Hastelloy G30 Tubing is corrosion resistant alloy with excellent corrosion resistance to oxidizing environments. Hastelloy G30 Tube has been very successful as phosphoric acid heat exchanger tubing and for other process components in the fertilizer industry.The high chromium content of both of these Hastelloy G30 Pipe make them the premier choices for strong oxidizing solutions and mixed acid pickling services. Hastelloy G30 Seamless Tubes is a high Nickel based alloy which shows superior corrosion resistance over most other Nickel and Iron based alloys in phosphoric acids as well as many complex environments containing highly oxidising acids such as nitric, hydrofluoric and sulphuric. Hastelloy G30 Welded Pipes has good ductility, high corrosion resistance even in the welded condition, and prevents corrosion by nitric, phosphoric and sulphuric acids. Hastelloy G30 Welded Tubes is a nickel – chromium – iron material highly resistant to "wet process" phosphoric acid. Hastelloy UNS N06030 Pipes are known throughout the chemical process industry as the premier corrosion resistant materials. The resistance of Hastelloy Din 2.4603 Tubes to the formation of grain boundary precipitates in the heat-affected zone makes it suitable for use in most chemical process applications in the as-welded condition.
Jinie Technology (Jiangsu) Co., LTD is a known stockist and manufacturing house of Hastelloy G30 Tube, which is an improved version of nickel – chromium – iron molybdenum-copper alloy. Hastelloy G30 Tubes are used in environments with very high temperature above 540 Degree C (1000 Degree F) where deformation resistance and higha surface stability are chiefly required. Alloy G30 Tubes has many advantages over other metals and materials in handling phosphoric, sulphuric and nitric acids and in fluoride environments and oxidising acid mixtures. We have ready stock of Hastelloy G30 Seamless Tube and Hastelloy G30 Welded Tube in our stockyard.We are well known supplier and stockist of Hastelloy G30 Seamless Pipes.We have technical experts staff who have wide experience in dealing with Alloy G30 Seamless Tubing.
Hastelloy G30 Tube Specifications
|
Size |
15 NB to 150 NB IN |
|
Type |
Seamless / ERW / Welded / Fabricated / Hollow / LSAW Pipes |
|
wall thickness |
035" –.095′, (special wall thicknesses available) |
|
Schedule |
SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
|
Finish |
Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
|
Form |
Round, Square, Rectangular, Hydraulic, Straight or 'U' bent Tubes Etc |
|
Length |
Single Random, Double Random & Cut Length. |
|
End |
Plain End, Beveled End, Threaded. |
|
Surface Finish |
1/2 inch through 1" tubing is mechanically polished with an inner diameter (ID) of 20 Ra µ-inch (0.5 µm) |
|
Outer diameter (OD) of 32 µ-inch (0.8 µm). |
|
|
1-1/2 and 2 inch Alloy G30tubing is available with a sanitary finish that is better than traditional commercial grade tube finish, and suitable for applications in sanitary/ high purity hygienic industries. |
|
|
3 inch Alloy G30tubing is available with a mill finish ID and OD. |
|
|
Marking |
All s are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer's request.) |
|
We can also cut, thread, and groove Hastelloy G30 Tubes to meet your specifications. |
|
Hastelloy G30 Tube Chemical Composition,%
|
NI |
CR |
FE |
MO |
W |
CU |
NB |
CO |
MN |
SI |
C |
|
Balance |
30 |
15 |
5.5 |
2.5 |
2 |
0.8 |
5 max |
1.5 max |
0.8 max |
0.03 max |
Hastelloy G30 Tube Mechanical Properties
|
HASTELLOY GRADE |
TENSILE STRENGTH |
YIELD STRENGTH( 0.2% ) |
ELONGATION AT BREAK |
REDUCTION OF AREA |
|
G30 |
1096 MPa |
1000 MPa |
12% |
57% |
Hastelloy G30 Tube Equivalent Grade
|
STANDARD |
UNS |
WNR. |
|
HASTELLOY G30 |
N06030 |
2.4603 |
Hastelloy G30 pipe and tube Application field
Aero-engine: Hastelloy G30 pipe can be used to manufacture parts and components of aero-engines, such as turbine blades and turbine disks. These parts need to work in high-temperature environments and withstand high pressure and vibration loads, and Hastelloy G-30 can meet these requirements.
Gas turbine: Hastelloy G30 pipe can be used to manufacture parts and components of gas turbines, such as turbine blades and turbine disks. These parts need to work in high-temperature environments and withstand high pressure and heat loads, and Hastelloy G30 pipe provides excellent strength, hardness, and corrosion resistance.
Petrochemical industry: Hastelloy G30 pipe can be used to manufacture parts and components of petrochemical equipment, such as pipelines and valves. These equipment need to work in high-temperature environments and withstand the corrosive effects of acid and alkali liquids, while Hastelloy G30 pipe can provide good corrosion resistance.
Marine engineering: Hastelloy G30 pipe can be used to manufacture parts and components for marine engineering structures, such as components for offshore platforms and ship parts. These components need to work in seawater environments and withstand the erosive effects of high-strength and highly corrosive media, while Hastelloy G30 pipe provides excellent corrosion resistance and strength guarantees.