Hastelloy X plate

 

JN Alloy is largest Stockiest of Hastelloy X Plate supplier with huge inventory of Alloy X Hot Rolled Plate, ASTM B435 UNS N06002 Polished Plate and Hastelloy X Cold Rolled Plate. We offer Din 2.4665 Coils in various sizes at best price. We are leading manufacturer of Alloy X strip & Hastelloy X Sheet.

 

Alloy X Plate is an austenitic nickel base alloy containing approximately 22 percent chromium for outstanding resistance to oxidation at high temperatures. In addition, Hastelloy X Sheet, which is solid solution strengthened, possesses exceptional strength at elevated temperatures. Hastelloy X Coil has good high temperature and stress rupture properties above 1450°F and can be used for applications up to 2200°F. In addition Hastelloy X Clad Plate contains high levels of nickel and molybdenum providing good levels of corrosion resistance similar to high nickel alloys more customarily used in corrosion applications. The plate form of this versatile metal alloy has some special traits that make it a top choice for extreme environment parts. Hastelloy X Plate is an iron – molybdenum – nickel – chromium alloy that holds an excellent grouping of oxidation resistance, high temperature power and formability. The mixture of metals like nickel, chromium, iron, and molybdenum grants Hastelloy X plate outstanding load-bearing abilities. Parts crafted from these rugged plates stand up to heavy loads without bending or cracking. They also handle vibration very well over long periods.

 

This durability is vital for gear in settings with continuous operation. A major benefit of ASME SB435 Hastelloy X Sheet is that it retains mechanical properties at very high temperatures, up to 1800°F. This means plates keep a big fraction of strength even when red hot. This thermal resistance results from elements in its metal makeup reinforcing the nickel matrix. Parts made from plates thus survive and function in hot furnace areas that quickly wear out regular steel.

 

JN Alloys offers a variety of specifications for the highly demanding HASTELLOY X PLATE. These plates are made of HASTELLOY X grade, which has better plate quality enhancement. Numerous industries rely heavily on our plates, which come in a variety of sizes and specifications. These plates are thicker and harder with magnificent strength. In addition, we provide adaptability in dimension and size based on the application. In addition, we provide plates at various quality levels at low prices. Additionally, these plates are chosen for use at higher temperatures. It can be easily made into a variety of shapes and sizes. Likewise, these plates are joined with hostile to eroding properties with a huge warm reach. Once the fabrication of these sheets is done, we sent them for inspection so that they don't have any damage or scratches on them. Various Destructive and Non Destructive Testing is carried out on these Sheets as well as plates including the Hardness test, Fatigue test, Tension test, Bend test, Flattening test, Flaring resistance. We also see to it that these Sheets, Plates are packed appropriately, to avoid destruction during transit.

 

Hastelloy X Sheet & Plate Specification

 

Alloy X Plate Specification

ASTM B435 UNS N06002, ASME SB435, MSRR, AMS, BS

Grades

Hastelloy X Plate, Hastelloy N Plate, Hastelloy S Plate and sheet.

Hastelloy X Plate Sizes

1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Hastelloy X Plate Thickness

0.1mm to 100 mm Thk

Hastelloy X Plate Width

10-2500mm

Hastelloy X Plate Length

2m, 2.44m, 3m, or as required

Hastelloy X Sheet ASTM

ASTM B435

Hastelloy X Sheet AMS

AMS 5536

Hastelloy X Plate Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Hastelloy X Sheet Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Hastelloy X Plate Stock in form of

Hastelloy X Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate

Material

JIS: N0, N2, N1, NW2200, NW2201, NW4400, NW5500, NW6002, etc
DIN:H-Ni99.96, H-Ni99.95, H-Ni99.92, H-Ni99.90, H-Ni99.5, H-Ni99, etc

Hastelloy X Plate ASTM Standard

ASTM A162, GB/T2054, DIN177502002, ASTM B127, ASTM B435, ASTM B582, ASTM B575, ASTM B168, ASTM B443, ASTM B463, ASTM B626, ASTM B536, etc

Hastelloy X Plate Dimensions

As the customer required

Hastelloy X profiling

To provide a full profiling service we use numerous profiling methods including:

Laser Plate Cutting

Plasma Plate Cutting

Oxy-propane Flame Cutting

 

Hastelloy X Plates Chemical Composition

 

Grade

Al

C

Mn

Co

S

Si

Cr

Mo

Fe

W

B

Co

Ti

Cu

P

Hastelloy X

50 max

.05-.15

1.0 max

1.0 max

03 max

1.0 max

20.5-23.0

8.0-10.0

17.0-20.0

2-1.0

01 max

5-2.5

15 max

50 max

04 ma

 

ASTM B435 Hastelloy X Plates Mechanical Physical Properties

 

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Hastelloy X

8.22 g/cm³

1355°C

655 MPa

240 MPa

35%

 

Hastelloy X Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Hastelloy X

2.4665

N06002

 

Hastelloy X plates applications

 

Off-Shore Oil Drilling Companies

Pharmaceutical Equipment

Power Generation

Chemical Equipment

Petrochemicals

Sea Water Equipment

Gas Processing

Heat Exchangers

Specialty Chemicals

Condensers

Pharmaceuticals

Pulp and Paper Industry

 

Come To Us
And Start Your RFQs Now.
contact us