Hastelloy G30 plate

 

JN Alloy is largest Stockiest of Hastelloy G30 Plate supplier with huge inventory of Alloy G30 Hot Rolled Plate, ASTM B575 UNS N06030 Polished Plate and Hastelloy G30 Cold Rolled Plate. We offer Din 2.4603 Coils in various sizes at best price. We are leading manufacturer of Alloy G30 strip & Hastelloy G30 Sheet.

 

Hastelloy G30 plate is known for its impressive tensile and yield strength, making it perfect for demanding industrial applications. Tensile strength is the maximum stress a material can withstand while being stretched or pulled before breaking, while yield strength is the stress at which it starts to deform plastically. These characteristics ensure Hastelloy G30 plate can handle significant loads without permanent damage, even in tough environments like chemical processing and power generation. The alloy G30 has good fatigue resistance means it can withstand repeated mechanical stresses, ensuring long-term reliability in rotating equipment and vibrating systems. It retains its mechanical properties over a wide temperature range, making it suitable for high-temperature applications like heat exchangers and reactors. Hastelloy G30 plate hot working involves forming the alloy at elevated temperatures, typically between 1800°F and 2150°F (982°C to 1177°C). This method helps shape the alloy while ensuring it retains its key properties, such as ductility and toughness. The resistance of the alloy to the formation of grain boundary precipitates in the heat-affected zone makes it suitable for use in most chemical process applications in the as-welded condition.

 

JN Alloys is a trusted supplier of high-quality Hastelloy G30 plates in China. Our Hastelloy G30 plates are known for their exceptional resistance to a wide range of corrosive chemicals, making them suitable for use in various industrial applications, Our Hastelloy G30 plates are manufactured using top-grade raw materials and cutting-edge technology, ensuring superior quality and performance. These plates are highly resistant to corrosion, oxidation, and environmental cracking, making them ideal for use in harsh environments, With a strong focus on product quality and customer satisfaction, we take pride in offering competitive prices and reliable delivery services for our Hastelloy G30 plates. Whether you require standard sizes or custom dimensions, we have the capabilities to meet your specific requirements, Choose JN Alloys as your reliable supplier of Hastelloy G30 plates in China and experience the difference in quality and service. Contact us today to learn more about our products and services.

 

Nickel Alloy G30 Plate Specification

 

Specifications

ASTM B581/B619/B366/B626

Size

1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Thickness

0.1mm to 12 mm Thk

Form

Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Finish

Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

 

2.4603 Hastelloy Plate Chemical Composition

 

Element

Content (%)

Nickel, Ni

43

Chromium, Cr

28.0-31.5

Iron, Fe

13-17

Cobalt, Co

5

Molybdenum, Mo

4-6

Tungsten, W

1.50 - 4

Manganese, Mn

1.50

Copper, Cu

1 - 2 .40

Silicon, Si

0.8

Phosphorous, P

0.040

Carbon, C

0.030

Sulfur, S

0.020

 

Hastelloy Alloy G30 Plate Mechanical Properties

 

Properties

Metric

Imperial

Tensile strength

1096 MPa

159000 psi

Yield strength (@0.2%)

1000 MPa

145000 psi

Modulus of elasticity (plate heat treated to 1177°C, rapid quenched)

202 GPa

29300 ksi

Elongation at break (in 50.8 mm)

12%

12%

Reduction of area

57%

57%

Hardness, Brinell (converted from Rockwell C hardness)

304

304

Hardness, Knoop (converted from Rockwell C hardness)

326

326

Hardness, Rockwell C

32

32

Hardness, Vickers (converted from Rockwell C hardness)

316

316

 

Hastelloy G-30 Sheet, Plate & Coil Physical Properties

 

Properties

Metric

Imperial

Density

8.22 g/cm³

0.297 lb/in³

Melting point

1371ºC

2500ºF

 

Hastelloy G30 Plate Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

Hastelloy G30

2.4603

N06030

 

Applications of Hastelloy G-30 UNS N06030 plate

 

Phosphoric acid equipment

Fertilizer production

Pickling operations

Nuclear fuel reprocessing

Sulphuric acid equipment

Pesticide production

Petrochemical products

Nuclear waste disposal

Nitric acid equipment

Gold extraction

 