Incoloy 825 plate
JN Alloy is largest Stockiest of Incoloy 825 Plate supplier with huge inventory of Alloy 825 Hot Rolled Plate, ASTM B424 UNS N08825 Polished Plate and Incoloy 825 Cold Rolled Plate. We offer Din 2.4858 Coils in various sizes at best price. We are leading manufacturer of Incoloy Alloy 825 strip & Incoloy 825 Sheet.
Incoloy 825 sheet is ductile over different temperatures right from cryogenic range to temperatures up to 1000 degrees C. The fabricability of the Incoloy 825 sheet allows it to be easily welded and formed within the system. Chemically, Incoloy 825 plate is an alloy that contains 74% Nickel, 15.5% Chromium and 8.0% iron with additions of copper, molybdenum, and titanium, a combination which gives the alloy good heat resisting properties. The content of chromium and molybdenum along with nickel in Werkstoff Nr. 2.4858 plate gives the alloy a high level of resistance to chloride related stress cracking and pitting. The Incoloy Alloy 825 Cold Rolled Plate is processed further after the initial hot-rolling process to give it superb hardness, enhanced properties coupled with a superior surface finish. The Incoloy 825 plate has 662MPa minimum tensile strength and 338MPa minimum yield strength when annealed whereas Alloy 825 Sheet has 758MPa minimum tensile strength and 421MPa minimum yield strength when annealed. The Inconel 825 plate possesses some good mechanical properties from the cryogenic to the moderately high-temperature range. However, when the material is exposed to a temperature above 540 degrees C, its microstructure can change, resulting in lower ductility and reduced impact strength. However, the Alloy 825 sheet can be strengthened by using the process of cold work substantially. It has a good impact strength at room temperature and can retain it even at cryogenic temperatures.
JN Alloys is a leading manufacturer of these sheets and plates and we supply them in all sizes. Our company has an illustrious clientele that increases to market in several countries, and is recognized as an innovator in the market when it comes to their products and finishing excellent quality. The Nickel Alloy 825 Plate are essentially narrow versions of the plates and sheets. The strips are used to create pipes and to line other material made applications. The material is a high nickel alloy that has molybdenum, titanium and niobium along with chromium. This composition makes the uns n08825 sheet operable under high temperatures up to 870 degrees Celsius. The DIN 2.4858 Plate is used in applications where the strength and corrosion resistance are the prime concerns. JN Alloys all-round group of professionals with highly effective background moments and comprehensive experience in manufacturing and managing of Inconel 825. The business also has an worldwide level revenue staff that carefully works with customers all over China and worldwide.
Incoloy 825 Plate Specification
|
Specifications |
ASME SA168 / ASTM A168 |
|
Form |
Blank (Circle), Rolls, Rolling Sheet, soft annealed, Rolling Plate, Flat Sheet, tread plate, Flats, Clad Plate, Sheet, annealed, sheared, descaled, Flat Shim, Plain Sheet, Plate, Strip, Checker Plate, Coils, Shim Sheet, Foils |
|
Standard |
ASME, API snd ASTM |
|
Finishs |
Cold rolled sheet, 2B, Hot rolled plate, 2D, SATIN, BA NO(8) |
|
Thickness |
4.0mm upto 100mm |
|
Hardness |
Half Hard, Soft, Spring Hard, Hard, Quarter Hard |
|
Specialize in Alloy 825 Plate Suppliers |
Perforated Sheets, Shim Sheet, B. Q. Profile. |
Chemical Composition of Incoloy Alloy 825 Sheet & Plate
|
Grade |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
Al |
Ti |
|
Incoloy 825 |
0.05 max |
1 max |
0.5 max |
0.03 max |
1.50 – 3 |
22.00 min |
38 – 46 |
19.50 – 23.50 |
0.02 max |
0.06 – 1.20 |
Mechanical Properties of Incoloy 825 Sheet & Plates
|
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
8.14 g/cm3 |
1400 °C (2550 °F) |
Psi – 80,000 , MPa – 550 |
Psi – 32,000 , MPa – 220 |
30 % |
Incoloy 825 Plates Equivalent Grades
|
STANDARD |
WERKSTOFFNR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
OR |
|
Incoloy 825 |
2.4858 |
N08825 |
NCF 825 |
NA 16 |
ЭП703 |
NFE30C20DUM |
NiCr21Mo |
XH38BT |
Din 2.4858 Incoloy 825 plate applications including
Radioactive waste handling
Calorifiers
Oil and gas recovery
Pollution control
Hot vessels for food, water, and seawater
Chemical processing
Nuclear fuel reprocessing
Marine exhaust systems
Pickling tank heaters, tanks, and equipment Acid production