Incoloy 825 pipe

 

JN Alloy is a distributor and manufacturer of Incoloy 825 Pipe, UNS N08825 Tube, Incoloy 825 Tube,2.4858 Incoloy 825 Tube, Incoloy 825 Pipe, Incoloy 825 Material, Incoloy 825 Tubing and Incoloy 825 Seamless Tubing.

 

Incoloy 825 Tube is made up of 38% nickel and 19% chromium in its composition. The Alloy 825 Tube therefore is resistant to many corrosive media, strong and is high heat resistant. Incoloy 825 is one of the most effective alloy choice for severe environments. Its usefulness in varying climate, especially with regards to general and local corrosion makes the Incoloy WERKSTOFF NR. 2.4858 Pipe in industries such as - chemical processing, pickling operations, pollution control, acid production, nuclear fuel reprocessing, as well as the handling of radioactive wastes. According to most Incoloy 825 Seamless Pipe manufacturer, the industry that reaps the benefits of this alloy is the oil and gas industry, where they are useful in the recovery, extraction and conveyance of media across. ASTM B423 UNS N08825 maintains its austenitic structure even after being exposed to high temperatures for a prolonged period of time. Incoloy 825 Seamless Pipe manufacturers have designed these pipes to resist oxidizing and reducing environments along with being resistant to sulfur rich environments. These pipes are also resistant to chloride-ion stress corrosion cracking. ASTM B423 UNS 8825 offers high tensile strength and ductility. They can work in a wide range of temperatures from 1000 degrees F to cryogenic. The material used in these pipes is easy to form and weld.

 

Jinie Technology (Jiangsu) Co., LTD is manufacturing and supplying a wide range of Incoloy 825 Pipes and tubes to domestic as well as global clients. We develop these using high-quality raw materials. We use the latest technology, which is regularly maintained to produce flawless products. The ASME SB 423 UNS N08825 pipes produced are tested for several mechanical properties like tensile and yield strength, elongation along with both non-destructive electric and hydrostatic tests. These hot finished or cold worked ASTM B423 UNS N08825 pipes are well suited for use in applications that demand the need for general corrosion resistance properties. Regular welded pipes are susceptible to intergranular corrosion. However, the Incoloy 825 Welded Pipe resists getting sensitized by grain boundary precipitates and in turn, is resistant to intergranular corrosion. This is an effect of the presence of titanium and the corresponding heat treatment. The outstanding resistance to corrosives in reducing environments has been attributed to the presence of copper in the Alloy 825 Pipe. Whereas the inclusion of nickel not only improves the high temperature properties of the metal but also is the reason why the Incoloy 825 Pipe is sufficiently able to combat chlorine related stress corrosion. Jinie Technology (Jiangsu) Co., LTD has well qualified and sincere employees that are working with dedication to provide dimensionally accurate pipes and tubes with perfect finishing.

 

ASME SB 423 UNS N08825 Incoloy Seamless Pipe Specification

 

Incoloy 825 Pipe International Specification

ASTM B423, ASTM B775,ASTM B705, ASTM B829, ASTM B704, ASTM B163, ASTM B751

ISO 6207, DIN 17751

Standard Specification

ASME, ASTM, AISI, AMS, JIS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB

Incoloy 825 Seamless Pipe Size

OD: 4 to 219mm

Wall Thickness: 0.5 to 20mm

ASME SB 423 UNS N08825 Incoloy Welded Pipe Size

OD: 5.0 - 1219.2 mm

Incoloy Alloy 825 EFW Pipe Size

OD: 5.0 - 1219.2 mm

Incoloy 825 Alloy Pipe WT

SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS

Nickel Alloy 825 Pipe manufacturing techniques

Seamless / ERW / EFW/ Welded / Fabricated / CDW/ LSAW/ Seam-Welded / Redrawn

Origin of Incoloy N08825 pipe material

Indian, European, Korean, Japanese

Werkstoff 2.4858 Incoloy Pipe End Types

BE : Beveled end

BBE : Bevel both ends

BLE : Bevel large end

BSE : Bevel small end

TOE / POE = Threaded One End / Plain One End

TOE / BOE = Threaded One End / Beveled One End

POE / BOE = Plain One End / Beveled One End

TBE = Threaded Both Ends

PBE = Plain Both Ends

Form

Round, Square, Rectangular

Incoloy 825 Din 2.4858 Pipe Length

Single Random, Double Random & Required Length End: Plain End, Beveled End, Threaded

UNS N08825 Incoloy 825 Pipe Delivery Condition

Annealed and Pickled, Hot Finished, Polished, Bright Annealed, Cold Drawn

Incoloy 8825 Pipe Packing

Ply Wooden Boxes

PE Fabric Bundles

Steel Strips Bundled

Standard seaworthy export packing

Plastic Bags, or as required

 

UNS N08825 Welded Pipe Chemical Properties

 

Grade

C

Mn

Si

Fe

S

Cr

Cu

Ti

825

min.

–

–

–

22.0

–

19.5

1.5

0.6

max.

0.05

1.0

0.5

–

0.015

23.5

3.0

1.2

 

Incoloy Alloy 825 Round Pipe Properties Table

 

Grade

Tensile Strength (MPa) min

Yield Strength 0.2% Proof (MPa) min

Elongation (% in 50mm) min

Hardness

Rockwell B (HR B) max

Brinell (HB) max

825

Psi – 80,000 , MPa – 550

Psi – 32,000 , MPa –220

30

–

–

 

Incoloy 825 Welded Pipe Equivalent

 

Grade

UNS No

Old British

Euronorm

GOST

Japanese JIS

BS

En

No

AFNOR

Incoloy 825

N08825

NA 16

NiCr21Mo

2.4858

NFE30C20DUM

ЭП703

NCF 825

 

Applications for Incoloy 825, Nickel Alloy 825, UNS N08825

 

1. Chemical industry: Incoloy 825 pipe is widely used in corrosive environments in chemical processes, such as sulfuric acid production, acid and alkali treatment, chloride manufacturing, etc.
2. Marine engineering: Due to its strong corrosion resistance to seawater and salt water, Incoloy 825 pipe is often used in seawater treatment devices, offshore oil exploration, etc. in marine engineering.
3. Energy industry: Incoloy 825 pipes can be used in heat exchangers, refining units, etc. in the fields of oil, natural gas, and petrochemical industries.
4. Food industry: Since the Incoloy 825 pipe has strong resistance to the acidic environment of food, it can also be used in acidic food processing and storage equipment in the food industry.
In short, Incoloy 825 pipe has important applications in chemical, marine, energy, and food fields due to its good corrosion resistance, high-temperature performance, and welding performance.
 