Incoloy 800 plate
JN Alloy is largest Stockiest of Incoloy 800 Plate supplier with huge inventory of Alloy 800 Hot Rolled Plate, ASTM B409 UNS N08800 Polished Plate and Incoloy 800 Cold Rolled Plate. We offer Din 1.4876 Coils in various sizes at best price. We are leading manufacturer of Incoloy alloy 800 strip & Incoloy 800 Sheet.
Incoloy 800 Sheets(UNS N08800 Sheets) is a widely used material of construction for equipment that must have high strength and resist carburization, oxidation and other harmful effects of high-temperature exposure. It has improved creep and stress-rupture characteristics in the 1100 Degree F (593 Degree C) to 1800 Degree F (982 Degree C) temperature range. Nickel 800 Sheets are also used for chemical and petrochemical processing. The chemical composition of Incoloy 800 alloy plate consists mainly of nickel, chromium and iron. Among them, nickel is the main element that improves the corrosion resistance of the alloy, chromium helps enhance the oxidation resistance and high-temperature strength of the alloy, and iron provides the matrix structure of the alloy. In addition, the alloy also contains certain amounts of elements such as carbon, silicon and manganese to further enhance its overall performance. Incoloy 800 alloy plate has very good corrosion resistance, especially in reducing and oxidizing media. It also has good resistance to chemicals such as sulfuric acid, hydrochloric acid and alkaline solutions in high temperature environments. Incoloy 800 plate has good oxidation resistance in high temperature environments and can work at temperatures up to 1100°C for a long time. Lastly, Incoloy 800 plate has high yield strength and creep strength and can maintain its mechanical properties in high and low temperature environments.
JN Alloys Distributor of Incoloy Alloy 800 Sheet & supplies DIN 1.4876 Incoloy Coils to internationally approved quality standards for applications.We are well-known Exporter of Incoloy Alloy 800 Plate in China and have excellent quality to fully satisfy customer's requirements. Our commitment to service is recognized worldwide make us well known trader of 800 Incoloy plate in China.We have been Supplier of Incoloy 800 plate for more than 19 years and have developed the resources, skills and inventory to satisfy the demanding needs of a multitude of markets. We offer Incoloy 800 Coils in various sizes at best price which helps us to prove one of the best stockholder 800 Alloy Plate in China.
ASTM B409 Incoloy 800 plate Product Specifications
|
Type |
sheared, Flats, descaled, Plate, Foils, Coils, annealed, Strip, Rolls, Sheet, Clad Plate, Checker Plate, Rolling Plate, Plain Sheet, Rolling Sheet, Flat Shim, Shim Sheet, Flat Sheet, soft annealed, Blank (Circle), tread plate, |
|
Grade |
Nickel Iron Chromium Alloy 800 - UNS N08800 - Incoloy 800 |
|
Length |
0-12 millimeter or as per need |
|
Specification of Incoloy 800 Plate |
ASTM B409 UNS N08800, ASME SB409, MSRR, BS, AMS 4544 sheet |
|
Width of Alloy 800 Plate |
0 millimeter to 2500 millimeter or as per need |
|
UNS N08800 Plate Thickness |
0.3 millimeterto 1200 millimeter or as per need |
|
Plate Process |
Hot/ Cold Rolled |
|
Plate surface |
No.1 finish hot rolled ASTM B409 Alloy 800 Plate, No. 2D, BA, No.1, No. 2B, No.4, No.3, No.7, No.6, 2D, 2B, mirror, BA NO(8), Hot rolled plate , hairline, brush, SATIN, 1D, Cold rolled sheet (CR), 8K, satin etc. |
Incoloy 800 Plate, Sheet & Coil Chemical Composition
|
Grade |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
Al |
Ti |
|
800 |
0.10 max |
1.50 max |
1.00 max |
0.015 max |
0.75 max |
39.50 min |
30.00 – 35.00 |
19.00 – 23.00 |
0.15 – 0.60 |
0.15 – 0.60 |
ASTM B409 UNS N08800 Plate Mechanical Properties
|
Element |
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
|
800 |
7.94 g/cm3 |
1385 °C (2525 °F) |
Psi – 75,000 , MPa – 520 |
Psi – 30,000 , MPa – 205 |
30 % |
Incoloy 800 Plate Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
EN |
OR |
|
Incoloy 800 |
1.4876 |
N08800 |
NCF 800 |
NA 15 |
ЭИ670 |
Z8NC32-21 |
X10NiCrAlTi32-20 |
XH32T |
Nickel alloy 800 sheet Application Industries
Chemical industry
Nuclear Engineering
Aerospace
Gas turbine components
Heat treating industry
Fertilizer Industry
Pulp and paper industry
Petro Chemical Industry
Food processing