Hastelloy C276 plate

 

JN Alloy is the largest stockist of Hastelloy C276 plates. We have a large inventory of Alloy C276 hot-rolled plates, ASTM B575 UNS N10276 polished plates, and Hastelloy C276 cold-rolled plates. We offer DIN 2.4819 coils in various sizes at the best price. We are a leading manufacturer of Alloy C276 strip & Hastelloy C276 sheet.

 

Hastelloy Plate is made up of a nickel-based alloy. There are different grades of the Hastelloy materials. These were first invented for molten fluoride salt containers. Hastelloy C276 plate is a high-performance superalloy of the stainless steel grade.

 

Hastelloy C276 Plate is made with a strong mix of nickel, chromium, and molybdenum. It also has tungsten added to keep these elements stable.

The Hastelloy Plate exhibits good corrosion resistance properties coupled with enhanced oxidation resistance.

 

The Hastelloy C276 Sheet is very resistant to pitting. This is especially true in water because it has a high amount of molybdenum in its chemical composition.

 

ASME SB 575

 

The UNS N10276 plate also resists damage from salt water in tight spaces. Other common materials can be harmed in these conditions.

UNS N10276 Plate is usually remedy heat-treated at 2050 degrees F and fast quenched.

 

There are many types of nickel alloy, but Hastelloy C276 Plate is the most commonly used.

 

Alloy C276 Plate shows superb deterioration resistance in a range of extreme settings and also media. Like lots of other nickel alloys, it is pliable, easily developed and also welded.

 

JN UNS N10276 Steel Plate Manufacturer

 

JN Alloys is one of the leading manufacturers and suppliers of Hastelloy products. Hastelloy C276 Sheet Plate are one of the best-selling products from our inventory.

 

We offer a wider range of outcomes. This way, our clients can find any product or component they need. We are manufacturing these plates as per the needs and requirements of our clients.

 

Hastelloy C276 Sheet Plates are available in different sizes, wall thicknesses, lengths, and specifications. We are following all industrial and international quality standards while producing these plates. This helps us to deliver perfectly suitable plates to our clients from all over the globe.

 

We are supplying Hastelloy C276 sheet plate in qualitative variety. We are producing these plates by making effective use of good-quality alloy. Our high-quality Hastelloy C276 Sheet Plate has many useful features.

 

It has high tensile strength and is easy to use. It is also very strong and has good dimensional accuracy. The surface finishes are excellent, and it can withstand high temperatures.

 

Under the strict guidance of our skilled professionals, we are producing excellent quality of the Hastelloy C276 Sheet Plate. With the use of the latest technology and modern machinery, we are enhancing the quality and quantity of products. This makes us able to deliver Hastelloy C276 Sheet Plate in the required amount.

 

Hastelloy Alloy C276 Plate Specification

 

Product Type

Hastelloy C276 ASTM B575 Sheet, Hastelloy C276 ASTM B575 Plate

Specification

ASTM B575 / ASME SB575

Tolerances (width / thickness)

EN 10258/ DIN 59381)

EN 10151 2.4819 Hastelloy C-276 Strips

EN 10088 Hastelloy C276 SB575 strips

Dimensions

Cold rolled Alloy C276 Plates 0.5-6.4 mm

Hot rolled Alloy C276 Plates 3.0–10.0 mm

Thickness

0.1 to 100 mm Thk

Width

10-2500mm

Length

2m, 2.44m, 3m, or as required

Finish

SATIN, 2B, 2D, BA NO (8), Cold rolled sheet (CR), Hot rolled plate (HR), No.1 finish hot rolled, 1D, No.4, BA, 8K, hairline, brush, mirror etc.

Hardness

Soft, Hard, Half Hard, Quarter Hard, Spring Hard

variety of shapes

Coils, Foils, Plates, Sheet, Strip, Plain Sheet, Checker Plates, Rolling Sheet, Flats, Clad Plates, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), Rolling Plates, Flat Shim, soft annealed, descaled, tread Plates, sheared, annealed

 

Chemical Composition of Hastelloy Alloy C276 Sheet & Plate

 

Grade

C

Mn

Si

S

Co

Ni

Cr

Fe

Mo

P

Hastelloy C276

0.010 max

1.00 max

0.08 max

0.03 max

2.50 max

50.99 min*

14.50 – 16.50

4 – 7

15 – 17

0.04 max

 

Mechanical Properties of Hastelloy C276 Sheet & Plates

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

8.89 g/cm3

1370 °C (2500 °F)

Psi – 1,15,000 , MPa – 790

Psi – 52,000 , MPa – 355

40 %

 

Hastelloy C276 Plates Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

GOST

EN

OR

Hastelloy C276

2.4819

N10276

NW 0276

ХН65МВУ

NiMo16Cr15W

ЭП760

 

ASTM B575 Hastelloy C276 Sheet Application

 

Pollution control stack liners, ducts, dampers, scrubbers, stack-gas reheaters, fans and fan housings.

 

Flue gas desulfurization systems.

 

Chemical processing components like heat exchangers, reaction vessels, evaporators, and transfer piping.

 

Sour gas wells.

 

Pulp and paper production.

 

Waste treatment.

 

Pharmaceutical and food processing equipment.

 

Come To Us
And Start Your RFQs Now.
contact us