Incoloy 800HT plate

 

JN Alloy is largest Stockiest of Incoloy 800HT Plate supplier with huge inventory of Alloy 800HT Hot Rolled Plate, ASTM B409 UNS N08811 Polished Plate and Incoloy 800HT Cold Rolled Plate. We offer Din 1.4859 oils in various sizes at best price. We are leading manufacturer of Incoloy Alloy 800HT strip & Incoloy 800HT Sheet.

 

Incoloy 800HT Plate are high-performance superalloys. The Incoloy 800ht Plate is designed with a superior chemical composition of 30-35% nickel, 19-23% chromium, and iron content above 39.5%. The Alloy 800ht Plate is stabilized by titanium and offers excellent creep strength in temperatures ranging up to 1290 degrees F. Alloy 800HT Sheets is a widely used material of construction for equipment that must have high strength and resist carburization, oxidation and other harmful effects of high-temperature exposure. Chemical composition present in the Incoloy 800HT are chromium, aluminum, titanium, manganese and silicon are some of the essential component present in the grade that is useful in offering the excellent corrosion to resistance property. The alloy is widely used in high temperature environment due to its excellent highly unmatched properties and specifications. There are many Incoloy 800HT grades available in the markets that are used in fabricating good quality of sheets and plates.

 

JN Alloys develop and support quality and advancement and direct them in our items through nonstop endeavors and quality control. We benefit our clients a top notch quality item profile, helping them to pick an appropriate one for their industry. We are an ISO 9001: 2015 ensured organization, committed to building and managing client situated engagements. The Incoloy 800ht sheet is welded and processed following standard shop fabrication processes. These sheets can be solid-solution hardened, work-hardened, and precipitation hardened. We are a producer, merchant, stockist, provider and exporter of Inconel 800HT Plates, which contain a squeeze of Aluminum and Titanium, giving them great crawl quality at higher temperatures. The Petrochemical and warmth treatment offices utilize UNS N08811 Incoloy 800HT Plates as they withstand high-temperature erosion and oxidation. Our WNR 1.4959 Incoloy 800HT Plates can be effortlessly machined and are impervious to sulphidation and carburization, with a rigidity of 531 Mpa, passing on the plates to work in the power era and oil refining industry.

 

ASTM B168 Incoloy 800Ht Sheets, Plates Specification

 

Specifications

ASTM B409 / ASME SB409

Width

1000mm / 1219mm /1250mm / 1500mm / 2000mm

Length

2000 mm / 2440 mm / 2500 mm / 3000 mm / 6000 mm

Thickness

0.1mm to 12 mm Thk

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish

Hot rolled plate (HR), Cold rolled sheet (CR)

Form

Coils, Foils, Rolls, Plain Sheet, Strip, Flats, Blank (Circle), Ring (Flange) etc.

 

Alloy 800Ht Chequered Plate Equivalent Grade

 

STANDARD

WERKSTOFF NR.

UNS

Incoloy 800HT

1.4859

N08811

 

Incoloy 800Ht Cold Rolled Sheets Chemical Composition

 

Grade

Cr

Fe

Ni

C

Mn

Cu

Si

S

Incoloy 800HT

19.5 – 23.5

1.0 max

38.0 – 46.0

0.05 max

1.0 max

1.5 – 3.0

0.5 max

0.03 max

 

Alloy 800Ht Polished Cold Drawn Plates Mechanical Properties

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

8.47 g/cm3

1413 °C (2580 °F)

Psi – 95,000 , MPa – 655

Psi – 45,000 , MPa – 310

40 %

 

Incoloy 800HT Plates sheets Applications Industry

 

Chemical tanks

Pulp & Paper Industries

Petrochemical Industries

Power Generation Industries

Oil & Gas Industries

Desalination

Architecture and Construction

Food Processing Equipment

Biofuels plant

Cargo tanks for ships and trucks

Chemical Industries Pumps, fans, centrifuges, sulphur melting coils,

Digester in sulphate and sulfite plants, blow tanks, blow lines

Come To Us
And Start Your RFQs Now.
contact us