JN ALLOY supplies Hastelloy G30 SO flanges, Hastelloy G30 WN flanges, UNS N06030 blind flanges, 2.4603 Hastelloy G30 plain flanges, ASTM B564 UNS N06030 SW flanges, Hastelloy G30 spectacle blind flanges, Hastelloy G30 threaded flanges, 2.4603 spacer ring, UNS N06030 paddle blind/blank, Hastelloy G30 bleed/test/drip ring, Hastelloy G30 reducing flange.
Hastelloy G30 Flanges are composed of nickel, chromium, iron, cobalt, molybdenum, tungsten, and manganese. It is a high-performance alloy. Hastelloy G30 Flanges can withstand high temperatures without deforming. These flanges have high surface stability. Hastelloy G30 Flanges are used in an environment where resistance to deformation and high stability is highly needed. These flanges have characteristics like good fatigue performance, fracture toughness, and plastic. It also shows creep and oxidation resistance. Hastelloy G30 Flanges have physical properties such as density and melting point. These flanges also show mechanical properties at high temperatures and room temperatures, such as tensile strength, yield strength, and modulus of elasticity. Reduction of area and hardness are also some of its main characteristics. Flanges have thermal properties, linear coefficient of thermal expansion, and thermal conductivity. Hastelloy G30 Flanges offer very high resistance to the nitric acid and hydrofluoric acid solutions used in the pickling of stainless steel. At a temperature of 140°F or 60°C, this particular application needs to dilute 15% nitric acid and 5% hydrofluoric acid. It also provides great resilience to industrial phosphoric acid. These flanges are mostly used in the fertilizer industry as an acid evaporators. Hastelloy G30 Flanges are used in chemical processing. In this process, phosphoric acid, sulfuric acid, and nitric acid are involved. It is also used in gas scrubbers, acid production, pickling, petrochemical, nuclear fuel reprocessing, and nuclear gas processing. It is suitable to use in welded conditions.
Hastelloy G30 Flanges exhibit commendable tensile strength, durability, flexibility, and longevity. They capture the attention of our customers with their ease of fabrication, machinability, exemplary workability, and superior finish, contributing to their robust construction. At Jinie Technology (Jiangsu) Co., LTD, our commitment is to craft top-tier Hastelloy G30 flanges in sync with industry demands and evolving trends. Our rigorous adherence to international quality standards profoundly influences the manufacture of our entire flange range. Our unique, precision-based approach is evident in the production of our distinctive Hastelloy Long Weld Neck Flanges. We ensure all details, including sizes and dimensions, adhere to the highest accuracy, further cementing our commitment to quality.
Types Of Hastelloy G30 Flanges
|
Products |
Size |
|
|
ASTM B564 Hastelloy G30 Slip-On Flanges |
ASTM B564 Hastelloy G30 Weld Neck Flanges |
Sizes 1/8″ – 40″ |
|
ASTM B564 Hastelloy G30 Blind Flanges |
ASTM B564 Hastelloy G30 Lap Joint Flanges |
|
|
ASTM B564 Hastelloy G30 Threaded Flanges |
ASTM B564 Hastelloy G30 Socket Weld Flanges |
|
|
ASTM B564 Hastelloy G30 Plate Flanges |
ASTM B564 Hastelloy G30 Ring Joint Type Face (RTJ) Flanges |
|
|
ASTM B564 Hastelloy G30 Spectacle Blind Flanges |
ASTM B564 Hastelloy G30 High Hub Blind Flanges |
|
|
ASTM B564 Hastelloy G30 Orifice Flanges |
ASTM B564 Hastelloy G30 Reducing Flanges |
|
|
ASTM B564 Hastelloy G30 Square Flanges |
ASTM B564 Hastelloy G30 Groove & Tongue Flanges |
|
|
ASTM B564 Hastelloy G30 Long Neck Weld Flanges |
ASTM B564 Hastelloy G30 Spades and Ring Spacers Flanges |
|
|
ASTM B564 Hastelloy G30 Weldo / Nipo Flanges |
ASTM B564 Hastelloy G30 Expander Flanges |
|
Hastelloy g30 Flanges Specification
Material: ASTM B564 Standard Specification for Nickel Alloy Forgings
Standard: ASME B16.5, ASME B16.47, DIN, EN, BS, JIS
Size: 1/2"-48", DN6-DN400
Class: 150#,300#,400#,600#,900#,1500#,2500#
Hastelloy G30 Flange Chemical Composition
|
C |
Cr |
Co |
Fe |
Mn |
Mo |
Ni |
Si |
W |
Cu |
|
0.03Max |
30.0 |
5Max |
15.0 |
1.5Max |
5.5 |
Blance |
0.8Max |
2.5 |
2.0 |
Alloy G30 Flange Mechanical Properties
|
Tensile Strength |
Yield Strength |
Elongation |
||
|
ksi |
Mpa |
ksi |
Mpa |
% |
|
85 |
586 |
35 |
241 |
30 |
Hastelloy G30 Flange Equivalent Grades
|
STANDARD |
WERKSTOFF NR. |
UNS |
|
Hastelloy G30 |
2.4603 |
N06030 |
ASTM B564 Hastelloy G30 Flanges Weight Chart
|
Pipe Normal Diam. |
O.D. Flange |
Thk. Of Flange Min |
Diam. |
Diameter of Raised Face |
Length Hub.Y |
Thread Length |
Diam. |
Diam. |
Number |
Diam. of |
KG |
LB |
|
|
inch |
dn |
O |
C |
of |
G |
Y |
T |
of Bolt |
of Bolt |
of Bolts |
Bolts |
||
|
1/2" |
15 |
89 |
11.2 |
Hub |
35.1 |
15.7 |
15.7 |
Circle |
Holes |
4 |
(inch) |
0.4 |
0.9 |
|
3/4" |
20 |
98.5 |
12.7 |
38.1 |
42.9 |
15.7 |
15.7 |
69.9 |
15.8 |
4 |
1/2" |
0.7 |
1.5 |
|
1" |
25 |
108 |
14.2 |
49.3 |
50.8 |
17.5 |
17.5 |
79.3 |
15.8 |
4 |
1/2" |
0.8 |
1.8 |
|
1-1/4" |
32 |
117.5 |
15.7 |
58.7 |
63.5 |
20.6 |
20.6 |
88.9 |
15.8 |
4 |
1/2" |
1.2 |
2.6 |
|
1-1/2" |
40 |
127 |
17.5 |
65 |
73.2 |
22.4 |
22.4 |
98.6 |
15.8 |
4 |
1/2" |
1.5 |
3.3 |
|
2" |
50 |
152.5 |
19.1 |
77.7 |
91.9 |
25.4 |
25.4 |
120.7 |
19.1 |
4 |
5/8" |
2.3 |
5.1 |
|
2-1/2" |
65 |
178 |
22.4 |
90.4 |
104.6 |
28.4 |
28.4 |
139.7 |
19.1 |
4 |
5/8" |
3.7 |
8.1 |
|
3" |
80 |
190.5 |
23.9 |
108 |
127 |
30.2 |
30.2 |
152.4 |
19.1 |
4 |
5/8" |
4.1 |
9 |
|
3-1/2" |
90 |
216 |
23.9 |
122.2 |
139.7 |
31.8 |
31.8 |
177.8 |
19.1 |
8 |
5/8" |
5.1 |
11.2 |
|
4" |
100 |
228.5 |
23.9 |
134.9 |
157.2 |
33.3 |
33.3 |
190.5 |
19.1 |
8 |
5/8" |
5.9 |
13 |
|
5" |
125 |
254 |
23.9 |
163.6 |
185.7 |
36.6 |
36.6 |
215.9 |
22.4 |
8 |
3/4" |
7 |
15.4 |
|
6" |
150 |
279.5 |
25.4 |
192 |
215.9 |
39.6 |
39.6 |
241.3 |
22.4 |
8 |
3/4" |
8.4 |
18.5 |
|
8" |
200 |
343 |
28.4 |
246.1 |
269.7 |
44.5 |
44.5 |
298.5 |
22.4 |
8 |
3/4" |
13 |
28.6 |
|
10" |
250 |
406.5 |
30.2 |
304.8 |
323.9 |
49.3 |
49.3 |
362 |
25.4 |
12 |
7/8" |
18 |
39.5 |
|
12" |
300 |
482.5 |
31.8 |
365.3 |
381 |
55.6 |
55.6 |
431.8 |
25.4 |
12 |
7/8" |
29 |
64 |
|
14" |
350 |
533.5 |
35.1 |
400.1 |
412.8 |
57.2 |
57.2 |
476.3 |
28.5 |
12 |
1" |
39 |
86 |
|
16" |
400 |
597 |
36.6 |
457.2 |
469.9 |
63.5 |
63.5 |
539.8 |
28.5 |
16 |
1" |
47 |
103 |
|
18" |
450 |
635 |
39.6 |
505 |
533.4 |
68.3 |
68.3 |
577.9 |
31.8 |
16 |
1 1/8" |
57 |
126 |
|
20" |
500 |
698.5 |
42.9 |
558.8 |
584.2 |
73.2 |
73.2 |
635 |
31.8 |
20 |
1 1/8" |
76 |
167 |
|
24" |
600 |
813 |
47.8 |
663.4 |
692.2 |
82.6 |
82.6 |
749.3 |
35.1 |
20 |
1 1/4" |
97 |
214 |
Hastelloy G30 flanges Application
Wire wound resistors.
Bimetal contacts.
Electric and electronic applications.
Marine engineering.
Chemical and hydrocarbon processing equipment.
Gasoline and freshwater tanks.
Crude petroleum stills.
De-aerating heaters.
Boiler feed water heaters and other heat exchangers.
Pumps, shafts and fasteners.
Industrial heat exchangers.