Hastelloy C276 Pipe and Tube

 

JN ALLOY supplies Hastelloy C276 Pipe,Hastelloy C276 Tube,UNS N10276 Pipe tube, 2.4819 Hastelloy C276 Pipe and tube, Hastelloy Alloy C276 Pipe, Hastelloy Alloy C276 Tube, Hastelloy C276 Seamless Pipe, ASTM B474 UNS N10276 Welded Pipe, ASTM B622 UNS N10276 Seamless tube, Hastelloy C276 Pipe Price.

 

The Hastelloy C276 consists of elements like nickel, chromium, molybdenum, and tungsten, which gives the alloy its unique mechanical properties. The Hastelloy C276 Pipe is known for its excellent resistance to corrosion in various chemical environments. The unique properties make Hastelloy C276 Pipe the most popular, and hence it is one of the most abundantly used products. The high nickel content in the ASTM B622 UNS N10276 material makes it resistant to pitting and crevice corrosion in reducing environments. On the other hand, the chromium content of the Hastelloy C276 Seamless Pipe offers resistance in oxidizing media. The ASTM B622 UNS N10276 is also capable of withstanding wet chlorine gas, hypochlorite, etc., with high corrosive effects. The Hastelloy C276 Welded Pipe has low carbon content, which helps to minimize the carbide precipitation during welding. It is done to maintain the corrosion resistance properties in the as-welded structures of the Alloy C276 Pipe. This specified nickel Hastelloy C276 Seamless Pipe is also resistant to the formation of grain boundary precipitates, especially its occurrence in the weld heat-affected zone. Thus the Hastelloy C276 Welded Pipe is well suited to be used in chemical process application in an as-welded condition.

 

Jinie Technology (Jiangsu) Co., LTD is a leading manufacturer and supplier of Hastelloy C276 Pipes, offering high-quality solutions for industries that require superior corrosion resistance and durability. Hastelloy C276 Pipes are manufactured using nickel-molybdenum-chromium alloys, which provide exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking in both oxidizing and reducing environments. Known for their excellent mechanical properties, Hastelloy C276 Seamless Pipes and Welded Pipes perform reliably under high temperatures and pressures, ensuring long-term functionality in challenging environments. The low carbon content in Hastelloy pipes minimizes carbide precipitation during welding, ensuring excellent corrosion resistance even in as-welded conditions. Additionally, the smooth surface of Hastelloy pipes allows for efficient transportation of materials, making them suitable for applications in pharmaceutical production and chemical reactors.
 

Hastelloy C276 Pipe and Tubes Specifications

 

Specifications

ASTM B622, ASME SB622,ASTM B474,ASTM B626

Standard

ASTM, ASME, and API

Seamless Pipes& Tubes Size

1/8"NB--24" NB

Welded Pipes & Tubes Size

1/8"NB--48" NB

Length

Single Random, Double Random & Cut Length

Schedule

SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS

Types

Seamless / Welded/ EFW

Form

Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes

End

Plain End, Beveled End, Threaded

 

UNS N10276 Pipe Tube Chemical Composition

 

Mo

Cr

Fe

W

Co≤

C≤

Si≤

Mn≤

V≤

P≤

S≤

Ni

15.0-17.0

14.5-16.5

4.0-7.0

3.0-4.5

2.5

0.01

0.08

1.0

0.35

0.04

0.03

balance

 

Nickel alloy C276 Pipes Mechanical properties

 

Element

Density

Melting Point

Tensile Strength,min

Yield Strength,min

Elongation, min

Hastelloy C276

8.89g/cm3

1370℃

690MPa

283MPa

40%

 

Hastelloy C276 Equivalent Grades

 

STANDARD

WERKSTOFF NR.

UNS

JIS

GOST

EN

OR

Hastelloy C276

2.4819

N10276

NW 0276

ХН65МВУ

NiMo16Cr15W

ЭП760

 

Application field of Hastelloy C276 pipe and tube

 

Chemical and petroleum industry: Hastelloy C276 tubes are often used in the manufacture of reactors, heat exchangers, distillation towers and pipelines and other equipment.


Ocean engineering: Seawater contains high corrosive substances such as chloride and salt. The corrosion resistance of alloy C276 pipes makes it an ideal choice in the field of ocean engineering for the manufacture of seawater treatment equipment and offshore platform structures.


Nuclear industry: In nuclear power plants, Hastelloy C276 tubes are widely used in the manufacture of nuclear reactor components and nuclear fuel processing equipment, and its high temperature resistance and low magnetic properties are critical to the safety and performance of nuclear facilities.


Chemical processing: ASTM B622 UNS N10276 seamless pipe and tube can protect equipment from corrosion damage and ensure the stability and continuity of chemical production.
 