. These Inconel 600 plate | UNS N06600 is also being considered in advanced reactor concepts because of its high allowable design strength at elevated temperatures, especially between the ranges of 1200 Degree F – 1400 Degree F (649 Degree C – 760 Degree C). Inconel 600 plate maintains excellent mechanical properties and strength even at elevated temperatures, making it suitable for high-temperature applications. ASME SB 168 UNS N06600 Sheets resist oxidation and creep deformation at high temperatures, ensuring durability and reliability in demanding conditions. The Inconel 600 plate is easy to fabricate, allowing for convenient shaping, cutting, and welding to meet specific project requirements. ASTM B168 UNS N06600 plate is also said to be resistant to oxidation. Hence it is suitable for applications and services that are prone to oxidation.

 

We, at JN Alloys, develop and sustain quality and advancement and direct them in our items through persistent endeavors and quality control. UNS N06600 Hot Rolled Plate has a high tensile strength since they are treated with solution strengthening process and precipitation hardening process. The high resistance to oxidation is due to the content of chromium in it whereas the resistance to corrosion in Inconel 600 Cold Rolled Plate is due to the high content of base element nickel. We have been producing and supplying these plates for generations now. These Inconel 600 Sheet and Plates highlights astounding disintegration resistance, high versatility level and sturdiness. Further, these are available in different sizes as indicated by the requirements of our clients. We benefit our clients a superior quality item profile, helping them to pick a reasonable one for their industry. We are an ISO 9001: 2015 ensured organization, committed to building and managing client situated engagements.

 

Inconel 600 Sheet Specifications

 

Grade

Inconel 600 | UNS N06600

Standard

ASTM B168 / ASME SB168

Thickness

0.1mm To 100 mm

Size

1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form

Sheets, Plates, Coils, Slatting Coils, Perforated Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

ASME SB 168 UNS N06600 Sheet Chemical Composition

 

Alloy

C

Mn

Si

S

Cu

Fe

Ni

Cr

Grade 600

0.15 maximum

1.00 maximum

0.50 maximum

0.015 maximum

0.50 maximum

6.00 – 10.00

72.00 min

14.00 – 17.00

 

Alloy 600 Plate Mechanical Properties

 

Grade

Density

Melting Range

Tensile Stress

Yield Stress (0.2%Offset)

Elongation

Alloy 600

8.47 g/cm3

1413 °C (2580 °F)

Psi – 95,000 , MPa – 655

Psi – 45,000 , MPa – 310

40 %

 

Alloy 600 Plate Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

Inconel 600

2.4816

N06600

NCF 600

NA 13

МНЖМц 28-2,5-1,5

NC15FE11M

NiCr15Fe

 

Uses Of ASTM B168 UNS N06600 Plate

 

Steam Generators: Utilized for its high temperature and corrosion resistance properties.

Chemical Processing: Resistant to corrosion in aggressive chemical environments.

Food Processing: Employed in equipment and components for its corrosion resistance and hygiene factors.

Superheaters: Used in the construction of superheaters in power plants due to their high-temperature strength.

Jet Engines: Applied in components exposed to high-temperature and corrosive conditions in aviation.

Electronic Parts: Used for its high-temperature strength and resistance in electronic applications.

Come To Us