Inconel 600 pipe

 

JN Alloy is a distributor and manufacturer of Inconel 600 Pipe, ASTM B474 UNS N06600 Tube, Inconel 600 Tube, 2.4816 Inconel 600 Tube, Inconel 600 Tube, Inconel 600 Material, Inconel 600 Tubing and Inconel 600 Seamless Tubing.

 

Nickel Alloy 600 pipe, also known as Inconel 600 pipe, is an extremely versatile nickel-chromium alloy capable of resisting oxidation in temperatures up to 2000 ºF (1093 ºC). It's also used in cryogenic environments, thanks to a minimum of 72% Nickel combined with chromium in its chemical composition. It exhibits corrosion resistance to both organic and inorganic compounds, as well as chloride-ion stress induced cracking. Nickel Alloy 600 is used in a variety of critical applications that require protection from corrosion and heat. It consists of 72% Nickel, 14-17% Cr, 6-10% Fe, 1% Mn, and 0.5% Si. Inconel 600 Pipe is a nickel-chromium alloy with good oxidation resistance to 2000 degree F. Inconel Alloy 600 Pipe has good strength and resistance to general corrosion in a variety of elements and Resists stress-corrosion cracking. In comparison to welded pipes, the seamless variety can bear a pressure of about 20% higher. Hence, the specified seamless quality ASME SB 167 UNS N06600 pipe are compatible with applications that have the need for general corrosion resistance. The temperature range for this alloy is from 2000 °F right down to cryogenic temperatures. It is their heat resistance properties also make them attractive for several businesses.

 

Our offered Inconel 600 Seamless Pipe orInconel 600 Welded pipe commonly used for thermocouple, furnace muffles, heat exchangers, food processing.Alloy 600 Pipe stock size range is OD:.125″ – 4″and schedule Sch10 – Sch80.Our ability to provide Inconel Alloy 600 Seamless Pipe on a project basis is one of our strongest capabilities and is unmatched in our industry.We are able to provide Inconel Alloy 600 pipes of all sizes and compositions. Some sizes and compositions that are standardized (e.g. by ASTM, AMS and BS) are already in stock in our storages around the world.Our in-stock selection of Inconel 600 piping products covers a wide range of alloys, sizes and forms. Inconel 600 Round Pipes extensive use in the energy and nuclear power markets. The Alloy 600 Seamless Tube is produced through a cold rolling procedure and has less absolute roughness and high dimensional precision. These pipes are suitable for instrumental applications. The pipes are specialized for larger diameter pipes. Jinie Technology (Jiangsu) Co., LTD has an enviable reputation as a supplier of high quality Inconel 600 pipe in China.

 

Standard Specification For Inconel 600 Pipes & Tubes

 

Standards

Astm b474, ASTM B163, ASTM / ASME B167, B517, B516 / SB167, SB517, SB516

Outer Diameter

6.00 mm OD up to 914.4 mm OD, Sizes up to 24" NB

Thickness

0.3mm – 50 mm

Type

Seamless / ERW / Welded Pipes

Schedule

SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS

Seamless Pipes & Tubes Size

1 / 8″ NB – 24″ NB

ERW Pipes & Tubes Size

1 / 8″ NB – 36″ NB

Length

Single Random, Double Random & Required Length

 

ASTM B163 N06600 Tubing Chemical Composition

 

Grade

C

Mn

Si

S

Cu

Fe

Ni

Cr

Inconel 600

0.15 max

1.00 max

0.50 max

0.015max

0.50 max

6.00 – 10.00

72.00 min

14.00 – 17.00

 

Nickel Alloy 600 Tubes Mechanical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Inconel 600

8.47 g/cm3

1413 °C (2580 °F)

Psi – 95,000 , MPa – 655

Psi – 45,000 , MPa – 310

40 %

 

2.4816 Alloy 600 Tube Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

Inconel 600

2.4816

N06600

NCF 600

NA 13

МНЖМц 28-2,5-1,5

NC15FE11M

NiCr15Fe

 

ASTM B163 Inconel 600 Seamless Tubes Applications

 

Jet Engine exhaust systems
Sour gas production tubes
Motor racing exhaust systems
Nuclear waste reprocessing equipment
Chemical Processing
Chimney Linings
Aerospace equipment
 